Assessment of three oxide/oxide ceramic matrix composites: Mechanical performance and effects of heat treatments

[1]  Thomas Behrendt,et al.  Development and Validation of Oxide/Oxide CMC Combustors Within the HiPOC Program , 2013 .

[2]  I. Kuběna,et al.  Strength, elasticity and failure of composites with pyrolyzed matrices based on polymethylsiloxane resins with optimized ratio of D and T components , 2013 .

[3]  R. Hay,et al.  Creep of Nextel™ 610 Fiber at 1100°C in Air and in Steam , 2013 .

[4]  M. Friess,et al.  Influence of Fiber Fabric Density and Matrix Fillers as well as Fiber Coating on the Properties of OXIPOL Materials , 2012 .

[5]  P. Mechnich,et al.  Degradation of oxide fibers by thermal overload and environmental effects , 2012 .

[6]  D. Koch,et al.  Experimental and numerical evaluation of bending and tensile behaviour of carbon-fibre reinforced SiC , 2012 .

[7]  M. Gerendás,et al.  Design and Development Approach for Gas Turbine Combustion Chambers Made of Oxide Ceramic Matrix Composites , 2011 .

[8]  M. Balasubramanian,et al.  Effect of intermediate heat treatment on mechanical properties of SiCf/SiC composites with BN interphase prepared by ICVI , 2011 .

[9]  Anilesh Kumar,et al.  Investigation of effect of siliconization conditions on mechanical properties of 3D-stitched C–SiC composites , 2011 .

[10]  P. Mechnich,et al.  Improving the Microstructural Stability of Nextel™ 610 Alumina Fibers Embedded in a Porous Alumina Matrix , 2010 .

[11]  Robert L. Smith,et al.  Estimation of fracture energy from the work of fracture and fracture surface area: I. Stable crack growth , 2009 .

[12]  Lai-fei Cheng,et al.  Comparison of the mechanical hysteresis of carbon/ceramic-matrix composites with different fiber preforms , 2009 .

[13]  J. Yang,et al.  Control of Interface Properties in Oxide Composites Via Fugitive Coatings , 2008 .

[14]  S. Mall,et al.  Frequency effects on fatigue behavior of Nextel720™/alumina at room temperature , 2008 .

[15]  G. Motz,et al.  The PIP‐Process: Precursor Properties and Applications , 2008 .

[16]  R. Hay,et al.  Precipitation Coating of Monazite on Woven Ceramic Fibers: II. Effect of Processing Conditions on Coating Morphology and Strength Retention of Nextel™ 610 and 720 Fibers , 2008 .

[17]  A. Boccaccini,et al.  Crack resistance curve in glass matrix composite reinforced by long Nicalon® fibres , 2008, Journal of Materials Science.

[18]  P. Mechnich,et al.  Microstructural Coarsening of Nextel™ 610 Fibers Embedded in Alumina-Based Matrices , 2008 .

[19]  D. Wilson,et al.  High Temperature Properties of Nextel 610 and Alumina‐Based Nanocomposite Fibers , 2008 .

[20]  Stefan Hackemann,et al.  WHIPOX®: Ein faserverstärkter oxidkeramischer Werkstoff für Hochtemperatur– Langzeitanwendungen , 2007 .

[21]  M. Ruggles‐Wrenn,et al.  Influence of hold times on the elevated-temperature fatigue behavior of an oxide–oxide ceramic composite in air and in steam environment , 2007 .

[22]  S. Mall,et al.  Effects of steam environment on high-temperature mechanical behavior of NextelTM720/alumina (N720/A) continuous fiber ceramic composite , 2006 .

[23]  F. Zok Developments in Oxide Fiber Composites , 2006 .

[24]  D. Stöver,et al.  Carbon-fibre-reinforced carbon composite filled with SiC particles forming a porous matrix , 2006 .

[25]  H. Schneider,et al.  Temperature Stability of 3M Nextel™ 610, 650, and 720 Fibers ‐ A Microstructural Study , 2006 .

[26]  Reinhard A. Simon Progress in Processing and Performance of Porous‐Matrix Oxide/Oxide Composites , 2005 .

[27]  A. R. Boccaccini,et al.  Fracture behaviour of mullite fibre reinforced–mullite matrix composites under quasi-static and ballistic impact loading , 2005 .

[28]  Carlos G. Levi,et al.  Processing and Performance of an All‐Oxide Ceramic Composite , 2005 .

[29]  K. Chawla,et al.  Thermal degradation of fiber coatings in mullite-fiber-reinforced mullite composites , 2005 .

[30]  R. John,et al.  Stresses Due to Temperature Gradients in Ceramic‐Matrix‐Composite Aerospace Components , 2004 .

[31]  Stephen W. Freiman,et al.  Correlation of Fracture Toughness and Strength , 2004 .

[32]  X. Gong,et al.  In-Plane Mechanical Properties of an All-Oxide Ceramic Composite , 2004 .

[33]  J. Yang,et al.  Effects of Thermal Aging on the Mechanical Properties of a Porous‐Matrix Ceramic Composite , 2004 .

