Homogeneous corrosion of high pressure torsion treated Mg–Zn–Ca alloy in simulated body fluid
暂无分享,去创建一个
Yufeng Sun | Shijie Zhu | S. Guan | J. H. Gao | Z. Ren | B. Wang | B. Wang
[1] Ying Chen,et al. Dynamic degradation behavior of MgZn alloy in circulating m-SBF , 2010 .
[2] Yufeng Zheng,et al. Degradation and cytotoxicity of lotus-type porous pure magnesium as potential tissue engineering scaffold material , 2010 .
[3] Changsong Dai,et al. Corrosion behaviors of Mg and its alloys with different Al contents in a modified simulated body fluid , 2009 .
[4] T. Langdon,et al. Developing grain refinement and superplasticity in a magnesium alloy processed by high-pressure torsion , 2008 .
[5] M. Liu,et al. Influence of the β-phase morphology on the corrosion of the Mg alloy AZ91 , 2008 .
[6] M. Wei,et al. Corrosion process of pure magnesium in simulated body fluid , 2008 .
[7] R. Raman,et al. In vitro degradation and mechanical integrity of calcium-containing magnesium alloys in modified-simulated body fluid. , 2008, Biomaterials.
[8] Yuki Ito,et al. High-pressure torsion using ring specimens , 2008 .
[9] Tadashi Kokubo,et al. How useful is SBF in predicting in vivo bone bioactivity? , 2006, Biomaterials.
[10] R. Valiev,et al. Formation of nanograined structure and decomposition of supersaturated solid solution during high pressure torsion of Al-Zn and Al-Mg alloys , 2004 .