Electrical breakdown of nanowires.

Instantaneous electrical breakdown measurements of GaN and Ag nanowires are performed by an in situ transmission electron microscopy method. Our results directly reveal the mechanism that typical thermally heated semiconductor nanowires break at the midpoint, while metallic nanowires breakdown near the two ends due to the stress induced by electromigration. The different breakdown mechanisms for the nanowires are caused by the different thermal and electrical properties of the materials.

[1]  Lianmao Peng,et al.  Current-voltage characteristics and parameter retrieval of semiconducting nanowires , 2006 .

[2]  Jiaqi Huang,et al.  Mass transportation mechanism in electric-biased carbon nanotubes. , 2010, Nano letters.

[3]  I. Blech Electromigration in thin aluminum films on titanium nitride , 1976 .

[4]  Elaine Lai,et al.  Photoluminescence, thermal transport, and breakdown in joule-heated GaN nanowires. , 2009, Nano letters.

[5]  K. Maex,et al.  Plasticity of electromigration-induced hillocking and its effect on the critical length , 2002 .

[6]  Ferdinand Kuemmeth,et al.  Imaging electromigration during the formation of break junctions. , 2007, Nano letters.

[7]  K. Jiang,et al.  Breaking single-walled carbon nanotube bundles by Joule heating , 2008 .

[8]  Younan Xia,et al.  Synthesis and electrical characterization of silver nanobeams. , 2006, Nano letters.

[9]  Yue Zhang,et al.  Electrical breakdown of ZnO nanowires in metal-semiconductor-metal structure , 2010 .

[10]  K. H. Chen,et al.  Catalytic growth and characterization of gallium nitride nanowires. , 2001, Journal of the American Chemical Society.

[11]  D. R. Strachan,et al.  Real-time TEM imaging of the formation of crystalline nanoscale gaps. , 2008, Physical review letters.

[12]  Eric Pop,et al.  Thermally limited current carrying ability of graphene nanoribbons. , 2011, Physical review letters.

[13]  Jing Zhu,et al.  Functional Faceted Silver Nano-Hexapods: Synthesis, Structure Characterizations, and Optical Properties , 2008 .

[14]  Y. Bando,et al.  In situ TEM-STM recorded kinetics of boron nitride nanotube failure under current flow. , 2009, Nano letters.

[15]  Younan Xia,et al.  Uniform Silver Nanowires Synthesis by Reducing AgNO3 with Ethylene Glycol in the Presence of Seeds and Poly(Vinyl Pyrrolidone) , 2002 .

[16]  P. Avouris,et al.  Current saturation and electrical breakdown in multiwalled carbon nanotubes. , 2001, Physical review letters.

[17]  François Léonard,et al.  Size-dependent effects on electrical contacts to nanotubes and nanowires. , 2006, Physical review letters.

[18]  R. Stratton,et al.  Field and thermionic-field emission in Schottky barriers , 1966 .

[19]  C. Durkan,et al.  Controlled fabrication of 1–2nm nanogaps by electromigration in gold and gold-palladium nanowires , 2007 .

[20]  Lianmao Peng,et al.  In situ electrical measurements of polytypic silver nanowires , 2008, Nanotechnology.

[21]  Charles M Lieber,et al.  Ultrathin Au nanowires and their transport properties. , 2008, Journal of the American Chemical Society.

[22]  Y. Liu,et al.  Analytical analysis of heat conduction in a suspended one-dimensional object , 2009 .

[23]  Andrew M. Minor,et al.  Void formation induced electrical switching in phase-change nanowires. , 2008, Nano letters.