Sintered product of rejects and shale modular cellular bricks and preparing method thereof

The invention discloses a sintered product of rejects and shale modular cellular bricks and a preparing method thereof. The preparing method of the product comprises the following steps of: ensuring that the raw material with the fineness being lower than 0.5 to 0.25 mm occupies 65 percent of all the raw materials through rough crushing, fine crushing and sifting; blending rejects and shale in proportion by weight of 70 to 85 percent: 15 to 30 percent, and adding water and uniformly stirring, and putting the material into a storage warehouse to be stored, wherein the quantity of water added is excessive; feeding the stored material into a molding machine to be conducted to semi-hard plastic extrusion molding; sintering at the maximum temperature of 1000 to 1080 DEG C for 8 to 16 hours; ensuring that the firing time is 28 to 36 hours; and slacking the material in water after kiln discharging and sorting. The main material of the product adopts rejects which are abandoned by most mines and required to be conducted to safe disposal, the preparing method can effectively and conjunctively utilize rejects, change waste into valuable, meet the requirements of energy saving and emission reduction, and achieve significant social benefit and economic benefit.