Texture evolution during sub-critical annealing and its effect on yield strength anisotropy of laser directed energy deposited Ti-6Al-2Zr-1Mo-1V alloy

[1]  R. Chen,et al.  Multistep low-to-high-temperature heating as a suitable alternative to hot isostatic pressing for improving laser powder-bed fusion-fabricated Ti-6Al-2Zr-1Mo-1V microstructural and mechanical properties , 2022, Materials Science and Engineering: A.

[2]  A. Clare,et al.  Composition fine-tuning for directed energy deposition of Ti-6Al-4V , 2022 .

[3]  Guodong Zhang,et al.  Wire-fed electron beam directed energy deposition of Ti–6Al–2Zr–1Mo–1 V alloy and the effect of annealing on the microstructure, texture, and anisotropy of tensile properties , 2021, Additive Manufacturing.

[4]  M. Fitzpatrick,et al.  The ageing response of direct laser deposited metastable β-Ti alloy, Ti–5Al–5Mo–5V–3Cr , 2021, Additive Manufacturing.

[5]  Shenmin Zhang,et al.  The microstructure and tensile properties of additively manufactured Ti–6Al–2Zr–1Mo–1V with a trimodal microstructure obtained by multiple annealing heat treatment , 2021, Materials Science and Engineering: A.

[6]  Xinghua Yu,et al.  A review on wire and arc additive manufacturing of titanium alloy , 2021 .

[7]  Yu Qin,et al.  A critical dislocation velocity for serration mechanism transition in a nickel-chromium solid solution alloy , 2021 .

[8]  S. Babu,et al.  Phase transformation pathways in Ti-6Al-4V manufactured via electron beam powder bed fusion , 2021, Acta Materialia.

[9]  Ming Yan,et al.  Additive manufacturing of metals: Microstructure evolution and multistage control , 2021 .

[10]  Z. Li,et al.  Effect of α texture on the anisotropy of yield strength in Ti–6Al–2Zr–1Mo–1V alloy fabricated by laser directed energy deposition technique , 2021 .

[11]  R. Hague,et al.  Microstructure and tensile properties of additive manufactured Ti-6Al-4V with refined prior-β grain structure obtained by rapid heat treatment , 2021, Materials Science and Engineering: A.

[12]  T. Becker,et al.  The influence of microstructural texture and prior beta grain recrystallisation on the deformation behaviour of laser powder bed fusion produced Ti–6Al–4V , 2021 .

[13]  S. Gong,et al.  Effects of the crystallographic and spatial orientation of α lamellae on the anisotropic in-situ tensile behaviors of additive manufactured Ti–6Al–4V , 2021 .

[14]  Y. Qi,et al.  Generalized stacking fault energies and critical resolved shear stresses of random α-Ti-Al alloys from first-principles calculations , 2021 .

[15]  Ming-Wei Wu,et al.  Intensification of preferred orientation in the additive manufactured Ti-6Al-4V alloy after heat treatment , 2020 .

[16]  P. Blackwell,et al.  Influence of laser power and powder feed rate on the microstructure evolution of laser metal deposited Ti-5553 on forged substrates , 2020 .

[17]  Yusheng Shi,et al.  Selective laser melting of near-α titanium alloy Ti-6Al-2Zr-1Mo-1V: Parameter optimization, heat treatment and mechanical performance , 2020 .

[18]  S. Gong,et al.  Anisotropy in microstructure and tensile properties of Ti–5Al–5Mo–5V–1Cr–1Fe produced via additive manufacturing , 2020 .

[19]  Guoqing Chen,et al.  The role of pyramidal 〈  +  〉 dislocations in the grain refinement mechanism in Ti-6Al-4V alloy processed by severe plastic deformation , 2020 .

[20]  A. K. Syed,et al.  The role of microstructure and local crystallographic orientation near porosity defects on the high cycle fatigue life of an additive manufactured Ti-6Al-4V , 2020, Materials Characterization.

[21]  Q. Fan,et al.  Plastic deformation mode and α/β slip transfer of Ti–5Al-2.5Cr-0.5Fe-4.5Mo–1Sn–2Zr–3Zn titanium alloy at room temperature , 2020 .

[22]  Xin Lin,et al.  Effects of subtransus heat treatments on microstructure features and mechanical properties of wire and arc additive manufactured Ti–6Al–4V alloy , 2020 .

