Effect of silicon content on microstructure of Al-Si/SiCp composite layer cladded on A380 Al alloy by TIG welding process

[1]  Y. Şahin Abrasive wear behaviour of SiC/2014 aluminium composite , 2010 .

[2]  H. Zoch,et al.  Spray forming of hypereutectic Al–Si alloys , 2009 .

[3]  K. Acker,et al.  Metal matrix composite production by means of laser dispersing of SiC and WC powder in Al alloy , 2009 .

[4]  Abdolreza Simchi,et al.  Effect of SiC particles on the laser sintering of Al-7Si-0.3Mg alloy , 2008 .

[5]  R. Sun,et al.  Microstructure and hardness of laser clad SiCp–Al composite coatings on Al alloys , 2008 .

[6]  J. Hosson,et al.  Microstructure and wear studies of laser clad Al-Si/SiC(p) composite coatings , 2007 .

[7]  Larry D. Hefti,et al.  Commercial Airplane Applications of Superplastically Formed AA5083 Aluminum Sheet , 2007 .

[8]  D. Fu,et al.  Effect of the silicon content and thermomechanical treatment on the dry sliding wear behavior of spray-deposited Al–Si/SiCp composites , 2007 .

[9]  Muneharu Kutsuna,et al.  Comparison between diode laser and TIG cladding of Co-based alloys on the SUS403 stainless steel , 2006 .

[10]  J. Sokolowski,et al.  Thermal analysis and microscopical characterization of Al–Si hypereutectic alloys , 2006 .

[11]  Jiang Xu,et al.  Microstructure and wear properties of laser cladding Ti–Al–Fe–B coatings on AA2024 aluminum alloy , 2006 .

[12]  D. Walter,et al.  Solid State Reactions in the Al‐Si‐C System , 2005 .

[13]  T. Ma,et al.  Dry sliding wear behavior of cast SiC-reinforced Al MMCs , 2003 .

[14]  N. Chen,et al.  In situ formation of MoSi2/SiC composite coating on pure Al by laser cladding , 2003 .

[15]  H. Ye,et al.  An overview of the development of Al-Si-Alloy based material for engine applications , 2003 .

[16]  Rui M. Vilar,et al.  Laser cladding , 2003, Advanced Laser Technologies.

[17]  J. L. Baldonedo,et al.  Interfacial reactions in an Al-Cu-Mg (2009)/SiCw composite during liquid processing Part I Casting , 2001 .

[18]  T. Yue,et al.  Cavitation erosion and corrosion behaviour of laser surface alloyed MMC of SiC and Si3N4 on Al alloy AA6061 , 2000 .

[19]  K. Al-Rubaie,et al.  Two-body abrasive wear of Al–SiC composites , 1999 .

[20]  K. Al-Rubaie,et al.  Three-body abrasion of Al–SiC composites , 1999 .

[21]  S. Lim,et al.  High-speed tribological properties of some Al/SiCp composites : II. Wear mechanisms , 1999 .

[22]  S. Lim,et al.  High-speed tribological properties of some Al/SiCp composites: I. Frictional and wear-rate characteristics , 1999 .

[23]  A. Hamdi,et al.  Ion implantation and diamond-like coatings of aluminum alloys , 1997 .

[24]  C. Xie,et al.  Laser cladding of iron- base alloy on al-si alloy and its relation to cracking at the interface , 1996 .

[25]  E. Lugscheider,et al.  PVD coatings on aluminium substrates , 1995 .

[26]  P. K. Datta,et al.  Surface engineering practice : processes, fundamentals, and applications in corrosion and wear , 1989 .