Crack inhibition to enhance strength-ductility of CM247LC alloy fabricated by laser powder bed fusion

[1]  Lan Huang,et al.  Effect of yttrium addition on microstructural evolution and high temperature mechanical properties of Ni-based superalloy produced by selective laser melting , 2022, Materials Science and Engineering: A.

[2]  H. Yu,et al.  Cracking inhibition behavior and the strengthening effect of TiC particles on the CM247LC superalloy prepared by selective laser melting , 2022, Materials Science and Engineering: A.

[3]  Changjun Han,et al.  Corrosion fatigue behavior and anti-fatigue mechanisms of an additively manufactured biodegradable zinc-magnesium gyroid scaffold. , 2022, Acta biomaterialia.

[4]  Yicha Zhang,et al.  Interfacial Characteristics and Formation Mechanisms of Copper–steel Multimaterial Structures Fabricated via Laser Powder Bed Fusion Using Different Building Strategies , 2022, Chinese Journal of Mechanical Engineering: Additive Manufacturing Frontiers.

[5]  S. Luo,et al.  Avoiding cracks in additively manufactured non-weldable directionally solidified Ni-based superalloys , 2022, Additive Manufacturing.

[6]  J. Moverare,et al.  Modelling of Additive Manufacturability of Nickel-Based Superalloys for Laser Powder Bed Fusion , 2022, Acta Materialia.

[7]  Baode Sun,et al.  Effect of carbon content on the microstructure, tensile properties and cracking susceptibility of IN738 superalloy processed by laser powder bed fusion , 2022, Additive Manufacturing.

[8]  Changjun Han,et al.  Effect of Scanning Strategies on the Microstructure and Mechanical Properties of Inconel 718 Alloy Fabricated by Laser Powder Bed Fusion , 2022, Advanced Engineering Materials.

[9]  S. Seo,et al.  Effects of hot isostatic pressing treatment on the microstructure and tensile properties of Ni-based superalloy CM247LC manufactured by selective laser melting , 2022, Materials Science and Engineering: A.

[10]  M. Fu,et al.  Multi-scale defects in powder-based additively manufactured metals and alloys , 2022, Journal of Materials Science & Technology.

[11]  Chaolin Tan,et al.  Duplex strengthening via SiC addition and in-situ precipitation in additively manufactured composite materials , 2022, Composites Part B: Engineering.

[12]  A. Huang,et al.  Scanning Strategy Induced Cracking and Anisotropic Weakening in Grain Texture of Additively Manufactured Superalloys , 2022, Additive Manufacturing.

[13]  Wei Zhou,et al.  Mitigation of liquation cracking in selective laser melted Inconel 718 through optimization of layer thickness and laser energy density , 2022, Journal of Materials Processing Technology.

[14]  J. Andersson,et al.  Influence of laser powder bed fusion process parameters on the microstructure and cracking susceptibility of nickel-based superalloy Alloy 247LC , 2022, Results in Materials.

[15]  Moataz M. Attallah,et al.  Direct laser deposition of crack-free CM247LC thin walls: Mechanical properties and microstructural effects of heat treatment , 2021, Materials & Design.

[16]  Jinghao Xu,et al.  Influence of laser powder bed fusion process parameters on the microstructure of solution heat-treated nickel-based superalloy Alloy 247LC , 2021, Materials Characterization.

[17]  Yutian Ding,et al.  Grain refinement and crack inhibition of hard-to-weld Inconel 738 alloy by altering the scanning strategy during selective laser melting , 2021 .

[18]  Moataz M. Attallah,et al.  A Melt Pool Temperature Model in Laser Powder Bed Fabricated CM247LC Ni Superalloy to Rationalize Crack Formation and Microstructural Inhomogeneities , 2021, Metallurgical and Materials Transactions A.

[19]  Guijun Bi,et al.  Progress and perspectives in laser additive manufacturing of key aeroengine materials , 2021, International Journal of Machine Tools and Manufacture.

[20]  Y. Lo,et al.  Experimental investigation into microstructure, mechanical properties, and cracking mechanism of IN713LC processed by laser powder bed fusion , 2021, Materials Science and Engineering: A.

[21]  R. Setchi,et al.  Material-structure-performance integrated laser-metal additive manufacturing , 2021, Science.

[22]  Ping Li,et al.  Selective laser melting of Al-3.48Cu-2.03Si-0.48Sc-0.28Zr alloy: Microstructure evolution, properties and metallurgical defects , 2021 .

[23]  S. Griffiths,et al.  Combining alloy and process modification for micro-crack mitigation in an additively manufactured Ni-base superalloy , 2020 .

[24]  Zhiheng Hu,et al.  Cracking criterion for high strength Al–Cu alloys fabricated by selective laser melting , 2020 .

