Microtexture in additively manufactured Ti-6Al-4V fabricated using directed energy deposition

Abstract The additive manufacturing (AM) of α + β titanium alloys using electron beam (EB) and laser directed energy deposition (DED) processes has been widely characterized in both the as-deposited and post processed conditions. Fine basket weave α lath structures are commonly observed in both the as-deposited and post processed hot isostatically pressed (HIP) conditions for both laser and EB DED processes, but more in-depth knowledge of the crystallographic texturing and variant selection of the α laths growing from the primary β-grains across the height of EB DED Ti-6Al-4V structures is not well established. At locations near the substrate in both conditions, microtexturing is weak, but EB DED builds exhibit a strong microtexture and pronounced variant selection with increasing build height. On the other hand, the laser DED builds displayed weak texturing and no prominent variant selection across all heights. With the addition of HIP post processing, there was no change in microtexturing of the coarsened α laths for both the laser and EB structures, and the same variant selection observed in the as-deposited EB DED builds was present.

[1]  H. Bunge Texture Analysis in Materials Science , 1982 .

[2]  B. Stucker,et al.  Microstructures and Mechanical Properties of Ti6Al4V Parts Fabricated by Selective Laser Melting and Electron Beam Melting , 2013, Journal of Materials Engineering and Performance.

[3]  Christoph Leyens,et al.  Mechanical properties of additive manufactured titanium (Ti–6Al–4V) blocks deposited by a solid-state laser and wire , 2011 .

[4]  A. Rollett,et al.  Austenite Reconstruction Elucidates Prior Grain Size Dependence of Toughness in a Low Alloy Steel , 2018, Metallurgical and Materials Transactions A.

[5]  Yunzhi Wang,et al.  Variant selection during α precipitation in Ti–6Al–4V under the influence of local stress – A simulation study , 2013 .

[6]  R. Yang,et al.  Effect of β (110) texture intensity on α-variant selection and microstructure morphology during β→α phase transformation in near α titanium alloy , 2017 .

[7]  Heat treatment of Ti6Al4V produced by Selective Laser Melting: Microstructure and mechanical properties , 2012 .

[8]  C. Emmelmann,et al.  Additive Manufacturing of Metals , 2016 .

[9]  H. Fraser,et al.  The role of crystallographic and geometrical relationships between α and β phases in an α/β titanium alloy , 2003 .

[10]  C. Kenel,et al.  In situ investigation of phase transformations in Ti-6Al-4V under additive manufacturing conditions combining laser melting and high-speed micro-X-ray diffraction , 2017, Scientific Reports.

[11]  M. L. Griffith,et al.  Solidification in direct metal deposition by LENS processing , 2001 .

[12]  H. Bhadeshia,et al.  Dual orientation and variant selection during diffusional transformation of austenite to allotriomorphic ferrite , 2010 .

[13]  K. Chou,et al.  EBSD study of beam speed effects on Ti-6Al-4V alloy by powder bed electron beam additive manufacturing , 2018, Journal of Alloys and Compounds.

[14]  N. Gey,et al.  Study of the α → β phase transformation of a Ti-6Al-4V sheet by means of texture change , 2000 .

[15]  A. Nassar,et al.  Additive Manufacturing of Ti-6Al-4V Using a Pulsed Laser Beam , 2015, Metallurgical and Materials Transactions A.

[16]  Weidong Huang,et al.  Formation mechanism of the α variant and its influence on the tensile properties of laser solid formed Ti-6Al-4V titanium alloy , 2017 .

[17]  A. Beese,et al.  Impact of Interlayer Dwell Time on Microstructure and Mechanical Properties of Nickel and Titanium Alloys , 2017, Metallurgical and Materials Transactions A.

[18]  Adam L. Pilchak,et al.  Evolution of Texture from a Single Crystal Ti-6Al-4V Substrate During Electron Beam Directed Energy Deposition , 2017, Metallurgical and Materials Transactions A.

[19]  Konrad Wissenbach,et al.  Ductility of a Ti‐6Al‐4V alloy produced by selective laser melting of prealloyed powders , 2010 .

