Low-activation joining of SiC/SiC composites for fusion applications

Abstract Research at PNNL has been directed at high-strength, low-activation joints using solid-state displacement reactions. This paper reports on further development and optimization of displacement reaction joints for the TITAN collaboration. The results reveal that fully dense and high-quality joints between SiC-composite bars are fabricated at 1623 K–1723 K using 30 MPa pressure in purified argon atmospheres. Scanning electron micrographs reveal typical interpenetrating phase microstructures in the joints, which are about 10 μm thick. Blocky SiC particles are observed to nucleate preferentially at the SiC-joint interface but are more plate-like within the joint. X-ray spectroscopy reveals a uniform distribution of constituent elements consistent with the interpenetrating phases.

[1]  S. Morozumi Joining of silicon carbide , 1989 .

[2]  S. Morozumi,et al.  Bonding mechanism between silicon carbide and thin foils of reactive metals , 1985 .

[3]  R. Pailler,et al.  SiC filament/titanium matrix composites regarded as model composites , 1984 .

[4]  Yigal D. Blum,et al.  Coatings and joining for SiC and SiC-composites for nuclear energy systems , 2007 .

[5]  J. L. Brimhall,et al.  Synthesis of Ti3SiC2SiC and TiSi2SiC composites using displacement reactions in the TiSiC system , 1996 .

[6]  A. Kohyama,et al.  Recent advances and issues in development of silicon carbide composites for fusion applications , 2009 .

[7]  M. Backhaus-Ricoult Solid State Reactions Between Silicon Carbide and Various Transition Metals , 1989 .

[8]  M. Naka,et al.  Ti3SiC2 phase in SiC/SiC joint brazed with Cu43T57 alloy , 1990 .

[9]  Shujuan Wang,et al.  The characterization of an SCS6/Ti–6Al–4V MMC interphase , 1989 .

[10]  G. Maugin The Thermomechanics of Plasticity and Fracture , 1992 .

[11]  M. Backhaus-Ricoult PHYSICOCHEMICAL PROCESSES AT METAL-CERAMIC INTERFACES , 1990 .

[12]  B. Riccardi,et al.  Joining of SiC/SiCf ceramic matrix composites for fusion reactor blanket applications , 2000 .

[13]  W. Pan,et al.  Mechanical properties of polycrystalline Ti3SiC2 at ambient and elevated temperatures , 2001 .

[14]  M. Ferraris,et al.  Microstructure and mechanical properties of low-activation glass-ceramic joining and coating for SiC/SiC composites , 2000 .

[15]  M. Backhaus-Ricoult Diffusion Processes and Interphase Boundary Morphology in Ternary Metal-Ceramic Systems , 1986 .

[16]  M. Chandrasekaran,et al.  Interaction between titanium and SiC , 1990 .

[17]  D. B. Gundel,et al.  Interfacial reaction kinetics of coated SiC fibers with various titanium alloys , 1991 .