Structural characteristics and ablative behavior of C/C–ZrC–SiC composites reinforced with “Z-pins like” Zr–Si–B–C multiphase ceramic rods

[1]  Wei Sun,et al.  Novel “Z-pins like” vanadium rods prepared by solid phase sintering to improve ablation resistance of the C/C-ZrC-SiC composites , 2019, Journal of the European Ceramic Society.

[2]  Zhi-jun,et al.  Preparation and Anti-oxidation Properties of HfB2-WB2-Si/SiC-SiCNW Composite Coating , 2017 .

[3]  Hongwei Liu,et al.  Effect of ZrC–SiC content on microstructure and ablation properties of C/C composites , 2016 .

[4]  Xue Feng,et al.  Formation mechanisms of characteristic structures on the surface of C/SiC composites subjected to thermal ablation , 2016 .

[5]  Hejun Li,et al.  Ablation behaviour of C/C and C/C–ZrC–SiC composites with cone-shaped holes under an oxyacetylene flame , 2016 .

[6]  Bingwei Lu,et al.  Bio‐Inspired Microstructure Design to Improve Thermal Ablation and Oxidation Resistance: Experiment on SiC , 2015 .

[7]  Elena Yazhenskikh,et al.  Viscosity model for oxide melts relevant to fuel slags. Part 1: Pure oxides and binary systems in the system SiO2–Al2O3–CaO–MgO–Na2O–K2O , 2015 .

[8]  LI Xiu-qia Preparation and Performance of ZrC / SiC Multi-components Modified C/C Composites , 2014 .

[9]  Xiaohong Shi,et al.  Ablation in different heat fluxes of C/C composites modified by ZrB2–ZrC and ZrB2–ZrC–SiC particles , 2013 .

[10]  Xinghong Zhang,et al.  Effects of oxygen partial pressure and atomic oxygen on the microstructure of oxide scale of ZrB2–SiC composites at 1500 °C , 2013 .

[11]  L. Chai,et al.  Microstructure and Mechanical Properties of C/C–ZrC–SiC Composites Fabricated by Reactive Melt Infiltration with Zr, Si Mixed Powders , 2013 .

[12]  H. Hu,et al.  Mechanism of ablation of 3D C/ZrC–SiC composite under an oxyacetylene flame , 2013 .

[13]  Lai-fei Cheng,et al.  Ablation properties of 2D C/SiC-ZrB 2 composite , 2012 .

[14]  Zhan Wei-gang,et al.  Ablation Performances of Multi-phased C/C-ZrC-SiC Ultra-high Temperature Composites , 2011 .

[15]  Hejun Li,et al.  Microstructures and Ablation Resistance of ZrC Coating for SiC-Coated Carbon/Carbon Composites Prepared by Supersonic Plasma Spraying , 2011 .

[16]  Zhang Weigang Self-Healing Oxidation Resistance of C/C Composite Covering a Broader Temperatures Range , 2011 .

[17]  X. Chun Formation Mechanism of Zircon Phase in ZrB_2-SiC Ceramic Composites during Oxidation , 2011 .

[18]  Yue Zhang,et al.  Oxidation of zirconium diboride–silicon carbide ceramics under an oxygen partial pressure of 200 Pa: Formation of zircon , 2010 .

[19]  G. Hilmas,et al.  Evolution of structure during the oxidation of zirconium diboride–silicon carbide in air up to 1500 °C , 2007 .

[20]  Zhai Ping ZIRCONIUM DIBORIDE-SILICON CARBIDE CERAMIC COMPOSITES , 2006 .

[21]  Guo‐Jun Zhang,et al.  Boron carbide and nitride as reactants for in situ synthesis of boride-containing ceramic composites , 2004 .

[22]  Guo‐Jun Zhang,et al.  Reactive Hot Pressing of ZrB2–SiC Composites , 2004 .

[23]  Tang Jian Diffusion Path and Reaction Mechanism between Ti and B_4C , 2000 .

[24]  G. Karniadakis,et al.  Simulation of Heat and Momentum Transfer in Complex Microgeometries , 1994 .

[25]  W. L. Vaughn,et al.  Active‐to‐Passive Transition in the Oxidation of Silicon Carbide and Silicon Nitride in Air , 1990 .