Ultra-precision cryogenic machining of viscoelastic polymers
暂无分享,去创建一个
[1] Y. Takeuchi,et al. Ultraprecision 3D Micromachining of Glass , 1996 .
[2] Shane Y. Hong,et al. Friction and cutting forces in cryogenic machining of Ti–6Al–4V , 2001 .
[3] A. Shih,et al. End Milling of Elastomers—Fixture Design and Tool Effectiveness for Material Removal , 2004 .
[4] Hans Nørgaard Hansen,et al. Dimensional micro and nano metrology , 2006 .
[5] A. Manz,et al. Lab-on-a-chip: microfluidics in drug discovery , 2006, Nature Reviews Drug Discovery.
[6] Sangkee Min,et al. Recent Advances in Mechanical Micromachining , 2006 .
[7] Ian Papautsky,et al. Photodefinable polydimethylsiloxane (PDMS) for rapid lab-on-a-chip prototyping. , 2007, Lab on a chip.
[8] Roland Zengerle,et al. Microfluidic platforms for lab-on-a-chip applications. , 2007, Lab on a chip.
[9] T. Matsumura,et al. Cutting process of glass with inclined ball end mill , 2008 .
[10] Y. Kakinuma,et al. Micromachining of Soft Polymer Material applying Cryogenic Cooling , 2008 .
[11] Janez Kopac,et al. The influence of cryogenic cooling on process stability in turning operations , 2011 .