[34]  L. Zawada,et al.  Performance of Four Ceramic‐Matrix Composite Divergent Flap Inserts Following Ground Testing on an F110 Turbofan Engine , 2004 .

[35]  A. Demir,et al.  Mechanical property improvements in Nicalon SiC fibre reinforced silicon nitride ceramics by oxide coating of Si3N4 starting powders , 2004 .

[36]  Theodoros Loutas,et al.  On the identification of the failure mechanisms in oxide/oxide composites using acoustic emission , 2003 .

[37]  L. Zawada,et al.  Consequence of Intermittent Exposure to Moisture and Salt Fog on the High‐Temperature Fatigue Durability of Several Ceramic‐Matrix Composites , 2003 .

[38]  R. Hay,et al.  Characterization and High‐Temperature Mechanical Behavior of an Oxide/Oxide Composite , 2003 .

[39]  P. Cantonwine Strength of thermally exposed alumina fibers Part II bundle behavior , 2003 .

[40]  P. Cantonwine Strength of thermally exposed alumina fibers Part I Single filament behavior , 2003 .

[41]  R. Chen,et al.  Mechanical properties of Al2O3/ZrO2 composites , 2002 .

[42]  W. Curtin,et al.  Stress Rupture in Ceramic-Matrix Composites: Theory and Experiment , 2002 .

[43]  D. Wilson,et al.  High performance oxide fibers for metal and ceramic composites , 2001 .

[44]  H. Schneider,et al.  Effect of Interphase Characteristics on Long-Term Durability of Oxide-Based Fibre-Reinforced Composites , 2001 .

[45]  A. Boccaccini,et al.  Determining the fracture resistance of fibre-reinforced glass matrix composites by means of the chevron-notch flexural technique , 2001 .

[46]  Lai-fei Cheng,et al.  Mechanical properties of 3D fiber reinforced C/SiC composites , 2001 .

[47]  S. Mall,et al.  Fatigue behavior of Nextel™ 312/Blackglas™ ceramic matrix composite with tensile and zero mean load , 2001 .

[48]  H. Schneider,et al.  Temperature-induced fibre/matrix interactions in porous alumino silicate ceramic matrix composites , 2000 .

[49]  A. Bunsell,et al.  Fine diameter ceramic fibres , 2000 .

[50]  K. Chawla,et al.  Interface engineering in oxide fibre/oxide matrix composites , 2000 .

[51]  M. Lewis,et al.  Oxide CMCs: interphase synthesis and novel fibre development , 2000 .

[52]  F. Lange,et al.  Processing and properties of an all-oxide composite with a porous matrix , 2000 .

[53]  Robert A. Jurf,et al.  Advances in Oxide-Oxide CMC , 1999 .

[54]  S. Freiman,et al.  Fracture Toughness Data for Brittle Materials | NIST , 1998 .

[55]  G. Morscher,et al.  Annealing effects on creep of polycrystalline alumina-based fibers , 1998 .

[56]  D. M. Wilson,et al.  Statistical tensile strength of NextelTM 610 and NextelTM 720 fibres , 1997 .

[57]  K. Chawla,et al.  Mechanical behaviour of mullite composites reinforced with mullite fibres , 1995 .

[58]  A. Evans,et al.  Processing of damage-tolerant, oxidation-resistant ceramic matrix composites by a precursor infiltration and pyrolysis method , 1995 .

[59]  S. Barinov,et al.  The work-of-fracture of brittle materials: Principle, determination, and applications , 1994 .

[60]  M. Sakai,et al.  Work-of-fracture of brittle materials with microcracking and crack bridging , 1992 .

[61]  Karl M. Prewo,et al.  Silicon carbide fibre reinforced glass-ceramic matrix composites exhibiting high strength and toughness , 1982 .

[62]  K. Rezwan,et al.  Oxidation-induced microstructural changes of a polymer-derived Nextel™ 610 ceramic composite and impact on the mechanical performance , 2013, Journal of Materials Science.

[63]  Thomas Behrendt,et al.  Improvement of Oxide/Oxide CMC and Development of Combustor and Turbine Components in the HiPOC Program , 2011 .

[64]  Stephen Thomas Gonczy,et al.  Nextel™ 312/Silicon Oxycarbide Ceramic Composites , 2005 .

[65]  Walter Krenkel,et al.  Net Shape Manufacturing of Fabric Reinford Oxide/Oxide Components Via Resin Transfer Moulding and Pyrolysis , 2004 .

[66]  R. Venkatesh Interphase effects on the bend strength and toughness of an oxide fibre/oxide matrix composite , 2002 .

[67]  Theo Fett,et al.  Ceramics: Mechanical Properties, Failure Behaviour, Materials Selection , 1999 .

[68]  R. Bradt,et al.  Fracture toughness testing of brittle materials , 1993 .

[69]  O. Sbaizero,et al.  Mode I Fracture Resistance of a Laminated Fiber-Reinforced Ceramic , 1991 .