Effects of solution treatment before extrusion on the microstructure, mechanical properties and corrosion of Mg-Zn-Gd alloy in vitro

[1]  M. Dargusch,et al.  Influence of surface condition on the corrosion of ultra-high-purity Mg alloy wire , 2016 .

[2]  M. Dargusch,et al.  Stress corrosion cracking of several hot-rolled binary Mg-X alloys , 2015 .

[3]  E. Han,et al.  In vitro corrosion of as-extruded Mg–Ca alloys—The influence of Ca concentration , 2015 .

[4]  D. Zander,et al.  Influence of Ca and Zn on the microstructure and corrosion of biodegradable Mg–Ca–Zn alloys , 2015 .

[5]  C. Dong,et al.  Effect of heat treatment on the corrosion resistance and mechanical properties of an as-forged Mg–Zn–Y–Zr alloy , 2015 .

[6]  Xing-gang Li,et al.  Microstructure and phase transformation of as-cast and annealed Mg–4Zn–1Y alloy containing quasi-crystal phase , 2015, Rare Metals.

[7]  M. Dargusch,et al.  Influence of hot rolling on the corrosion behavior of several Mg–X alloys , 2015 .

[8]  W. Ding,et al.  Formation mechanism of quasicrystals at the nanoscale during hot compression of Mg alloys , 2014 .

[9]  Yufeng Zheng,et al.  Corrosion and characterisation of dual phase Mg–Li–Ca alloy in Hank’s solution: The influence of microstructural features , 2014 .

[10]  X. L. Liu,et al.  The effect of double extrusion on the microstructure and mechanical properties of Mg–Zn–Ca alloy , 2013 .

[11]  Yunping Li,et al.  Effect of pretreatment and annealing on microstructure and mechanical properties of Mg–1.5Zn–0.25Gd (at%) alloys reinforced with quasicrystal , 2013 .

[12]  W. Ding,et al.  Excellent mechanical properties of an ultrafine-grained quasicrystalline strengthened magnesium alloy with multi-modal microstructure , 2013 .

[13]  W. Ding,et al.  Microstructure and mechanical properties of as-cast and solution-treated Mg-Zn-Gd-based alloys reinforced with quasicrystals , 2013 .

[14]  Jun Luo,et al.  Effects of trace Gd concentration on texture and mechanical properties of hot-rolled Mg–2Zn–xGd sheets , 2013 .

[15]  W. Ding,et al.  Effect of Icosahedral Quasicrystalline Fraction and Extrusion Ratio on Microstructure, Mechanical Properties, and Anisotropy of Mg-Zn-Gd-Based Alloys , 2013, Metallurgical and Materials Transactions A.

[16]  E. Han,et al.  The effect of Zn concentration on the corrosion behavior of Mg-xZn alloys , 2012 .

[17]  H. Kato,et al.  The effect of nanoquasicrystals on mechanical properties of as-extruded Mg-Zn-Gd alloy , 2012 .

[18]  Chao Xu,et al.  Ultra high-strength Mg–Gd–Y–Zn–Zr alloy sheets processed by large-strain hot rolling and ageing , 2012 .

[19]  Baoping Zhang,et al.  Effects of calcium on texture and mechanical properties of hot-extruded Mg–Zn–Ca alloys , 2012 .

[20]  W. Ding,et al.  Effects of extrusion and heat treatment on the mechanical properties and biocorrosion behaviors of a Mg-Nd-Zn-Zr alloy. , 2012, Journal of the mechanical behavior of biomedical materials.

[21]  K. Hagihara,et al.  Effect of multimodal microstructure evolution on mechanical properties of Mg–Zn–Y extruded alloy , 2011 .

[22]  E. Han,et al.  Excellent room-temperature ductility and formability of rolled Mg–Gd–Zn alloy sheets , 2011 .

[23]  Yingwei Song,et al.  Influences of the quantity of Mg2Sn phase on the corrosion behavior of Mg–7Sn magnesium alloy , 2011 .

[24]  M. Escudero,et al.  Corrosion behaviour of AZ31 magnesium alloy with different grain sizes in simulated biological fluids. , 2010, Acta biomaterialia.

[25]  A. Singh,et al.  Rare-earth free wrought-processed magnesium alloy with dispersion of quasicrystal phase , 2009 .

[26]  Jie Zhou,et al.  Effects of ECAE temperature and billet orientation on the microstructure, texture evolution and mechanical properties of a Mg–Zn–Y–Zr alloy , 2009 .

[27]  M. Liu,et al.  Influence of pH and chloride ion concentration on the corrosion of Mg alloy ZE41 , 2008 .

[28]  L. Wagner,et al.  The relation between microstructure and corrosion behavior of AZ80 Mg alloy following different extrusion temperatures , 2008 .

[29]  W. Ding,et al.  Effects of extrusion on the microstructure and mechanical properties of Mg–Zn–Gd alloy reinforced with quasicrystalline particles , 2008 .

[30]  W. Ding,et al.  Effect of heat treatment on corrosion and electrochemical behaviour of Mg–3Nd–0.2Zn–0.4Zr (wt.%) alloy , 2007 .

[31]  W. Ding,et al.  Stable icosahedral phase in Mg-Zn-Gd alloy , 2006 .

[32]  Huang Yujian,et al.  Corrosion resistance properties of electroless nickel composite coatings , 2004 .

[33]  K. Maruyama,et al.  The activity of non-basal slip systems and dynamic recovery at room temperature in fine-grained AZ31B magnesium alloys , 2003 .

[34]  Barry L. Mordike,et al.  Structural aspects of high performance Mg alloys design , 2002 .

[35]  T. Mukai,et al.  Ductility enhancement in AZ31 magnesium alloy by controlling its grain structure , 2001 .

[36]  G. Song,et al.  Corrosion behaviour of AZ21, AZ501 and AZ91 in sodium chloride , 1998 .