SiC Coatings for Carbon/Carbon Composites Fabricated by Vacuum Plasma Spraying Technology
暂无分享,去创建一个
Jinliang Sun | Xuebin Zheng | Y. Niu | M. Ren | H. Li | Cui Hu
[1] C. Ding,et al. Microstructure characteristics of silicon carbide coatings fabricated on C/C composites by plasma spraying technology , 2011 .
[2] Hejun Li,et al. A MoSi2/SiC oxidation protective coating for carbon/carbon composites , 2011 .
[3] Dajie Zhang,et al. Microstructural evolution during silicon carbide (SiC) formation by liquid silicon infiltration using optical microscopy , 2010 .
[4] Heng Wu,et al. A Si―SiC oxidation protective coating for carbon/carbon composites prepared by a two-step pack cementation , 2009 .
[5] Xuanyong Liu,et al. Microstructure and Properties Characterization of Silicon Coatings Prepared by Vacuum Plasma Spraying Technology , 2009 .
[6] W. Bo,et al. SiCn/SiC oxidation protective coating for carbon/carbon composites , 2009 .
[7] Jingyi Deng,et al. Comparison of thermal and ablation behaviors of C/SiC composites and C/ZrB2–SiC composites , 2009 .
[8] P. Ding,et al. Oxidation behavior and kinetics of SiC/alumina-borosilicate coating for carbon-carbon composites , 2008 .
[9] R. W. Rauser,et al. Oxidation through coating cracks of SiC-protected carbon/carbon , 2008 .
[10] Jiecai Han,et al. Oxidation-resistant ZrB2-SiC composites at 2200 °C , 2008 .
[11] K. Prabhu,et al. Review of non-reactive and reactive wetting of liquids on surfaces. , 2007, Advances in colloid and interface science.
[12] T. Valente,et al. Plasma spray deposition of ultra high temperature ceramics , 2006 .
[13] Huang Jianfeng,et al. Influence of the preparation temperature on the phase, microstructure and anti-oxidation property of a SiC coating for C/C composites , 2004 .
[14] T. Valente,et al. Plasma spray deposition and high temperature characterization of ZrB2–SiC protective coatings , 2002 .
[15] Kevin Barraclough,et al. I and i , 2001, BMJ : British Medical Journal.
[16] H. Fukuda,et al. SiC/C multi-layered coating contributing to the antioxidation of C/C composites and the suppression of through-thickness cracks in the layer , 2001 .
[17] J. C. Bressiani,et al. Functionally gradient ceramic coating for carbon–carbon antioxidation protection , 2001 .
[18] M. Ferraris,et al. Protective Coating for Carbon‐Carbon Composites , 2001 .
[19] M. Ferraris,et al. Joining of surface modified Carbon/Carbon composites using a barium-aluminum-boro-silicate glass , 1998 .
[20] Guan Jie,et al. Improvement in oxidation resistance of the nuclear graphite by reaction-coated SiC coating , 1995 .
[21] Kazuo Kobayashi,et al. Formation and oxidation resistance of the coating formed on carbon material composed of B4C-SiC powders , 1995 .
[22] J. Sheehan. Oxidation protection for carbon fiber composites , 1989 .
[23] E. Fitzer. The future of carbon-carbon composites , 1987 .
[24] R. Mévrel,et al. Pack cementation processes , 1986 .