Creep and fracture behavior of as-cast Mg–11Y–5Gd–2Zn–0.5Zr (wt%)
暂无分享,去创建一个
W. Ding | C. Boehlert | D. Yin | Q. D. Wang
[1] M. F. Ashby,et al. CREEP DAMAGE MECHANICS AND MICROMECHANISMS , 2013 .
[2] Qudong Wang,et al. The elevated-temperature mechanical behavior of peak-aged Mg–10Gd–3Y–0.4Zr Alloy , 2011 .
[3] Qudong Wang,et al. Effects of heat treatments on microstructure and mechanical properties of Mg–11Y–5Gd–2Zn–0.5Zr (wt.%) alloy , 2011 .
[4] M. Celikin,et al. Creep resistance in magnesium alloys , 2010 .
[5] Yuman Zhu,et al. The 18R and 14H long-period stacking ordered structures in Mg–Y–Zn alloys , 2010 .
[6] Qudong Wang,et al. Thermal properties of Mg–11Y–5Gd–2Zn–0.5Zr (wt.%) alloy , 2009 .
[7] Qudong Wang,et al. Microstructure and creep behavior of the extruded Mg–4Y–4Sm–0.5Zr alloy , 2009 .
[8] Qudong Wang,et al. Comparison of microstructure in Mg–10Y–5Gd–0.5Zr and Mg–10Y–5Gd–2Zn–0.5Zr alloys by conventional casting , 2009 .
[9] Weijia Tao,et al. Creep deformation mechanism of magnesium-based alloys , 2008 .
[10] B. Smola,et al. Creep behaviour of the creep resistant MgY3Nd2Zn1Mn1 alloy , 2008 .
[11] C. Boehlert,et al. Comparison of the Microstructure, Tensile, and Creep Behavior for Ti-24Al-17Nb-0.66Mo (Atomic Percent) and Ti-24Al-17Nb-2.3Mo (Atomic Percent) Alloys , 2007 .
[12] C. Boehlert. The tensile and creep behavior of Mg–Zn Alloys with and without Y and Zr as ternary elements , 2007 .
[13] Qudong Wang,et al. Effects of strontium and titanium on the microstructure, tensile properties and creep behavior of AM50 alloys , 2007 .
[14] W. Ding,et al. Precipitation in a Mg–10Gd–3Y–0.4Zr (wt.%) alloy during isothermal ageing at 250 °C , 2006 .
[15] Daniel B. Miracle,et al. In situ scanning electron microscopy observations of tensile deformation in a boron-modified Ti–6Al–4V alloy , 2006 .
[16] C. Boehlert,et al. The microstructure, tensile properties, and creep behavior of Mg-Zn alloys containing 0-4.4 wt.% Zn , 2006 .
[17] H. Somekawa,et al. Dislocation creep behavior in Mg–Al–Zn alloys , 2005 .
[18] B. Mordike,et al. Mechanisms of creep deformation in Mg-Sc-based alloys , 2005 .
[19] T. Mukai,et al. High temperature compressive properties over a wide range of strain rates in an AZ31 magnesium alloy , 2005 .
[20] A. Luo. Recent magnesium alloy development for elevated temperature applications , 2004 .
[21] H. Friedrich,et al. Newly developed magnesium alloys for powertrain applications , 2003 .
[22] M. E. Kassner,et al. Creep cavitation in metals , 2003 .
[23] K. Maruyama,et al. Creep deformation behavior and dislocation substructures of Mg–Y binary alloys , 2001 .
[24] J. G. Wang,et al. Creep of a heat treated Mg–4Y–3RE alloy , 2001 .
[25] S. Kamado,et al. Creep properties of Mg-Gd-Y-Zr alloys , 2001 .
[26] B. Mordike,et al. Magnesium: Properties — applications — potential , 2001 .
[27] K. Kainer. Verfahren und Produkte , 1997, HTM Journal of Heat Treatment and Materials.
[28] B. Muddle,et al. Characterisation of strengthening precipitate phases in a Mg–Y–Nd alloy , 2000 .
[29] D. Dunand,et al. Monkman-grant analysis of creep fracture in dispersion-strengthened and particulate-reinforced aluminum , 1999 .
[30] K. Maruyama,et al. Creep behavior and deformation microstructures of Mg–Y alloys at 550 K , 1998 .
[31] E. Aghion,et al. Creep studies of coarse-grained AZ91D magnesium castings , 1998 .
[32] V. Sklenička. High temperature intergranular damage and fracture , 1997 .
[33] Yiu-Wing Mai,et al. Advances in Fracture Research , 1997 .
[34] A. Luo,et al. Cast magnesium alloys for elevated temperature applications , 1994 .
[35] D. Northwood,et al. Strain-hardening and recovery during the creep of pure polycrystalline magnesium , 1994 .
[36] W. Miller. Creep of die cast AZ91 magnesium at room temperature and low stress , 1991 .
[37] G. Sundararajan. The Monkman-Grant relationship , 1989 .
[38] F. Povolo. Comments on the Monkman-Grant and the modified Monkman-Grant relationships , 1985 .
[39] I. Chen. Cavity growth on a sliding grain boundary , 1983 .
[40] T. Langdon,et al. Deformation mechanisms in h.c.p. metals at elevated temperatures—II. Creep behavior of a Mg-0.8% Al solid solution alloy , 1982 .
[41] T. Langdon,et al. Deformation mechanisms in h.c.p. metals at elevated temperatures—I. Creep behavior of magnesium , 1981 .
[42] J. E. Morgan,et al. An investigation into creep-resistant, as-cast magnesium alloys containing yttrium, zinc, neodymium and zirconium , 1981 .
[43] J. Čadek,et al. High temperature creep mechanisms in magnesium , 1970 .
[44] D. Miannay,et al. Time-Dependent Fracture Mechanics , 2001 .
[45] M. E. Kassner,et al. Five-power-law creep in single phase metals and alloys , 2000 .
[46] E. Aghion,et al. Dislocation analysis of crept AZ91D ingot castings , 1998 .