High-temperature crack-healing behaviour and strength recovery of (MoNb)Si2
暂无分享,去创建一个
Xiaohong Wang | P. Feng | Q. Lu | G. Wu | G. Zhu
[1] Xiaohong Wang,et al. Oxidation properties of self-propagating high temperature synthesized niobium disilicide , 2014 .
[2] Du Lihui,et al. OXIDATION BEHAVIOR OF IN SITU SYNTHESIZED MoSi2-SiC COMPOSITES AT 500 degrees C , 2013 .
[3] R. Tewari,et al. A Study on the Oxidation Behavior of Nb Alloy (Nb-1 pct Zr-0.1 pct C) and Silicide-Coated Nb Alloys , 2013, Metallurgical and Materials Transactions A.
[4] Shijie Zhu,et al. Crack Healing Behavior of SiC Whisker Reinforced Si3N4 Composite , 2013 .
[5] W. G. Sloof,et al. Multiple crack healing of a Ti2AlC ceramic , 2012 .
[6] A. Sharif. High-temperature oxidation of MoSi2 , 2010 .
[7] S. Ghosh,et al. Self‐Healing Materials: Fundamentals, Design Strategies, and Applications , 2009 .
[8] H. Kleebe,et al. Sintering Mechanisms of Zirconium and Hafnium Carbides Doped with MoSi2 , 2009 .
[9] K. Hellström,et al. Oxidation behaviour of a (Mo, W)Si2-based composite in dry and wet oxygen atmospheres in the temperature range 350–950 °C , 2009 .
[10] Jiecai Han,et al. Crack-healing behavior of zirconium diboride composite reinforced with silicon carbide whiskers , 2008 .
[11] R Telle,et al. Crack healing in alumina bioceramics. , 2008, Dental materials : official publication of the Academy of Dental Materials.
[12] Jian-sheng Wu,et al. Oxidation kinetics and high temperature in-situ observation of the oxidation behaviour of NbSi2 at 1023 K , 2006 .
[13] R. Mitra. Mechanical behaviour and oxidation resistance of structural silicides , 2006 .
[14] M. Chu,et al. Crack healing behavior of silicon carbide ceramics , 2004 .
[15] M. Chu,et al. Crack‐healing and mechanical behaviour of Al2O3/SiC composites at elevated temperature , 2004 .
[16] K. Houjou,et al. Crack-healing and oxidation behavior of silicon nitride ceramics , 2004 .
[17] M. Chu,et al. Crack Healing in Silicon Carbide , 2004 .
[18] Zhi-xiang Zheng,et al. Preliminary study of the crack healing and strength recovery of Al2O3-matrix composites , 2004 .
[19] T. Mitchell,et al. Deformation mechanisms of polycrystalline MoSi2 alloyed with 1 at.% Nb , 2003 .
[20] Chen Chuanzhong,et al. MICROSTRUCTURE OF HIGH-TEMPERATURE OXIDATION LAYER OF MOLYBDENUM DISILICIDE , 2003 .
[21] Shigemi Sato,et al. Crack-healing behavior of Si3N4/SiC ceramics under stress and fatigue strength at the temperature of healing (1000 °C) , 2002 .
[22] Y. Park,et al. Microstructure and Mechanical Properties of MoSi2/Nb Composites Made by MA-Pulse Discharge Sintering , 2000 .
[23] E. Summers,et al. Extrusion and selected engineering properties of Mo–Si–B intermetallics , 2000 .
[24] Makoto Yoshida,et al. Interfacial modification and impact properties of Nb/MoSi2 laminate composites by the addition of ZrO2, NbSi2, and SiC particles , 2000 .
[25] T. Mitchell,et al. Rapid solution hardening at elevated temperatures by substitutional Re alloying in MoSi2 , 2000 .
[26] A. K. Vasudevan,et al. Key developments in high temperature structural silicides , 1999 .
[27] E. Kaxiras,et al. Microalloying for ductility in molybdenum disilicide , 1999 .
[28] T. Nakano,et al. Effect of alloying elements on anomalous strengthening of NbSi2-based silicides with C40 structure , 1997 .
[29] R. Abbaschian,et al. Toughening MoSi2 with niobiúm metal—effects of morphology of ductile reinforcements , 1995 .
[30] A. Heuer,et al. High temperature plastic anisotropy in MoSi2 single crystals , 1995 .
[31] B. Linder,et al. Molybdenum disilicide heating elements: meeting advanced ceramics requirements , 1989 .
[32] T. Gupta. Crack Healing and Strengthening of Thermally Shocked Alumina , 1976 .
[33] A. Sharif. Effects of Nb-Alloying on High-Temperature Oxidation of MoSi_2 , 2014 .
[34] Zhang Laiq. Oxidation Behavior of in-situ Synthesized MoSi_2-SiC Composites at 700℃ , 2013 .
[35] 张来启,et al. 原位合成 MoSi 2 -SiC复合材料在 500℃的氧化行为 , 2013 .
[36] Wen-ming Guo,et al. Investigation of MoSi2 melt infiltrated RSiC and its oxidation behavior , 2012 .
[37] J.Th.M. De Hosson,et al. Oxidation-induced crack healing in Ti3AlC2 ceramics , 2008 .
[38] J. Svensson,et al. The beneficial effect of water vapour on the oxidation at 600 and 700 °C of a MoSi2-based composite , 2005 .
[39] A. Shan,et al. Tailoring the microstructure of molybdenum disilicide matrix composites with Nb additions , 2004 .
[40] Y. Zeng,et al. Oxidation behavior of hot-pressed MoSi2-TiC composite , 2001 .
[41] Y. Murata,et al. Solid solution softening and hardening in alloyed MoSi2 , 1998 .
[42] P. Tsakiropoulos,et al. Study of The Microstructure and Oxidation of NbSi 2 Base Alloys , 1994 .
[43] D. L. Douglass,et al. Grain Growth in Thin Films of ThO2, NpO2, and PuO2 , 1968 .