A dense structure Si-SiC coating for oxidation and ablation protection of graphite fabricated by impregnation-pyrolysis and gaseous silicon infiltration

[1]  Xiaohong Shi,et al.  Oxidation and ablation resistant properties of pack-siliconized Si-C protective coating for carbon/carbon composites , 2018 .

[2]  Dong-Yang Feng,et al.  Oxidation protective ZrB2-MoSi2-SiC-Si coating for graphite materials prepared by slurry dipping and vapor silicon infiltration , 2018 .

[3]  Yan Jiang,et al.  Oxidation protective MoSi2-SiC-Si coating for graphite materials prepared by slurry dipping and vapor silicon infiltration , 2017 .

[4]  P. Zhou,et al.  Dual layer SiC coating on matrix graphite sphere prepared by pack cementation and fluidized‐bed chemical vapor deposition , 2017 .

[5]  Yi Zeng,et al.  Microstructure evolution and thermomechanical properties of plasma‐sprayed Yb2SiO5 coating during thermal aging , 2017 .

[6]  Ling-jun Guo,et al.  Improving the oxidation resistance under thermal shock condition of SiC-coated C/C composites with refined SiC grain size using ferrocene , 2017 .

[7]  Wang Lu,et al.  A novel gradient SiC-ZrB2-MoSi2 coating for SiC coated C/C composites by supersonic plasma spraying , 2017 .

[8]  M. Eguchi,et al.  Synthesis of SiC coating from SiO by a chemical vapor deposition (CVD) process , 2017 .

[9]  Hejun Li,et al.  Mechanical and oxidation protective properties of SiC nanowires-toughened SiC coating prepared in-situ by a CVD process on C/C composites , 2016 .

[10]  P. Zhou,et al.  Micro Four‐Layer SiC Coating on Matrix Graphite Spheres of HTR Fuel Elements by Two‐Step Pack Cementation , 2016 .

[11]  Hejun Li,et al.  Influence of β-SiC on the microstructures and thermal properties of SiC coatings for C/C composites , 2016 .

[12]  W. Han,et al.  Ablation resistance of ZrB2SiC/SiC coating prepared by pack cementation for graphite , 2016 .

[13]  A. Abdollahi,et al.  Thermal shock resistance and isothermal oxidation behavior of C/SiC-SiCnano functionally gradient coating on graphite produced via reactive melt infiltration (RMI) , 2016 .

[14]  Hejun Li,et al.  Comparison of the oxidation behaviors of SiC coatings on C/C composites prepared by pack cementation and chemical vapor deposition , 2016 .

[15]  Jae-Won Park,et al.  Enhancing the oxidation resistance of graphite by applying an SiC coat with crack healing at an elevated temperature , 2016 .

[16]  Yiguang Wang,et al.  Ablation behavior of C/SiC composites in plasma wind tunnel , 2016 .

[17]  A. Abdollahi,et al.  C/SiC Gradient Oxidation Protective Coating on Graphite by Modified Reactive Melt Infiltration Method: Effects of Processing Parameters on Transition Interface Thickness and High-Temperature Anti-oxidation Behavior , 2016, Metallurgical and Materials Transactions A.

[18]  Hejun Li,et al.  Oxidation resistance and mechanical properties of HfC nanowire-toughened ultra-high temperature ceramic coating for SiC-coated C/C composites , 2016 .

[19]  Hejun Li,et al.  A SiC-ZrB2-ZrC coating toughened by electrophoretically-deposited SiC nanowires to protect C/C composites against thermal shock and oxidation , 2015 .

[20]  Suhrit Mula,et al.  Surface morphology evolution and ablation mechanism of SiC–Si multiphase ceramic coating on graphite under oxy-acetylene flame , 2014 .

[21]  Hejun Li,et al.  ZrB2–SiC gradient oxidation protective coating for carbon/carbon composites , 2014 .

[22]  L. Chai,et al.  Resistance to oxidation and ablation of SiC coating on graphite prepared by chemical vapor reaction , 2013 .

[23]  B. Harder,et al.  Oxidation Transitions for SiC Part II. Passive‐to‐Active Transitions , 2013 .

[24]  Jianfeng Huang,et al.  A mullite/SiC oxidation protective coating for carbon/carbon composites , 2013 .

[25]  Xiaohong Shi,et al.  Effect of LaB6 on the thermal shock property of MoSi2-SiC coating for carbon/carbon composites , 2013 .

[26]  Hejun Li,et al.  Oxidation protection of C/C composites with a multilayer coating of SiC and Si + SiC + SiC nanowires , 2012 .

[27]  B. Drevet,et al.  Resistance to oxidation of graphite silicided by reactive infiltration , 2011 .

[28]  F. Sarasini,et al.  Silicon Carbide Based Plasma Sprayed Coatings , 2011, International Thermal Spray Conference.

[29]  L. Qin,et al.  SiC nanowire-toughened SiC–MoSi2–CrSi2 oxidation protective coating for carbon/carbon composites , 2010 .

[30]  H. Tian,et al.  Synthesis and characterization of carbon/silica superhydrophobic multi-layer films , 2010 .

[31]  Heng Wu,et al.  A Si―SiC oxidation protective coating for carbon/carbon composites prepared by a two-step pack cementation , 2009 .

[32]  W. Bo,et al.  SiCn/SiC oxidation protective coating for carbon/carbon composites , 2009 .

[33]  Lang Liu,et al.  Microstructure and property of SiC coating for carbon materials , 2007 .

[34]  Hejun Li,et al.  Yttrium silicate oxidation protective coating for SiC coated carbon/carbon composites , 2006 .

[35]  Junmin Qian,et al.  Porous SiC ceramics fabricated by reactive infiltration of gaseous silicon into charcoal , 2004 .

[36]  Monica Ferraris,et al.  Multilayer coating with self-sealing properties for carbon-carbon composites , 2003 .

[37]  Soojin Park,et al.  The effects of MoSi2 on the oxidation behavior of carbon/carbon composites , 2001 .

[38]  P. Molian,et al.  A novel laser technique for oxidation-resistant coating of carbon-carbon composite , 2001 .

[39]  W. Rhim,et al.  Thermophysical properties measurement of molten silicon by high-temperature electrostatic levitator: density, volume expansion, specific heat capacity, emissivity, surface tension and viscosity , 2000 .