LAYERED CERAMICS: Processing and Mechanical Behavior

▪ Abstract Recent progress in the field of mechanical behavior of layered ceramics is reviewed. Several processing techniques are described with reference to the fabrication of ceramic laminates. T...

[1]  W. Lee,et al.  The Deflection of Cracks at Interfaces , 1997 .

[2]  Zhigang Suo,et al.  Cracking of Laminates Subjected to Biaxial Tensile Stresses , 1996 .

[3]  P. Sarkar,et al.  Electrophoretic Deposition (EPD): Mechanisms, Kinetics, and Application to Ceramics , 1996 .

[4]  M. Oechsner,et al.  Crack Bifurcation in Laminar Ceramic Composites , 1996 .

[5]  S. M. Hsu,et al.  Hertzian Contact Response of Tailored Silicon Nitride Multilayers , 1996 .

[6]  Xiaozhi Hu,et al.  Surface Properties of Ceramic Laminates Fabricated by Die Pressing , 1996 .

[7]  B. Lawn,et al.  Damage-resistant alumina-based layer composites , 1996 .

[8]  B. Marple,et al.  Graded Casting: Process Control for Producing Tailored Profiles , 1995 .

[9]  D. Wilkinson,et al.  MoSi2-based sandwich composite made by tape casting , 1995 .

[10]  B. Lawn,et al.  In Situ Processing of Silicon Carbide Layer Structures , 1995 .

[11]  Z. Suo,et al.  Surface cracking in layers under biaxial, residual compressive stress , 1995 .

[12]  B. Lawn,et al.  Contact Fatigue of a Silicon Carbide with a Heterogeneous Grain Structure , 1995 .

[13]  D. Marshall,et al.  High-temperature stability of monazite-alumina composites , 1995 .

[14]  J. Halloran,et al.  Fibrous monoliths: non-brittle fracture from powder-processed ceramics , 1995 .

[15]  D. Marshall,et al.  Ceramic Composites of Monazite and Alumina , 1995 .

[16]  O. Prakash,et al.  Crack deflection in ceramic/ceramic laminates with strong interfaces , 1995 .

[17]  F. Lange,et al.  Flexural Properties of Brittle Multilayer Materials: II, Experiments , 1994 .

[18]  V. Gupta,et al.  Energy criterion for crack deflection at an interface between two orthotropic media , 1994 .

[19]  Brian R. Lawn,et al.  Effect of Grain Size on Hertzian Contact Damage in Alumina , 1994 .

[20]  B. Lawn,et al.  A model for microcrack initiation and propagation beneath hertzian contacts in polycrystalline ceramics , 1994 .

[21]  J. Halloran,et al.  Fibrous Monolithic Ceramics: III, Mechanical Properties and Oxidation Behavior of the Silicon Carbide/Boron Nitride System , 1994 .

[22]  F. Lange,et al.  Flexural Properties of Brittle Multilayer Materials: I, Modeling , 1994 .

[23]  Brian R. Lawn,et al.  Deformation and fracture of mica-containing glass-ceramics in Hertzian contacts , 1994 .

[24]  B. Lawn,et al.  Making Ceramics "Ductile" , 1994, Science.

[25]  N. Padture In situ-toughened silicon carbide , 1994 .

[26]  P. Sarkar,et al.  Electrophoretic Deposition and its Use to Synthesise YSZ/Al2O3 Micro‐Laminate Ceramic/Ceramic Composites , 1993 .

[27]  Z. Suo,et al.  Tunneling Cracks in Constrained Layers , 1993 .

[28]  A. Jagota,et al.  Crack Growth and Damage in Constrained Sintering Films , 1993 .

[29]  H. M. Chan,et al.  Flaw-tolerance and crack-resistance properties of alumina-aluminum titanate composites with tailored microstructures , 1993 .

[30]  S. D. Nunn,et al.  Fibrous Monolithic Ceramics: I, Fabrication, Microstructure, and Indentation Behavior , 1993 .

[31]  J. Halloran,et al.  Fibrous Monolithic Ceramics: II, Flexural Strength and Fracture Behavior of the Silicon Carbide/Graphite System , 1993 .

[32]  B. Lawn Fracture of Brittle Solids by Brian Lawn , 1993 .

[33]  T. Clyne,et al.  Fracture behaviour of ceramic laminates in bending—I. Modelling of crack propagation , 1993 .

[34]  T. Clyne,et al.  Fracture behaviour of ceramic laminates in bending—II. Comparison of model predictions with experimental data , 1993 .

[35]  V. Gupta,et al.  Calculation, Measurement, and Control of Interface Strength in Composites , 1993 .

[36]  J. Moya,et al.  Al2TiO5 Formation in Alumina/Titania Multilayer Composites , 1992 .

[37]  M. Harmer,et al.  Design of a Laminated Ceramic Composite for Improved Strength and Toughness , 1992 .

[38]  W. Clegg,et al.  The fabrication and failure of laminar ceramic composites , 1992 .

[39]  P. Sarkar,et al.  Structural Ceramic Microlaminates by Electrophoretic Deposition , 1992 .

[40]  D. Wilkinson,et al.  Strength and flaw elimination assessment in tape cast ceramic laminates , 1992 .

[41]  H. M. Chan,et al.  Improved Flaw Tolerance in Alumina Containing 1 vol% Anorthite via Crystallization of the Intergranular Glass , 1992 .

[42]  M. Harmer,et al.  Unique Opportunities for Microstructural Engineering with Duplex and Laminar Ceramic Composites , 1992 .

