16 – Ageing of composite insulators

[1]  Polymeric outdoor insulation , 1990 .

[2]  J. Wańkowicz,et al.  Distribution of natural pollution surface layers on silicone rubber insulators and their UV absorption , 1989 .

[3]  R. Hackam,et al.  Suppression mechanism of leakage current on RTV coated porcelain and silicone rubber insulators , 1991 .

[4]  A. E. Vlastos,et al.  Surface structural changes of naturally aged silicone and EPDM composite insulators , 1991 .

[5]  G. George,et al.  Characterization of a severely degraded silicone elastomer HV insulator-an aid to development of lifetime assessment techniques , 2005, IEEE Transactions on Dielectrics and Electrical Insulation.

[6]  M. Kumosa,et al.  Failure analyses of nonceramic insulators. Part 1: Brittle fracture characteristics , 2005, IEEE Electrical Insulation Magazine.

[7]  M. Kumosa,et al.  Failure analyses of nonceramic insulators: part II - the brittle fracture model and failure prevention , 2005, IEEE Electrical Insulation Magazine.

[8]  S. Karlsson,et al.  Biofilms on silicone rubber insulators; microbial composition and diagnostics of removal by use of ESEM/EDS - Composition of biofilms infecting silicone rubber insulators , 2004 .

[9]  S. Gubanski,et al.  Deterioration of internal interfaces between silicone and epoxy resin , 2006, Conference Record of the 2006 IEEE International Symposium on Electrical Insulation.

[10]  R. Gorur,et al.  Mold growth on nonceramic insulators and its impact on electrical performance , 2003 .

[11]  R. Mcafee,et al.  A study of biological contaminants on high voltage porcelain insulators, I , 1997 .

[12]  S. Kumagai,et al.  Electrical and environmental aging of silicone rubber used in outdoor insulation , 1999, IEEE Transactions on Dielectrics and Electrical Insulation.

[13]  Ulf W. Gedde,et al.  Hydrophobicity Recovery of Polydimethylsiloxane after Exposure to Corona Discharges , 1998 .

[14]  J. T. Burnham,et al.  IEEE Task Force Report: brittle fracture in nonceramic insulators , 2002 .

[15]  S. Gubanski,et al.  Properties of interfaces in silicone rubber , 2007, IEEE Transactions on Dielectrics and Electrical Insulation.

[16]  E. Brocard,et al.  Determination of the Brittle Fracture Process of Field Failed HV Insulators , 2005 .

[17]  Kiyotaka Izumi,et al.  Survey on the use of non-ceramic composite insulators , 1999, IEEE Transactions on Dielectrics and Electrical Insulation.

[18]  C. A. Spellman,et al.  Survey of polymeric insulator ageing factors , 1999 .

[19]  R. Hackam Outdoor HV composite polymeric insulators , 1999, IEEE Transactions on Dielectrics and Electrical Insulation.

[20]  S. Gubanski,et al.  Effects of biological contamination on insulator performance , 2000, Proceedings of the 6th International Conference on Properties and Applications of Dielectric Materials (Cat. No.00CH36347).

[21]  W. Barthlott,et al.  Purity of the sacred lotus, or escape from contamination in biological surfaces , 1997, Planta.

[22]  H. M. Schneider,et al.  Water drop corona effects on full-scale 500 kV non-ceramic insulators , 1999 .

[23]  J. Lambrecht,et al.  Hydratization of the PDMS backbone during water immersion test , 1998, 1998 Annual Report Conference on Electrical Insulation and Dielectric Phenomena (Cat. No.98CH36257).

[24]  M. Kuhl,et al.  FRP rods for brittle fracture resistant composite insulators , 2001 .

[25]  Andreas Thomas Franz Wolf,et al.  Mould fungus growth on sanitary sealants , 1989 .

[26]  R. Hackam,et al.  The loss and recovery of hydrophobicity of RTV silicone rubber insulator coatings , 1990 .

[27]  J. Mackevich,et al.  Polymer outdoor insulating materials. Part I: Comparison of porcelain and polymer electrical insulation , 1997 .

[28]  I. Jandrell,et al.  Review of aging and recovery of silicone rubber insulation for outdoor use , 1999, IEEE Transactions on Dielectrics and Electrical Insulation.

[29]  Xidong Liang,et al.  Analysis of the acid sources of a field brittle fractured composite insulator , 2006, IEEE Transactions on Dielectrics and Electrical Insulation.

[30]  R. Gorur,et al.  Effect of long-term corona on non-ceramic outdoor insulator housing materials , 2001 .

[31]  M. A. R. M. Fernando,et al.  Performance of nonceramic insulators under tropical field conditions , 2000 .

[32]  Sigbritt Karlsson,et al.  Aging of silicone rubber under ac or dc voltages in a coastal environment , 2001 .

[33]  J. Looms Insulators for High Voltages , 1988 .

[34]  Grant D. Smith,et al.  Crosslinked polydimethylsiloxane exposed to oxygen plasma studied by neutron reflectometry and other surface specific techniques , 2000 .

[35]  G. B. Rackliffe,et al.  Performance Evaluation of 15-KV Polymeric Insulators for Dead-End Type Applications on Distribution Systems , 1989, IEEE Power Engineering Review.

[36]  N. Yoshimura,et al.  Polydimethylsiloxane and alumina trihydrate system subjected to dry-band discharges or high temperature part I: chemical structure , 2004, IEEE Transactions on Dielectrics and Electrical Insulation.

[37]  A. J. Phillips,et al.  Aging of nonceramic insulators due to corona from water drops , 1999 .

[38]  R. Gorur,et al.  Surface recovery of silicone rubber used for HV outdoor insulation , 1994 .

[39]  R. L. Brown,et al.  Flashover mechanism of silicone rubber insulators used for outdoor insulation-II , 1995 .

[40]  S. Gubanski,et al.  Wettability of naturally aged silicon and EPDM composite insulators , 1990 .

[41]  H. Hillborg,et al.  Hydrophobicity changes in silicone rubbers , 1999, IEEE Transactions on Dielectrics and Electrical Insulation.

[42]  R. Gorur,et al.  Impact of corona on the long-term performance of nonceramic insulators , 2003, IEEE Transactions on Dielectrics and Electrical Insulation.

[43]  E. Cherney,et al.  Thermal conductivity of filled silicone rubber and its relationship to erosion resistance in the inclined plane test , 2004, IEEE Transactions on Dielectrics and Electrical Insulation.