[20]  G. Rohrer,et al.  Five-parameter grain boundary analysis of a titanium alloy before and after low-temperature annealing , 2008 .

[21]  Matthew S. Dargusch,et al.  Controlling the microstructure and properties of wire arc additive manufactured Ti–6Al–4V with trace boron additions , 2015 .

[22]  W. G. Burgers On the process of transition of the cubic-body-centered modification into the hexagonal-close-packed modification of zirconium , 1934 .

[23]  Ryan B. Wicker,et al.  Microstructures and mechanical properties of electron beam-rapid manufactured Ti–6Al–4V biomedical prototypes compared to wrought Ti–6Al–4V , 2009 .

[24]  Chee Kai Chua,et al.  Graded microstructure and mechanical properties of additive manufactured Ti–6Al–4V via electron beam melting , 2015 .

[25]  Todd Palmer,et al.  Anisotropic tensile behavior of Ti-6Al-4V components fabricated with directed energy deposition additive manufacturing , 2015 .

[26]  S. S. Al-Bermani,et al.  The Origin of Microstructural Diversity, Texture, and Mechanical Properties in Electron Beam Melted Ti-6Al-4V , 2010 .

[27]  M. L. Griffith,et al.  Understanding thermal behavior in the LENS process , 1999 .

[28]  J. Kruth,et al.  A study of the microstructural evolution during selective laser melting of Ti–6Al–4V , 2010 .

[29]  M. Preuss,et al.  The influence of rolling temperature on texture evolution and variant selection during α → β → α phase transformation in Ti–6Al–4V , 2012 .

[30]  A. A. Salem,et al.  Variant Selection During Cooling after Beta Annealing of Ti-6Al-4V Ingot Material , 2012, Metallurgical and Materials Transactions A.

[31]  Edward M. Lehockey,et al.  Mapping Residual Plastic Strain in Materials Using Electron Backscatter Diffraction , 2000 .

[32]  N. Gey,et al.  Specific analysis of EBSD data to study the texture inheritance due to the β → α phase transformation , 2003 .

[33]  H. Fraser,et al.  Precipitation of grain boundary α in a laser deposited compositionally graded Ti–8Al–xV alloy – an orientation microscopy study , 2004 .

[34]  Lijun Song,et al.  Fabrication of Ti-6Al-4V Scaffolds by Direct Metal Deposition , 2008 .

[35]  Structure‐Property Correlations for Additively Manufactured Ti‐6Al‐4V Components Produced Using Directed Energy Deposition Processes , 2016 .

[36]  D. Prior,et al.  In situ SEM-EBSD observations of the hcp to bcc phase transformation in commercially pure titanium , 2004 .

[37]  H. Wenk,et al.  In situ observation of texture evolution during α → β and β → α phase transformations in titanium alloys investigated by neutron diffraction , 2007 .

[38]  Todd Palmer,et al.  Role of geometry on properties of additively manufactured Ti-6Al-4V structures fabricated using laser based directed energy deposition , 2016 .

[39]  R. P. Martukanitz,et al.  Thermal and microstructural analysis of laser-based directed energy deposition for Ti-6Al-4V and Inconel 625 deposits , 2018 .

[40]  Moataz M. Attallah,et al.  Microstructure and tensile properties of selectively laser-melted and of HIPed laser-melted Ti–6Al–4V , 2013 .

[41]  Q. Chao,et al.  Variant selection and intervariant crystallographic planes distribution in martensite in a Ti-6Al-4V alloy , 2014 .

[42]  James C. Williams,et al.  Perspectives on Titanium Science and Technology , 2013 .

[43]  L. Murr,et al.  Microstructure and mechanical behavior of Ti-6Al-4V produced by rapid-layer manufacturing, for biomedical applications. , 2009, Journal of the mechanical behavior of biomedical materials.

[44]  S. L. Semiatin,et al.  Microstructure and texture evolution during solidification processing of Ti–6Al–4V , 2003 .

[45]  H. Fraser,et al.  Variant selection of grain boundary α by special prior β grain boundaries in titanium alloys , 2014 .

[46]  Bo Song,et al.  Effects of processing parameters on microstructure and mechanical property of selective laser melted Ti6Al4V , 2012 .

