Effect of Ga addition on the microstructure and magnetic properties of hydrogenation–disproportionation–desorption–recombination processed Nd–Fe–B powder
暂无分享,去创建一个
[1] M. Sagawa,et al. The origin of coercivity decrease in fine grained Nd-Fe-B sintered magnets , 2009 .
[2] H. Ohno,et al. 3DAP analysis of (Ga,Mn)As diluted magnetic semiconductor thin film. , 2009, Ultramicroscopy.
[3] T. Ohkubo,et al. Coercivity mechanism of hydrogenation disproportionation desorption recombination processed Nd–Fe–B based magnets , 2008 .
[4] Y. Shirai,et al. Relationship between Coercivity and Microstructural Changes During DR Treatment in the HDDR‐processed NdFeCoB Alloy , 2008 .
[5] D Lawrence,et al. In situ site-specific specimen preparation for atom probe tomography. , 2007, Ultramicroscopy.
[6] R. Langford,et al. Focused ion beams techniques for nanomaterials characterization , 2006, Microscopy research and technique.
[7] Y. Honkura,et al. Texture memory effect of Nd Fe B during hydrogen treatment , 2005 .
[8] K. F. Russell,et al. Strategies for fabricating atom probe specimens with a dual beam FIB. , 2005, Ultramicroscopy.
[9] K. Muller,et al. Memory of texture during HDDR processing of NdFeB , 2003, Digest of INTERMAG 2003. International Magnetics Conference (Cat. No.03CH37401).
[10] N. Tezuka,et al. Improvement of coercivity of anisotropic Nd-Fe-B HDDR powders by Ga addition , 2002 .
[11] N. Sano,et al. Intermediate hydrogenation phase in the hydrogenation–disproportionation–desorption–recombination process of Nd2Fe14B-based anisotropic magnets , 1999 .
[12] I. R. Harris,et al. Resistivity measurements on hydrogenation disproportionation desorption recombination phenomena in NdFeB alloys with Co, Ga and Zr additions , 1997 .
[13] I. R. Harris,et al. Fundamental and practical aspects of the hydrogenation, disproportionation, desorption and recombination process , 1996 .
[14] K. Morimoto,et al. Anisotropic Nd–Fe–B bonded magnets made from HDDR powders (invited) , 1996 .
[15] I. R. Harris,et al. Phase transformations during the disproportionation stage in the solid HDDR process in a Nd16Fe76B8 alloy , 1994 .
[16] D. Eckert,et al. The influence of particle size on the coercivity of sintered NdFeB magnets , 1991 .
[17] R. Ramesh,et al. Magnetization reversal in nucleation controlled magnets. II. Effect of grain size and size distribution on intrinsic coercivity of Fe‐Nd‐B magnets , 1988 .
[18] R. Ramesh,et al. Magnetization reversal in nucleation controlled magnets. I. Theory , 1988 .
[19] J. Livingston. Magnetic domains in sintered Fe‐Nd‐B magnets , 1985 .