Microstructure evolution and mechanical properties of laser additive manufactured Ti–5Al–2Sn–2Zr–4Mo–4Cr alloy
暂无分享,去创建一个
Xin Lin | Weidong Huang | H. Tan | Qiang Zhang | J. Chen
[1] Xin Lin,et al. Texture and microstructure characterization in laser additive manufactured Ti–6Al–2Zr–2Sn–3Mo–1.5Cr–2Nb titanium alloy , 2015 .
[2] Todd Palmer,et al. Anisotropic tensile behavior of Ti-6Al-4V components fabricated with directed energy deposition additive manufacturing , 2015 .
[3] Chao Zhang,et al. Bonding interface characteristic and shear strength of diffusion bonded Ti-17 titanium alloy , 2015 .
[4] C. Tuck,et al. Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti–6Al–4V , 2014 .
[5] Dong Liu,et al. Microstructure of TA2/TA15 graded structural material by laser additive manufacturing process , 2014 .
[6] Yanyan Zhu,et al. Microstructure and mechanical properties of hybrid fabricated Ti–6.5Al–3.5Mo–1.5Zr–0.3Si titanium alloy by laser additive manufacturing , 2014 .
[7] Hua-ming Wang,et al. Characterization of microstructure and mechanical properties of laser melting deposited Ti–6.5Al–3.5Mo–1.5Zr–0.3Si titanium alloy , 2014 .
[8] Christopher Tuck,et al. On the Texture Formation of Selective Laser Melted Ti-6Al-4V , 2014, Metallurgical and Materials Transactions A.
[9] Changmeng Liu,et al. Microstructural characterization of laser melting deposited Ti–5Al-5Mo–5V–1Cr–1Fe near β titanium alloy , 2013 .
[10] Hua-ming Wang,et al. Low cycle fatigue behavior of laser melting deposited TC18 titanium alloy , 2013 .
[11] B. Baufeld. Effect of deposition parameters on mechanical properties of shaped metal deposition parts , 2012 .
[12] Christoph Leyens,et al. Mechanical properties of additive manufactured titanium (Ti–6Al–4V) blocks deposited by a solid-state laser and wire , 2011 .
[13] Heat Treater's Guide: Practices and Procedures for Nonferrous Alloys , 2011 .
[14] S. S. Al-Bermani,et al. The Origin of Microstructural Diversity, Texture, and Mechanical Properties in Electron Beam Melted Ti-6Al-4V , 2010 .
[15] I. R. Pashby,et al. Deposition of Ti–6Al–4V using a high power diode laser and wire, Part I: Investigation on the process characteristics , 2008 .
[16] S. Kelly,et al. Microstructural evolution in laser-deposited multilayer Ti-6Al-4V builds: Part II. Thermal modeling , 2004 .
[17] S. Kelly,et al. Microstructural evolution in laser-deposited multilayer Ti-6Al-4V builds: Part I. Microstructural characterization , 2004 .
[18] G. Luetjering,et al. Thermo-mechanical processing of high strength β-titanium alloys and effects on microstructure and properties , 2001 .
[19] S. L. Semiatin,et al. The laser additive manufacture of Ti-6Al-4V , 2001 .
[20] S. L. Semiatin,et al. The effect of laser power and traverse speed on microstructure, porosity, and build height in laser-deposited Ti-6Al-4V , 2000 .