[25]  J. Andersson,et al.  Influence of Laser Powder Bed Fusion Process Parameters on Voids, Cracks, and Microhardness of Nickel-Based Superalloy Alloy 247LC , 2020, Materials.

[26]  Shibo Wu,et al.  Hot cracking behavior and mechanism of a third-generation Ni-based single-crystal superalloy during directed energy deposition , 2020 .

[27]  C. Colin,et al.  Processing a non-weldable nickel-base superalloy by Selective Laser Melting: role of the shape and size of the melt pools on solidification cracking , 2020 .

[28]  A. Dong,et al.  Inhibition of cracking by grain boundary modification in a non-weldable nickel-based superalloy processed by laser powder bed fusion , 2020 .

[29]  G. Cheng,et al.  A review on microstructures and properties of high entropy alloys manufactured by selective laser melting , 2020, International Journal of Extreme Manufacturing.

[30]  Moataz M. Attallah,et al.  Novel Hybrid Manufacturing Process of CM247LC and Multi-Material Blisks , 2020, Micromachines.

[31]  L. Tonelli,et al.  CoCr alloy processed by Selective Laser Melting (SLM): effect of Laser Energy Density on microstructure, surface morphology, and hardness , 2020 .

[32]  C. Leinenbach,et al.  Healing cracks in selective laser melting by 3D laser shock peening , 2019, Additive Manufacturing.

[33]  Moataz M. Attallah,et al.  Influence of powder characteristics on the microstructure and mechanical properties of HIPped CM247LC Ni superalloy , 2019, Materials & Design.

[34]  Xiaodong Li,et al.  An overview of residual stresses in metal powder bed fusion , 2019, Additive Manufacturing.

[35]  M. Amirjan,et al.  Effect of scanning strategy and speed on the microstructure and mechanical properties of selective laser melted IN718 nickel-based superalloy , 2019, The International Journal of Advanced Manufacturing Technology.

[36]  J. Humbeeck,et al.  Microstructure and mechanical properties of Hastelloy X produced by HP-SLM (high power selective laser melting) , 2019, Materials & Design (1980-2015).

[37]  Hua-ming Wang,et al.  On the solidification behaviour and cracking origin of a nickel-based superalloy during selective laser melting , 2019, Materials Characterization.

[38]  I. Ashcroft,et al.  Geometrical effects on residual stress in selective laser melting , 2019, Additive Manufacturing.

[39]  N. Tamura,et al.  Mechanism of heat affected zone cracking in Ni-based superalloy DZ125L fabricated by laser 3D printing technique , 2018, Materials & Design.

[40]  Xin Lin,et al.  The initiation and propagation mechanism of the overlapping zone cracking during laser solid forming of IN-738LC superalloy , 2018, Journal of Alloys and Compounds.

[41]  Chee Kai Chua,et al.  Modeling temperature and residual stress fields in selective laser melting , 2018 .

[42]  A. Kromm,et al.  Effect of hatch length on the development of microstructure, texture and residual stresses in selective laser melted superalloy Inconel 718 , 2017 .

[43]  T. Pollock,et al.  3D printing of high-strength aluminium alloys , 2017, Nature.

[44]  A. Clare,et al.  Fractal scan strategies for selective laser melting of ‘unweldable’ nickel superalloys , 2017 .

[45]  Moataz M. Attallah,et al.  Microstructure and yield strength of SLM-fabricated CM247LC Ni-Superalloy , 2017 .

[46]  Yang Liu,et al.  A study on the residual stress during selective laser melting (SLM) of metallic powder , 2016 .

[47]  Moataz M. Attallah,et al.  The influence of the laser scan strategy on grain structure and cracking behaviour in SLM powder-bed fabricated nickel superalloy , 2014 .

[48]  H. Assadi,et al.  Solidification crack initiation and propagation in pulsed laser welding of wrought heat treatable aluminium alloy , 2014 .

[49]  I. Kim,et al.  Anomalous deformation behavior and twin formation of Ni-base superalloys at the intermediate temperatures , 2011 .

[50]  C. Jo,et al.  Influence of heat treatment on microstructure and tensile properties of conventionally cast and directionally solidified superalloy CM247LC , 2008 .

[51]  A. Jacot,et al.  Last-stage solidification of alloys: Theoretical model of dendrite-arm and grain coalescence , 2003 .

[52]  W. Kurz,et al.  SINGLE-CRYSTAL LASER DEPOSITION OF SUPERALLOYS: PROCESSING-MICROSTRUCTURE MAPS , 2001 .

[53]  J. Drezet,et al.  A new hot-tearing criterion , 1999 .

[54]  D. G. McCartney,et al.  Alloys-by-design: Application to new superalloys for additive manufacturing , 2021 .