[23]  M. Cheikh,et al.  Role of grain size and crystallographic texture on tensile behavior induced by sliding mechanism in Ti-6Al-4V alloy , 2020 .

[24]  Zhibo Ma,et al.  Mechanical properties and microstructural evolution of TA15 Ti alloy processed by selective laser melting before and after annealing , 2020 .

[25]  Shijian Zheng,et al.  Twinning and Sequential Kinking in Lamellar Ti-6Al-4V Alloy , 2019, Acta Materialia.

[26]  W. M. Rainforth,et al.  Basal slip mediated tension twin variant selection in magnesium WE43 alloy , 2019, Acta Materialia.

[27]  S. Gong,et al.  Effect of α texture on the tensile deformation behavior of Ti–6Al–4V alloy produced via electron beam rapid manufacturing , 2019, Materials Science and Engineering: A.

[28]  J. Keist,et al.  Microtexture in additively manufactured Ti-6Al-4V fabricated using directed energy deposition , 2018, Materials Science and Engineering: A.

[29]  Xin Lin,et al.  Achieving superior ductility for laser solid formed extra low interstitial Ti-6Al-4V titanium alloy through equiaxial alpha microstructure , 2018 .

[30]  Shu Beng Tor,et al.  Anisotropy and heterogeneity of microstructure and mechanical properties in metal additive manufacturing: A critical review , 2018 .

[31]  Lin Xiao,et al.  Slip transmission behavior across α/β interface and strength prediction with a modified rule of mixtures in TC21 titanium alloy , 2017 .

[32]  Yanjin Lu,et al.  Crystallographic features of α variants and β phase for Ti-6Al-4V alloy fabricated by selective laser melting , 2017 .

[33]  Z. Li,et al.  Thermal expansion properties of laser melting deposited Ti-6.5Al-2Zr-1Mo-1V alloy during α + β zone annealing , 2017 .

[34]  Zemin Wang,et al.  Effect of crystallographic orientation on mechanical anisotropy of selective laser melted Ti-6Al-4V alloy , 2017 .

[35]  C. Emmelmann,et al.  Additive Manufacturing of Metals , 2016 .

[36]  Jing Li,et al.  Variant selection in laser melting deposited α + β titanium alloy , 2016 .

[37]  Olivier Rigo,et al.  Electron beam melted Ti–6Al–4V: Microstructure, texture and mechanical behavior of the as-built and heat-treated material , 2016 .

[38]  Xin Lin,et al.  Texture and microstructure characterization in laser additive manufactured Ti–6Al–2Zr–2Sn–3Mo–1.5Cr–2Nb titanium alloy , 2015 .

[39]  Chee Kai Chua,et al.  Graded microstructure and mechanical properties of additive manufactured Ti–6Al–4V via electron beam melting , 2015 .

[40]  Yunzhi Wang,et al.  Microstructure and transformation texture evolution during α precipitation in polycrystalline α/β titanium alloys – A simulation study , 2015 .

[41]  Hua-ming Wang,et al.  Influence of prior-β-grain size on tensile strength of a laser-deposited α/β titanium alloy at room and elevated temperatures , 2015 .

[42]  E. A. Payzant,et al.  Comparison of Residual Stresses in Inconel 718 Simple Parts Made by Electron Beam Melting and Direct Laser Metal Sintering , 2015, Metallurgical and Materials Transactions A.

[43]  Hua-ming Wang,et al.  Effect of heat treatment on microstructure and mechanical properties of laser deposited Ti60A alloy , 2014 .

[44]  Thomas R. Bieler,et al.  Methodology for estimating the critical resolved shear stress ratios of α-phase Ti using EBSD-based trace analysis , 2013 .

[45]  Philip B. Prangnell,et al.  Effect of build geometry on the β-grain structure and texture in additive manufacture of Ti6Al4V by selective electron beam melting , 2013 .

[46]  Huiping Tang,et al.  Microstructure evolution of sub-critical annealed laser deposited Ti–6Al–4V alloy , 2012 .

[47]  J. Mendez,et al.  Analysis of the different slip systems activated by tension in a α/β titanium alloy in relation with local crystallographic orientation , 2005 .

[48]  S. Zaefferer A study of active deformation systems in titanium alloys: dependence on alloy composition and correlation with deformation texture , 2003 .