Detachment Analysis of Dehumidified Repair Mortars Applied to Historical Masonry Walls

An innovative laboratory procedure for the pre-qualification of repair mortars is described. The tested mortars are suitable for use with new dehumidified plasters applied to historical masonry walls. Long-term plaster detachment frequently occurs because of the mechanical incompatibility of mortar. The procedure consists of the application of static loads to mixed stone block-mortar specimens with particular characteristics, in terms of geometry and adhesion at the interface. A numerical simulation based on the cohesive crack model was used to follow the experimental data, in order to describe the evolutionary phenomenon of detachment as a function of a small number of parameters. The methodology is currently being used at Sacro Monte di Varallo Special Natural Reserve (UNESCO heritage site) in Piedmont (Italy).

[1]  Fabrizio Barpi,et al.  A fractional order rate approach for modeling concrete structures subjected to creep and fracture , 2004 .

[2]  Alessandro Grazzini Experimental techniques for the evaluation of the durability of strengthening works on historical masonry , 2006 .

[3]  Fabrizio Barpi,et al.  Lifetime evaluation of concrete structures under sustained post-peak loading , 2005 .

[4]  Jean Marc Christian Tulliani,et al.  Organic-inorganic material for the consolidation of plaster , 2011 .

[5]  Fabrizio Barpi,et al.  Fuzzy parameters analysis of time‐dependent fracture of concrete dam models , 2002 .

[6]  M. Collepardi,et al.  Degradation and restoration of masonry walls of historical buildings , 1990 .

[7]  Alessandro Grazzini,et al.  Mechanical Properties and Freeze-Thaw Durability of Strengthening Mortars , 2013 .

[8]  J. Červenka,et al.  Mixed mode fracture of cementitious bimaterial interfaces: ; Part II: numerical simulation , 1998 .

[9]  Alessandro Grazzini,et al.  Experimental Procedure for the Pre-Qualification of Strengthening Mortars , 2012 .

[10]  H. W. Reinhardt,et al.  Experimental determination of crack softening characteristics of normalweight and lightweight concrete , 1986 .

[11]  P. Antonacia,et al.  Damage analysis of brick-to-mortar interfaces , 2016 .

[12]  Monica Favaro,et al.  Evaluation of compatibility and durability of a hydraulic lime-based plaster applied on brick wall masonry of historical buildings affected by rising damp phenomena , 2002 .

[13]  Fabrizio Barpi,et al.  The cohesive frictional crack model applied to the analysis of the dam-foundation joint , 2010 .

[14]  Fabrizio Barpi,et al.  Size-effects induced bifurcation phenomena during multiple cohesive crack propagation , 1998 .

[15]  Silvio Valente,et al.  Mechanical interaction between historical brick and repair mortar: experimental and numerical tests , 2011 .

[16]  Fabrizio Barpi,et al.  Modeling water penetration at dam-foundation joint , 2008 .