Effect of final annealing temperature on critical current density of Ag/Bi-(Pb)-Sr-Ca-Cu-O tapes

[1]  S. Dou,et al.  Improved critical current of superconducting Bi2223 - Ag tapes for current lead application by addition of `large' silver particles , 1996 .

[2]  S. Dou,et al.  Preparation of Ag - Bi-2223 tape by controlling the phase evolution prior to sintering , 1996 .

[3]  D. Larbalestier,et al.  Magnetic granularity, percolation and preferential current flow in a silver-sheathed Bi1.8Pb0.4Sr2Ca2Cu3O8+x tape , 1995 .

[4]  D. Larbalestier,et al.  Texture relationships and interface structure in Ag-sheathed Bi(Pb)-Sr-Ca-Cu-O superconducting tapes , 1994 .

[5]  D. Larbalestier,et al.  Further evidence that the critical current density of (Bi, Pb)2Sr2Ca2Cu3Ox silver-sheathed tapes is controlled by residual layers of (Bi, Pb)2Sr2CaCu2Oy at (001) twist boundaries , 1994 .

[6]  S. Dou,et al.  Ag-sheathed Bi(Pb)SrCaCuO superconducting tapes , 1993 .

[7]  S. Dou,et al.  Enhanced flux pinning through a phase formation-decomposition-recovery process in Ag-sheathed Bi(Pb)SrCaCuO wires , 1993, IEEE Transactions on Applied Superconductivity.

[8]  S. Dou,et al.  Critical current density, irreversibility line, and flux creep activation energy in silver-sheathed Bi/sub 2/Sr/sub 2/Ca/sub 2/Cu/sub 3/O/sub x/ superconducting tapes , 1993, IEEE Transactions on Applied Superconductivity.

[9]  S. Dou,et al.  Effect of a controlled melt process on phase transformation and electromagnetic properties of BiPbSrCaCuO/Ag superconducting wires , 1993 .

[10]  S. Dou,et al.  Microstructure and defects in Ag-clad Bi-Pb-Sr-Ca-Cu-O wires prepared through a controlled melt process , 1992 .

[11]  H. Liu,et al.  Stability of high-Tc phase in Ag-clad Bi-based superconducting wires , 1992 .

[12]  S. Dou,et al.  Improvement of flux pinning in the Ag-clad Bi-Pb-Sr-Ca-Cu-O wires through the use of a short period melt processing , 1992 .