Investigation of hot workability behavior of as-cast Mg–5Sn–2Ca (TX52) magnesium alloy through processing map
暂无分享,去创建一个
[1] K. P. Rao,et al. Study of hot forging behavior of as-cast Mg–3Al–1Zn–2Ca alloy towards optimization of its hot workability , 2014 .
[2] Xingxing Xu,et al. Effect of Sn addition on the microstructure and mechanical properties of Mg–6Zn–1Mn (wt.%) alloy , 2014 .
[3] K. P. Rao,et al. A Study on the Hot Deformation Behavior of Cast Mg-4Sn-2Ca (TX42) Alloy , 2014 .
[4] Yong‐Ho Kim,et al. Microstructure and mechanical properties of Mg–xLi–3Al–1Sn–0.4Mn alloys (x = 5, 8 and 11 wt%) , 2014 .
[5] Y. Ganjkhanlou,et al. Effect of Ca and Rare Earth Additions on the Texture, Microhardness, Microstructure and Structural Properties of As-Cast Mg–4Al–2Sn Alloys , 2014, Transactions of the Indian Institute of Metals.
[6] K. P. Rao,et al. Effect of calcium addition on the hot working behavior of as-cast AZ31 magnesium alloy , 2013 .
[7] K. P. Rao,et al. Compressive strength and hot deformation mechanisms in as-cast Mg-4Al-2Ba-2Ca (ABaX422) alloy , 2013 .
[8] Wei Gao,et al. Effects of Sn addition on the microstructure and mechanical properties of as-cast, rolled and annealed Mg–4Zn alloys , 2013 .
[9] Yuansheng Yang,et al. Microstructure and tensile properties of as-cast and as-aged Mg–6Al–4Zn alloys with Sn addition , 2013 .
[10] C. Desrayaud,et al. Effect of Ca-addition on dynamic recrystallization of Mg–Zn alloy during hot deformation , 2013 .
[11] Li Hongliang,et al. Effects of Sn Addition on as-Cast Microstructure and Mechanical Properties of Mg-3.8Zn-2.2Ca Magnesium Alloy , 2013 .
[12] K. P. Rao,et al. Hot workability analysis with processing map and texture characteristics of as-cast TX32 magnesium alloy , 2013, Journal of Materials Science.
[13] R. Mahmudi,et al. Effects of Sn additions on the microstructure and impression creep behavior of AZ91 magnesium alloy , 2013 .
[14] Nack J. Kim,et al. Texture Evolution in Mg-Zn-Ca Alloy Sheets , 2013, Metallurgical and Materials Transactions A.
[15] K. P. Rao,et al. Hot deformation behavior of Mg–2Sn–2Ca alloy in as-cast condition and after homogenization , 2012 .
[16] T. Pollock,et al. The Dependence of Creep Behavior on Elemental Partitioning in Mg-5Al-3Ca-xSn Alloys , 2012, Metallurgical and Materials Transactions A.
[17] Y. Park,et al. Microstructure, tensile properties and creep behavior of Mg–4Al–2Sn containing Ca alloy produced by different casting technologies , 2012 .
[18] K. P. Rao,et al. Properties and processing of magnesium-tin-calcium alloys , 2011 .
[19] R. Mahmudi,et al. The microstructure and impression creep behavior of cast, Mg–5Sn–xCa alloys , 2010 .
[20] Do hyung Kim,et al. The Effect of Microstructure Evolution on the Elevated Temperature Mechanical Properties in Mg-Sn-Ca System , 2008 .
[21] M. Ohno,et al. Phase equilibria, thermodynamics and solidification microstructures of Mg–Sn–Ca alloys, Part 2: Prediction of phase formation in Mg-rich Mg–Sn–Ca cast alloys , 2008 .
[22] Y. V. R. K. Prasad,et al. Processing maps: A status report , 2003 .
[23] K. Maruyama,et al. The activity of non-basal slip systems and dynamic recovery at room temperature in fine-grained AZ31B magnesium alloys , 2003 .
[24] Henry Hu,et al. Potential Magnesium Alloys for High Temperature Die Cast Automotive Applications: A Review , 2003 .
[25] Y. Prasad,et al. Modelling of hot deformation for microstructural control , 1998 .
[26] K. Ho,et al. Prediction of a {1122} hcp stacking fault using a modified generalized stacking-fault calculation , 1997 .
[27] Yellapregeda Prasad V.R.K.,et al. Hot Working Guide: A Compendium of Processing Maps , 1997 .
[28] M. Ashby,et al. Deformation-Mechanism Maps: The Plasticity and Creep of Metals and Ceramics , 1982 .
[29] S. Morozumi,et al. {112̄2}〈1123〉 Slip system in magnesium , 1973 .
[30] John J. Jonas,et al. Strength and structure under hot-working conditions , 1969 .
[31] J. E. Dorn,et al. ON THE THERMALLY ACTIVATED MECHANISM OF PRISMATIC SLIP IN MAGNESIUM SINGLE CRYSTALS. Technical Report No. 7 , 1960 .