Structure and Formation Mechanism of Surface Film of Ag-MoS2 Composite during Electrical Sliding Wear
暂无分享,去创建一个
F. Yi | W. Juan | L. Shu | Chen Shuxian | Yang Xi-ting
[1] Izhak Etsion,et al. Friction and wear of MoS2 films on laser textured steel surfaces , 2008 .
[2] K. Wong,et al. Surface and friction characterization of MoS2 and WS2 third body thin films under simulated wheel/rail rolling–sliding contact , 2008 .
[3] Aykut Canakci,et al. The effect of brush spring pressure on the wear behaviour of copper-graphite brushes with electrical current , 2007 .
[4] T. M. Yue,et al. Laser cladding of copper with molybdenum for wear resistance enhancement in electrical contacts , 2007 .
[5] Jiajun Liu,et al. Molybdenum disulfide coating deposited by hybrid treatment and its friction-reduction performance , 2007 .
[6] Ping Liu,et al. Sliding wear behavior of copper alloy contact wire against copper-based strip for high-speed electrified railways , 2007 .
[7] J. Bressan,et al. Study of wear in self-lubricating composites for application in seals of electric motors , 2006 .
[8] Wang Ke,et al. The influence of unidirectional pressure on electrical conductivity of carbon black filled polyethylene , 2006 .
[9] K. Wahl,et al. Preparation of chameleon coatings for space and ambient environments , 2006 .
[10] Niu Zhi-chuan,et al. Optical characteristics of InAs quantum dots on GaAs matrix by using various InGaAs structures , 2006 .
[11] Feng Yi,et al. Effect of the electric current on the friction and wear properties of the CNT–Ag–G composites , 2005 .
[12] M. Ozaki,et al. Perylene derivative sensitized multi-walled carbon nanotube thin film , 2005 .
[13] Ali Erdemir,et al. Historical developments and new trends in tribological and solid lubricant coatings. , 2004 .