[43]  Dong-joo Lee,et al.  R‐Curve Behavior and Strength for In‐Situ Reinforced Silicon Nitrides with Different Microstructures , 1992 .

[44]  T. Miyoshi,et al.  Fabrication and Fracture Behavior of Novel SiC Ceramics Having Rodlike Grains , 1992 .

[45]  David B. Marshall,et al.  Enhanced Fracture Toughness in Layered Microcomposites of Ce‐ZrO2 and Al2O3 , 1991 .

[46]  D. S. Pearson,et al.  Centrifugal Consolidation of Al2O3 and AI2O3/ZrO2 Composite Slurries vs Interparticle Potentials: Particle Packing and Mass Segregation , 1991 .

[47]  P. Becher Microstructural design of toughened ceramics , 1991 .

[48]  D. Marshall Crack Shielding in Ceria‐Partially‐Stabilized Zirconia , 1990 .

[49]  K. Kendall,et al.  A simple way to make tough ceramics , 1990, Nature.

[50]  B. Lawn,et al.  Role of grain size in the strength and R-curve properties of alumina , 1990 .

[51]  A. Evans Perspective on the Development of High‐Toughness Ceramics , 1990 .

[52]  A. Heuer,et al.  Novel composite microstructure and mechanical behavior of mollusk shell , 1989 .

[53]  B. Lawn,et al.  Role of interfacial grain-bridging sliding friction in the crack-resistance and strength properties of nontransforming ceramics , 1989 .

[54]  R. Moreno,et al.  Alumina and alumina/zirconia multilayer composites obtained by slip casting , 1989 .

[55]  A. Virkar,et al.  Indentation Fracture Response and Damage Resistance of Al2O3‐ZrO2 Composites Strengthened by Transformation‐Induced Residual Stresses , 1988 .

[56]  Rajendra K. Bordia,et al.  On constrained sintering—I. Constitutive model for a sintering body , 1988 .

[57]  A. Virkar,et al.  Measurement of Residual Stresses in Oxide–ZrO2 Three‐Layer Composites , 1988 .

[58]  D. Shetty,et al.  Strength Improvement in Transformation‐Toughened Alumina by Selective Phase Transformation , 1987 .

[59]  Y. Mai,et al.  Crack‐Interface Grain Bridging as a Fracture Resistance I, Mechanism in Ceramics: I, Experimental Study on Alumina , 1987 .

[60]  Jow-Lay Huang,et al.  Strengthening of Oxide Ceramics by Transformation‐Induced Stress , 1987 .

[61]  T. Chartier,et al.  Tape Casting of Al2O3/ZrO2 Laminated Composites , 1986 .

[62]  R. Cook,et al.  Microstructure-strength properties in ceramics. I: Effect of crack size on toughness , 1985 .

[63]  R. Raj,et al.  Sintering Behavior of Ceramic Films Constrained by a Rigid Substrate , 1985 .

[64]  A. Evans,et al.  Failure Mechanisms in Ceramic‐Fiber/Ceramic‐Matrix Composites , 1985 .

[65]  R. Steinbrech,et al.  Memory effect of crack resistance during slow crack growth in notched Al2O3 bend specimens , 1982 .

[66]  Richard Warren,et al.  Measurement of the fracture properties of brittle solids by hertzian indentation , 1978 .

[67]  John D. Currey,et al.  Mechanical properties of mother of pearl in tension , 1977, Proceedings of the Royal Society of London. Series B. Biological Sciences.

[68]  Michael V. Swain,et al.  Indentation plasticity and the ensuing fracture of glass , 1976 .

[69]  Kevin Kendall,et al.  Transition between cohesive and interfacial failure in a laminate , 1975, Proceedings of the Royal Society of London. A. Mathematical and Physical Sciences.

[70]  B. Lawn,et al.  Indentation fracture: principles and applications , 1975 .

[71]  B. Lawn,et al.  A comparative study of the fracture of various silica modifications using the Hertzian test , 1973 .

[72]  B. Lawn,et al.  Hertzian Fracture Experiments on Abraded Glass Surfaces as Definitive Evidence for an Energy Balance Explanation of Auerbach's Law , 1969 .

[73]  B. Lawn HERTZIAN FRACTURE IN SINGLE CRYSTALS WITH THE DIAMOND STRUCTURE , 1967 .

[74]  J. E. Gordon,et al.  A mechanism for the control of crack propagation in all-brittle systems , 1964, Proceedings of the Royal Society of London. Series A. Mathematical and Physical Sciences.

[75]  Raymond A. Cutler,et al.  Toughening of Layered Ceramic Composites with Residual Surface Compression , 1996 .

[76]  T. Clyne,et al.  The correlation of interfacial and macroscopic toughness in SiC laminates , 1993 .

[77]  G. Fantozzi,et al.  Interfacial reaction in zircon-alumina multilayer composites , 1991 .

[78]  John W. Hutchinson,et al.  Crack deflection at an interface between dissimilar elastic-materials , 1989 .

[79]  Theodore J. Reinhart,et al.  Engineered materials handbook , 1987 .

[80]  D. R. Clarke,et al.  Fracture of ceramics and glasses , 1987 .

[81]  R. Steinbrech,et al.  Increase of crack resistance during slow crack growth in Al2O3 bend specimens , 1983 .

[82]  B. Lawn,et al.  A Study of Dislocation Arrays at Spherical Indentations in LiF as a Function of Indentation Stress and Strain , 1969 .

[83]  R. Plunkett,et al.  Formulas for Stress and Strain , 1965 .