Crosspoint Localization of Spiral and Girth Welds of Spiral Steel Pipelines

Crosspoint of spiral and girth welds of spiral steel pipelines transporting high-pressure oil and gas is easy to crack due to welding defects and corrosion, so routine excavation and careful inspection are required. In order to reduce the workload and cost of excavation, it is necessary to determine the crosspoint’s angular position on the girth weld. This article proposes a low-cost and high-efficiency method for locating the spiral-girth weld crosspoint based on the inner Spherical Detector (SD). Theoretical analysis and experiments demonstrate that the magnetometer with a smaller lift-off could detect more noticeable magnetic valley of the spiral welds at the pipe bottom, so a smaller SD should be used; the spiral direction can be determined by the phase difference of the dual-channel magnetic signals, when dual magnetometers are symmetrically fixed about the median vertical plane on the rotation axis of the SD. When the girth weld, at least one spiral weld and the spiral direction are detected and determined, the crosspoint’s angular position can be calculated. The maximum localization error of the crosspoint is less than 30° and the average error is less than 20°, that is, no more than one hour’s angle, whose accuracy is sufficient for excavation and maintenance in the field, because it will reduce the amount of excavation by nearly half.

[1]  Zhili Feng,et al.  Numerical analysis of residual stress distribution in tubes with spiral weld cladding , 1998 .

[2]  Wim De Waele,et al.  A comprehensive study on the microstructure and mechanical properties of arc girth welded joints of spiral welded high strength API X70 steel pipe , 2020, Archives of Civil and Mechanical Engineering.

[3]  Mehdi Behzad,et al.  CFD–DEM approach to investigate the effect of drill pipe rotation on cuttings transport behavior , 2015 .

[4]  Jun Zhang,et al.  A Review of Passive RFID Tag Antenna-Based Sensors and Systems for Structural Health Monitoring Applications , 2017, Sensors.

[5]  S. Tu,et al.  Effect of helix angle on residual stress in the spiral welded oil pipelines: Experimental and finite element modeling , 2018, International Journal of Pressure Vessels and Piping.

[6]  Laurie E. Collins,et al.  Evaluation of UOE and Spiral-Welded Line Pipe for Strain Based Designs , 2010 .

[7]  Jae-Yeol Kim,et al.  Application of Ultrasonic Test System for Test Performance Improvement of Welding Flaw , 2006 .

[8]  Spyros A. Karamanos,et al.  The effect of spiral cold-bending manufacturing process on pipeline mechanical behavior , 2016, International Journal of Solids and Structures.

[9]  Jian Chen,et al.  Research on Burst Tests of Pipeline With Spiral Weld Defects , 2012 .

[10]  G. Chirikjian,et al.  A 3D Localization Approach for Subsea Pipelines Using a Spherical Detector , 2017, IEEE Sensors Journal.

[11]  Yao Wei EVOLUTION OF TRIAX MAGNETIC FLUX LEAKAGE INSPECTION FOR MITIGATION OF SPIRAL WELD ANOMALIES , 2011 .

[12]  Li Jian,et al.  Vibration Detection of Spanning Subsea Pipelines by Using a Spherical Detector , 2019, IEEE Access.

[13]  Yu Zhang,et al.  CFD and Experimental Investigations of Drag Force onSpherical Leak Detector in Pipe Flows at High ReynoldsNumber , 2014 .

[14]  W. Marsden I and J , 2012 .

[15]  Simon Labbé,et al.  Special Phased Array Applications for Pipeline Girth Weld Inspections , 2004 .

[16]  Gethin Wyn Roberts,et al.  Low-cost IMU and odometer tightly coupled integration with Robust Kalman filter for underground 3-D pipeline mapping , 2019, Measurement.

[17]  Mohammad A. Jaradat,et al.  Inertial Navigation System of Pipeline Inspection Gauge , 2020, IEEE Transactions on Control Systems Technology.

[19]  G. Tian,et al.  Residual magnetic field sensing for stress measurement , 2007 .

[20]  Konrad Reber Eddy Current Testing in Pipeline Inspection , 2015 .

[21]  L. Mingze,et al.  Lateral Pipeline Buckling Detection via Demagnetization and Interior Magnetic Measurement , 2020, IEEE Access.

[22]  Xu Chen,et al.  A comparison between fracture toughness at different locations of longitudinal submerged arc welded and spiral submerged arc welded joints of API X80 pipeline steels , 2015 .

[23]  Qingshan Feng,et al.  Preliminary Failure Assessment for Spiral Welded Defects of Pipeline , 2008 .