Crystallographic orientation control of pure chromium via laser powder bed fusion and improved high temperature oxidation resistance

[1]  T. Ishimoto,et al.  Crystallographic Orientation Control of 316L Austenitic Stainless Steel via Selective Laser Melting , 2020 .

[2]  T. Nakano,et al.  Additive manufacturing of dense components in beta‑titanium alloys with crystallographic texture from a mixture of pure metallic element powders , 2019, Materials & Design.

[3]  D. Kong,et al.  Corrosion of metallic materials fabricated by selective laser melting , 2019, npj Materials Degradation.

[4]  Dong-Ik Kim,et al.  Role of grain boundary engineered microstructure on high temperature steam oxidation behaviour of Ni based superalloy alloy 617 , 2019, Journal of Alloys and Compounds.

[5]  K. Hagihara,et al.  Excellent mechanical and corrosion properties of austenitic stainless steel with a unique crystallographic lamellar microstructure via selective laser melting , 2019, Scripta Materialia.

[6]  M. Elbestawi,et al.  Effect of Selective Laser Melting Process Parameters on the Quality of Al Alloy Parts: Powder Characterization, Density, Surface Roughness, and Dimensional Accuracy , 2018, Materials.

[7]  Chaofang Dong,et al.  Bio-functional and anti-corrosive 3D printing 316L stainless steel fabricated by selective laser melting , 2018, Materials & Design.

[8]  X. Wang,et al.  Effects of grain sizes on the oxidation behavior of Ni-based alloy 230 and N , 2018, Journal of Alloys and Compounds.

[9]  T. Nakano,et al.  Influence of unique layered microstructure on fatigue properties of Ti-48Al-2Cr-2Nb alloys fabricated by electron beam melting , 2018 .

[10]  K. Hagihara,et al.  Effect of scanning strategy on texture formation in Ni-25 at.%Mo alloys fabricated by selective laser melting , 2018 .

[11]  Shu Beng Tor,et al.  Anisotropy and heterogeneity of microstructure and mechanical properties in metal additive manufacturing: A critical review , 2018 .

[12]  A. Rollett,et al.  A Comprehensive Comparison of the Analytical and Numerical Prediction of the Thermal History and Solidification Microstructure of Inconel 718 Products Made by Laser Powder-Bed Fusion , 2017 .

[13]  W. Xiong,et al.  Grain Structure Control of Additively Manufactured Metallic Materials , 2017, Materials.

[14]  K. Hagihara,et al.  Crystallographic texture control of beta-type Ti–15Mo–5Zr–3Al alloy by selective laser melting for the development of novel implants with a biocompatible low Young's modulus , 2017 .

[15]  K. Hagihara,et al.  Successful additive manufacturing of MoSi2 including crystallographic texture and shape control , 2017 .

[16]  B. Jönsson,et al.  Oxidation Comparison of Alumina-Forming and Chromia-Forming Commercial Alloys at 1100 and 1200 °C , 2017, Oxidation of Metals.

[17]  K. Chou,et al.  Full length articleStress and deformation evaluations of scanning strategy effect in selective laser melting , 2016 .

[18]  Bo Cheng,et al.  Stress and deformation evaluations of scanning strategy effect in selective laser melting , 2016 .

[19]  H. Liao,et al.  Microstructure and wear behavior of in-situ hypereutectic Al–high Si alloys produced by selective laser melting , 2016 .

[20]  Yan Zhou,et al.  A novel titanium alloy manufactured by selective laser melting: Microstructure, high temperature oxidation resistance , 2016 .

[21]  H L Wei,et al.  Evolution of solidification texture during additive manufacturing , 2015, Scientific Reports.

[22]  X. Wang,et al.  Influence of grain orientation on the incipient oxidation behavior of Haynes 230 at 900 °C , 2015 .

[23]  K. Yi,et al.  The role of grain boundaries in the initial oxidation behavior of austenitic stainless steel containing alloyed Cu at 700 °C for advanced thermal power plant applications , 2015 .

[24]  S. Samal,et al.  Influence of Grain Shape, Size, and Grain Boundary Diffusion on High-Temperature Oxidation of Pure Metal Fe, Cu, and Zn , 2015, Metallurgical and Materials Transactions A.

[25]  Yunping Li,et al.  Effects of alloyed Si on the oxidation behaviour of Co–29Cr–6Mo alloy for solid-oxide fuel cell interconnects , 2015 .

[26]  Yuichiro Koizumi,et al.  Phase and grain size inhomogeneity and their influences on creep behavior of Co–Cr–Mo alloy additive manufactured by electron beam melting , 2015 .

[27]  Zhi-Gang Yang,et al.  Effect of grain size on the oxidation of Fe–13Cr–5Ni alloy at 973 K in Ar–21 vol%O2 , 2015 .

[28]  D. Gu,et al.  Selective laser melting additive manufactured Inconel 718 superalloy parts: High-temperature oxidation property and its mechanisms , 2014 .

