Microstructural features of the ZrO2 interfacial coatings on SiC fibers before and after exposition to air at high temperatures

[1]  B. Zaitsev,et al.  Interfacial Coatings on Inorganic Fibers for High Temperature Ceramic Matrix Composites , 2008 .

[2]  B. Kolesov,et al.  Raman study of yttria-stabilized zirconia interfacial coatings on Nicalon™ fiber , 2007 .

[3]  B. Zaitsev,et al.  Atomic force and scanning electron microscopy study of zirconia-coated silicon carbide fibers , 2007 .

[4]  R. Hay,et al.  Monazite Coatings on SiC Fibers I: Fiber Strength and Thermal Stability , 2006 .

[5]  R. Hay,et al.  Monazite Coatings on SiC Fibers II: Oxidation Protection , 2006 .

[6]  F. Zok Developments in Oxide Fiber Composites , 2006 .

[7]  T. Ogasawara,et al.  Potential strength of Nicalon™, Hi Nicalon™, and Hi Nicalon Type S™ monofilaments of variable diameters , 2006 .

[8]  A. Boronin,et al.  The yttria-stabilized zirconia and interfacial coating on Nicalon™ fiber , 2006 .

[9]  Seth T. Taylor,et al.  Kinetics of Thermal, Passive Oxidation of Nicalon Fibers , 2005 .

[10]  A. Kohyama,et al.  Effect of heat treatment on the tensile strength and creep resistance of advanced SiC fibers , 2004 .

[11]  P. Colomban,et al.  Rayleigh and Raman images of the bulk/surface nanostructure of SiC based fibres , 2004 .

[12]  J. Bouix,et al.  Sol-gel preparation and thermo-mechanical properties of porous xAl2O3–ySiO2 coatings on SiC Hi-Nicalon fibres , 2003 .

[13]  E. Carter,et al.  Exploiting Covalency to Enhance Metal–Oxide and Oxide–Oxide Adhesion at Heterogeneous Interfaces , 2003 .

[14]  Woo Y. Lee,et al.  Morphological Evolution and Weak Interface Development within Chemical-Vapor-Deposited Zirconia Coating Deposited on Hi-Nicalon™ Fiber , 2002 .

[15]  G. Busca,et al.  Vibrational and electronic spectroscopic properties of zirconia powders , 2001 .

[16]  J. White,et al.  Interfacial silicon oxide formation during synthesis of ZrO2 on Si(100) , 2000 .

[17]  P. Colomban,et al.  Sol-gel mullite matrix-SiC and -mullite 2D woven fabric composites with or without zirconia containing interphase: Elaboration and properties , 1996 .

[18]  P. D. Jero,et al.  Effect of interfacial roughness parameters on the fiber pushout behavior of a model composite , 1994 .

[19]  G. Grathwohl,et al.  Sol-gel coatings on ceramic fibers for ceramic matrix composites , 1992 .

[20]  P. D. Jero,et al.  Effect of Interfacial Roughness on the Frictional Stress Measured Using Pushout Tests , 1991 .

[21]  Anthony G. Evans,et al.  Overview no. 85 The mechanical behavior of ceramic matrix composites , 1989 .

[22]  S. W. Lee,et al.  The infrared and Raman spectra of ZrO2-SiO2 glasses prepared by a sol-gel process , 1988 .

[23]  G. Socrates,et al.  Infrared Characteristic Group Frequencies , 1980 .

[24]  D. J. Lockwood,et al.  Raman spectrum of synthetic zircon (ZrSiO4) and thorite (ThSiO4) , 1977 .

[25]  E. Subbarao,et al.  Axial thermal expansion of ZrO2 and HfO2 in the range room temperature to 1400°C , 1969 .