Assessing the effects of different dielectrics on environmentally conscious powder-mixed EDM of difficult-to-machine material (WC-Co)

Electrical discharge machining (EDM) is a well-known nontraditional manufacturing process to machine the difficult-to-machine (DTM) materials which have unique hardness properties. Researchers have successfully performed hybridization to improve this process by incorporating powders into the EDM process known as powder-mixed EDM process. This process drastically improves process efficiency by increasing material removal rate, micro-hardness, as well as reducing the tool wear rate and surface roughness. EDM also has some input parameters, including pulse-on time, dielectric levels and its type, current setting, flushing pressure, and so on, which have a significant effect on EDM performance. However, despite their positive influence, investigating the effects of these parameters on environmental conditions is necessary. Most studies demonstrate the use of kerosene oil as dielectric fluid. Nevertheless, in this work, the authors highlight the findings with respect to three different dielectric fluids, including kerosene oil, EDM oil, and distilled water using one-variable-at-a-time approach for machining as well as environmental aspects. The hazard and operability analysis is employed to identify the inherent safety factors associated with powder-mixed EDM of WC-Co.

[1]  Jagdeep Singh,et al.  Determination of multi-performance characteristics for powder mixed electric discharge machining of tungsten carbide alloy , 2016 .

[2]  Chitra Sharma,et al.  Research Developments in Additives Mixed Electrical Discharge Machining (AEDM): A State of Art Review , 2010 .

[3]  Stephen T. Newman,et al.  State of the art electrical discharge machining (EDM) , 2003 .

[4]  Muhammad P. Jahan,et al.  Modelling and experimental investigation on the effect of nanopowder-mixed dielectric in micro-electrodischarge machining of tungsten carbide , 2010 .

[5]  Reza Teimouri,et al.  Parametric study along with selection of optimal solutions in dry wire cut machining of cemented tungsten carbide (WC-Co) , 2013 .

[6]  Ramezanali Mahdavinejad,et al.  ED machining of WC-Co , 2005 .

[7]  Mahmudur Rahman,et al.  A review on the conventional and micro-electrodischarge machining of tungsten carbide , 2011 .

[8]  Y. Wong,et al.  Near-mirror-finish phenomenon in EDM using powder-mixed dielectric , 1998 .

[9]  Hamid Baseri,et al.  Experimental study of rotary magnetic field-assisted dry EDM with ultrasonic vibration of workpiece , 2013 .

[10]  Chitra Sharma,et al.  A Study of Multiobjective Parametric Optimization of Silicon Abrasive Mixed Electrical Discharge Machining of Tool Steel , 2010 .

[11]  M. L. Jeswani,et al.  Effect of the addition of graphite powder to kerosene used as the dielectric fluid in electrical discharge machining , 1981 .

[12]  Kuang-Yuan Kung,et al.  Material removal rate and electrode wear ratio study on the powder mixed electrical discharge machining of cobalt-bonded tungsten carbide , 2009 .

[13]  Yoke San Wong,et al.  Effects of flushing on electro-discharge machined surfaces , 1995 .

[14]  W. Zhao,et al.  The application of research on powder mixed EDM in rough machining , 2002 .

[15]  Abdulkadir Erden,et al.  A comparative study on the surface integrity of plastic mold steel due to electric discharge machining , 2005 .

[16]  Ching-Tien Lin,et al.  Electrical Discharge Machining (EDM) Characteristics Associated with Electrical Discharge Energy on Machining of Cemented Tungsten Carbide , 2008 .

[17]  Fei Liu,et al.  A decision-making framework model of cutting fluid selection for green manufacturing and a case study , 2002 .

[18]  F. Amorim,et al.  Aspects on the optimization of die-sinking EDM of tungsten carbide-cobalt , 2010 .

[19]  Wolfgang Dott,et al.  Electrical discharge machining: occupational hygienic characterization using emission-based monitoring. , 2006, International journal of hygiene and environmental health.

[20]  Agostino G. Bruzzone,et al.  Effect of Flushing and Electrode Material on Die Sinking EDM , 1999 .

[21]  M. Jose,et al.  Analysis of aerosol emission and hazard evaluation of electrical discharge machining (EDM) process. , 2010, Industrial health.

[22]  Wim Dewulf,et al.  Preliminary Environmental Assessment of Electrical Discharge Machining , 2011 .

[23]  S. H. Lee,et al.  Study of the effect of machining parameters on the machining characteristics in electrical discharge machining of tungsten carbide , 2001 .

[24]  I. Pashby,et al.  A review on the use of environmentally-friendly dielectric fluids in electrical discharge machining , 2004 .

[25]  Noriah Yusoff,et al.  Electrical Discharge Machining (EDM): Practices in Malaysian Industries and Possible Change towards Green Manufacturing , 2012 .

[26]  Yasuo Yamane,et al.  An Evaluation of Difficulty in Machining Difficult-to-Cut Materials by using Difficult-to-Cut Rating , 2004 .

[27]  Takahisa Masuzawa,et al.  Water-Based Dielectric Solution for EDM , 1983 .

[28]  Reza Kashiry Fard,et al.  Experimental investigation, intelligent modeling and multi-characteristics optimization of dry WEDM process of Al–SiC metal matrix composite , 2013 .

[29]  Sang Jo Lee,et al.  Improvement of surface integrity of electro-chemical discharge machining process using powder-mixed electrolyte , 2007 .

[30]  S. P. Sivapirakasam,et al.  Multi-attribute decision making for green electrical discharge machining , 2011, Expert Syst. Appl..

[31]  Masanori Kunieda,et al.  Advancing EDM through fundamental insight into the process , 2005 .

[32]  Jagdeep Singh,et al.  Effect of Powder Mixed Electrical Discharge Machining (PMEDM) on Difficult-to-machine Materials – a Systematic Literature Review , 2014 .

[33]  M. Ghoreishi,et al.  Statistical Modeling and Optimization of Process Parameters in Electro-Discharge Machining of Cobalt-Bonded Tungsten Carbide Composite (WC/6%Co) , 2013 .