Contribution to the Understanding of the Microstructure of First Generation Si‐C‐O Fibers

[1]  M. Jaffe,et al.  Characterization of Nicalon®: Strength, Structure, and Fractography , 2008 .

[2]  Tadanobu Inoue,et al.  Fracture Toughness of a Crystalline Silicon Carbide Fiber (Tyranno‐SA3®) , 2006 .

[3]  宏伸 市川 電子線照射不融化によるポリカルボシランからの高性能 SiC 繊維の開発 (総説) , 2006 .

[4]  A. Bunsell,et al.  A review of the development of three generations of small diameter silicon carbide fibres , 2006 .

[5]  P. Kroll Modeling the ‘free carbon’ phase in amorphous silicon oxycarbide , 2005 .

[6]  P. Scardi,et al.  Line broadening analysis using integral breadth methods: a critical review , 2004 .

[7]  P. Kroll Modelling and simulation of amorphous silicon oxycarbide , 2003 .

[8]  C. Labrugère,et al.  Characterization of nearly stoichiometric SiC ceramic fibres , 2001 .

[9]  A. Kohyama,et al.  Tensile strength and fracture surface characterization of Hi-Nicalon™ SiC fibers , 2001 .

[10]  T. Ishikawa,et al.  Fibre strength parameters measured in situ for ceramic-matrix composites tested at elevated temperature in vacuum and in air , 1999 .

[11]  A. Bunsell,et al.  Microstructural evolution of the latest generation of small‐diameter SiC‐based fibres tested at high temperatures , 1997 .

[12]  Lorenz S. Sigl,et al.  Effect of Interface Mechanical Properties on Pullout in a SiC‐Fiber‐Reinforced Lithium Aluminum Silicate Glass‐Ceramic , 1989 .

[13]  R. Bradt,et al.  Strength Distribution of Reinforcing Fibers in a Nicalon Fiber/Chemically Vapor Infiltrated Silicon Carbide Matrix Composite , 1989 .

[14]  L. Sawyer,et al.  Strength, structure, and fracture properties of ceramic fibers produced from polymeric precursors. I: Base-line studies , 1987 .

[15]  E. J. Mittemeijer,et al.  The determination of crystallite-size and lattice-strain parameters in conjunction with the profile-refinement method for the determination of crystal structures , 1983 .

[16]  D. G. Holloway,et al.  On the shape and size of the fracture zones on glass fracture surfaces , 1966 .

[17]  W. C. Levengood Effect of Origin Flaw Characteristics on Glass Strength , 1958 .

[18]  T. Ishikawa,et al.  Estimation of the fracture toughness of Tyranno Si-Ti-C-O fibres from flaw size and "fracture mirror" data measured in situ a 3-D woven SiC/SiC composite , 2001 .

[19]  R. E. Tressler,et al.  Microstructural instability and the resultant strength of SiCO (Nicalon) and SiNCO (HPZ) fibres , 1996 .

[20]  A. Jaras,et al.  Measurement of silicon carbide fibre strength in composites from studies of their fracture surfaces , 1993 .

[21]  A. Oberlin,et al.  Understanding Nicalon® fibre , 1993 .

[22]  J. L. Miquel,et al.  Study of Nicalon-based ceramic fibres and powders by EXAFS spectrometry, X-ray diffractometry and some additional methods , 1989 .

[23]  L. Porte,et al.  Evidence for a silicon oxycarbide phase in the Nicalon silicon carbide fibre , 1989 .

[24]  J. J. Mecholsky,et al.  Fractographic analysis of ceramics , 1978 .