Effects of grain-boundary segregation and precipitation on the hydrogen susceptibility of nickel
暂无分享,去创建一个
[1] H. Birnbaum. Hydrogen Related Fracture of Metals , 1983 .
[2] G. Hubler,et al. Effect of Helium, Iron, and Platinum Implantation on the Absorption of Hydrogen by Iron , 1980 .
[3] R. Staehle,et al. Effect of Sulfur Segregation on Intergranular Corrosion of Nickel in Dilute Sulfuric Acid Solutions , 1979 .
[4] Z. A. Foroulis,et al. Environment-sensitive fracture of engineering materials : proceedings of a symposium held at the fall meeting of the Metallurgical Society of AIME in Chicago, Illinois, October 24-26, 1977 , 1979 .
[5] I. Bernstein,et al. A quantitative analysis of hydrogen trapping , 1978 .
[6] M. Aucouturier,et al. Observation of Hydrogen Trapping in Fe-0.15 Wt% Ti Alloy by High Resolution Autoradiography , 1978 .
[7] C. Wert. Trapping of hydrogen in metals , 1978 .
[8] R. Latanision,et al. The intergranular embrittlement of nickel by hydrogen: The effect of grain boundary segregation , 1974, Metallurgical and Materials Transactions B.
[9] B. A. Wilcox,et al. Deformation and fracture of dispersion-strengthened nickel charged with hydrogen , 1972 .
[10] K. Schwabe,et al. Beitrag zur passivität des nickels , 1964 .