A laboratory study on stone matrix asphalt using ground tire rubber

Abstract This research investigated the feasibility using asphalt rubber (AR), produced by blending ground tire rubber (GTR) with an asphalt, as a binder for stone matrix asphalt (SMA). Two different sizes of GTR produced in Taiwan were used. The potential performance of AR–SMA mixtures was also evaluated. The results of this study showed that it was not feasible to produce a suitable SMA mixture using an asphalt rubber made by blending an AC-20 with 30% coarse GTR with a maximum size of 0.85 mm. However, SMA mixtures meeting typical volumetric requirements for SMA could be produced using an asphalt rubber containing 20% of a fine GTR with a maximum size of 0.6 mm. No fiber was needed to prevent drain-down when this asphalt rubber was used. The AR–SMA mixtures were not significantly different from the conventional SMA mixtures in terms of moisture susceptibility from the results of AASHTO T283 tests. The results of the wheel tracking tests at 60 °C show that rutting resistance of AR–SMA mixtures was better than that of the conventional SMA mixtures.