[47]  I. R. Pashby,et al.  Microstructure formation in Waspaloy multilayer builds following direct metal deposition with laser and wire , 2008 .

[48]  S. Saroja,et al.  Evaluation of misorientation angle-axis set between variants during transformation of bcc to hcp phase obeying Burgers orientation relation , 2006 .

[49]  P. S. Bate,et al.  Crystallographic variant selection in Ti–6Al–4V , 2004 .

[50]  Omer Van der Biest,et al.  Wire based additive layer manufacturing: Comparison of microstructure and mechanical properties of Ti–6Al–4V components fabricated by laser-beam deposition and shaped metal deposition , 2011 .

[51]  H. Fraser,et al.  Crystallographic and morphological relationships between β phase and the Widmanstätten and allotriomorphic α phase at special β grain boundaries in an α/β titanium alloy , 2007 .

[52]  C. Colin,et al.  As-Fabricated and Heat-Treated Microstructures of the Ti-6Al-4V Alloy Processed by Selective Laser Melting , 2011 .

[53]  N. Gey,et al.  An advanced approach to reconstructing parent orientation maps in the case of approximate orientation relations: Application to steels , 2012 .

[54]  S. Kelly,et al.  Microstructural evolution in laser-deposited multilayer Ti-6Al-4V builds: Part I. Microstructural characterization , 2004 .

[55]  N. Gey,et al.  Characterization of the variant selection occurring during the α→β→α phase transformations of a cold rolled titanium sheet , 2002 .

[56]  S. Saroja,et al.  Effect of cooling rate on transformation texture and variant selection during β → α transformation in Ti–5Ta–1.8Nb alloy , 2010 .

[57]  J. C. Huang,et al.  Texture analysis in hexagonal materials , 2003 .

[58]  Vasily Ploshikhin,et al.  Three-dimensional modeling of the microstructure evolution during metal additive manufacturing , 2018 .

[59]  M. Starink,et al.  Effect of self-accommodation on α/α boundary populations in pure titanium , 2003 .

[60]  Yanjin Lu,et al.  Crystallographic features of α variants and β phase for Ti-6Al-4V alloy fabricated by selective laser melting , 2017 .

[61]  Philip B. Prangnell,et al.  Effect of build geometry on the β-grain structure and texture in additive manufacture of Ti6Al4V by selective electron beam melting , 2013 .

[62]  Filippo Berto,et al.  Fatigue Behavior of Porous Ti-6Al-4V Made by Laser-Engineered Net Shaping , 2018, Materials.

[63]  Brent Stucker,et al.  Analysis of defect generation in Ti–6Al–4V parts made using powder bed fusion additive manufacturing processes , 2014 .

[64]  A. Wilkinson,et al.  Quantification of plastic strain of stainless steel and nickel alloy by electron backscatter diffraction , 2006 .

[65]  Maxime Moreaud,et al.  Three-dimensional microtomographic study of Widmanstätten microstructures in an alpha/beta titanium alloy , 2008 .

[66]  Eric J. Faierson,et al.  A framework to link localized cooling and properties of directed energy deposition (DED)-processed Ti-6Al-4V , 2017 .

[67]  Thomas R. Bieler,et al.  The effect of alpha platelet thickness on plastic flow during hot working of TI–6Al–4V with a transformed microstructure , 2001 .

[68]  C. Tuck,et al.  Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti–6Al–4V , 2014 .

[69]  Olivier Rigo,et al.  Electron beam melted Ti–6Al–4V: Microstructure, texture and mechanical behavior of the as-built and heat-treated material , 2016 .

[70]  S. Kelly,et al.  Microstructural evolution in laser-deposited multilayer Ti-6Al-4V builds: Part II. Thermal modeling , 2004 .

[71]  M. E. Schlienger,et al.  Laser-deposited advanced materials , 2001 .

[72]  J. S. Zuback,et al.  Additive manufacturing of metallic components – Process, structure and properties , 2018 .

[73]  N. Shamsaei,et al.  Mechanical Properties and Microstructural Features of Direct Laser-Deposited Ti-6Al-4V , 2015 .