[29]  H. Sun,et al.  High temperature corrosion behavior of Cu–20Co–30Cr alloys with different grain size , 2014 .

[30]  D. Gu,et al.  Selective laser melting additive manufacturing of Inconel 718 superalloy parts: Densification, microstructure and properties , 2014 .

[31]  S. Chevalier What did we learn on the reactive element effect in chromia scale since Pfeil's patent? , 2014 .

[32]  Ming-Chuan Leu,et al.  Additive manufacturing: technology, applications and research needs , 2013, Frontiers of Mechanical Engineering.

[33]  M. Sun,et al.  The high-temperature oxidation of bulk nanocrystalline 304 stainless steel in air , 2013 .

[34]  L. Höglund,et al.  High temperature oxidation of chromium: Kinetic modeling and microstructural investigation , 2013 .

[35]  M. P. Phaniraj,et al.  Effect of grain boundary characteristics on the oxidation behavior of ferritic stainless steel , 2011 .

[36]  J. Svensson,et al.  Oxidation of Binary FeCr Alloys (Fe–2.25Cr, Fe–10Cr, Fe–18Cr and Fe–25Cr) in O2 and in O2 + H2O Environment at 600 °C , 2011 .

[37]  X. Ledoux,et al.  On the Oxidation and Nitridation of Chromium at 1300 °C , 2010 .

[38]  M. Frary,et al.  Effects of crystallographic orientation on the early stages of oxidation in nickel and chromium , 2010 .

[39]  U. Krupp,et al.  Grain-Size Effects on the High-Temperature Oxidation Behaviour of Chromium Steels , 2010 .

[40]  T. Pollock,et al.  Microstructural evolution and failure characteristics of a NiCoCrAlY bond coat in “hot spot” cyclic oxidation , 2009 .

[41]  H. Fraser,et al.  Effects of process variables and size-scale on solidification microstructure in beam-based fabrication of bulky 3D structures , 2009 .

[42]  Yifu Shen,et al.  Effects of processing parameters on consolidation and microstructure of W–Cu components by DMLS , 2009 .

[43]  T. Narushima,et al.  Oxidation or Nitridation Behavior of Pure Chromium and Chromium Alloys Containing 10 mass%Ni or Fe in Atmospheric Heating , 2006 .

[44]  Todd R. Allen,et al.  The effect of grain boundary engineering on the oxidation behavior of INCOLOY alloy 800H in supercritical water , 2006 .

[45]  H. Harada,et al.  Chromium and chromium-based alloys: Problems and possibilities for high-temperature service , 2004 .

[46]  J. Szpunar,et al.  Grain boundary character distribution in oxides formed on (100) and (111) nickel single crystals coated with ceria gel , 1999 .

[47]  Y. Igarashi,et al.  Structure-dependent intergranular oxidation in Ni–Fe polycrystalline alloy , 1999 .

[48]  A. Garbacz,et al.  The relationship between texture and CSL boundaries distribution in polycrystalline materials—II. Analysis of the relationship between texture and coincidence grain boundary distribution , 1993 .

[49]  K. Arai,et al.  Grain boundaries in rapidly solidified and annealed Fe-6.5 mass% Si polycrystalline ribbons with high ductility , 1989 .

[50]  D. Baer,et al.  Differences in oxides on large-and small-grained 304 stainless steel , 1980 .

[51]  K. Lillerud,et al.  On High Temperature Oxidation of Chromium II . Properties of and the Oxidation Mechanism of Chromium , 1980 .

[52]  G. Sproule,et al.  Effect of oxide grain structure on the high-temperature oxidation of Cr , 1975 .

[53]  A. Gilbert Metallurgy of Chromium , 1968, Nature.

[54]  P. Footner,et al.  Oxidation of Iron–Chromium Binary Alloys , 1967, Nature.

[55]  D. Brandon,et al.  The structure of high-angle grain boundaries , 1966 .

[56]  C. Sims The Case for Chromium , 1963 .

[57]  A. T. Gwathmey,et al.  The structure of oxide films on different faces of a single crystal of copper , 1956 .

[58]  B. Lustman The Rate of Film Formation on Metals , 1942 .

[59]  Bhaskar Dutta,et al.  Additive Manufacturing Technology , 2016 .

[60]  M. Galetz,et al.  Factors affecting isothermal oxidation of pure chromium in air , 2018 .

[61]  K. Hagihara,et al.  Effect of building direction on the microstructure and tensile properties of Ti-48Al-2Cr-2Nb alloy additively manufactured by electron beam melting , 2017 .

[62]  S. P. Chenakin Initial oxidation kinetics of FeNi single crystals before and after ion bombardment , 1995 .

[63]  H. Araki,et al.  The effect of grain size on the corrosion behaviour of inconel 600 in high-temperature steam , 1981 .