Oxidation of Ti-6Al-4V alloy

Abstract Air oxidation behaviour of a Ti–6Al–4V alloy was examined over the temperature range of 600–800 °C for different time intervals ranging between 0.5 and 72 h. In addition to the determination of the oxidation kinetics by weight gain measurements, oxygen diffusion zone (ODZ) depth and hardness measurements were conducted on the cross-sections of the oxidised alloys to investigate the diffusion kinetics of oxygen into the substrate. The rate of oxidation evaluated according to the weight gain measurements fitted parabolic kinetics between 600 and 700 °C and linear kinetics above 700 °C by yielding activation energies of 276 and 191 kJ/mol, respectively. Analysis of the ODZ depth and hardness measurements resulted in an activation energy of 202 kJ/mol for oxygen diffusion in Ti–6Al–4V alloy. Finally, the kinetics of oxidation and oxygen diffusion were evaluated by the analysis of the experimental data with respect to temperature-compensated time parameter.

[1]  T. Bell,et al.  Surface engineering of timet 550 with oxygen to form a rutile-based, wear-resistant coating , 2002 .

[2]  F. Hauser,et al.  Deformation and Fracture Mechanics of Engineering Materials , 1976 .

[3]  E. Collings,et al.  Materials Properties Handbook: Titanium Alloys , 1994 .

[4]  F. Borgioli,et al.  Improvement of wear resistance of Ti-6Al-4V alloy by means of thermal oxidation , 2005 .

[5]  K. L. Dahm,et al.  The corrosion–wear behaviour of thermally oxidised CP-Ti and Ti–6Al–4V , 2004 .

[6]  F. Alsina,et al.  Structural, morphological and local electric properties of TiO2 thin films grown by pulsed laser deposition , 2007 .

[7]  H. Anada,et al.  The effect of various ternary additives on the oxidation behavior of TiAl in high-temperature air , 1996 .

[8]  I. Gurrappa An oxidation model for predicting the life of titanium alloy components in gas turbine engines , 2005 .

[9]  T. Bell,et al.  Surface modification of titanium alloys for combined improvements in corrosion and wear resistance , 1998 .

[10]  H. Cimenoglu,et al.  Effect of thermal oxidation on corrosion and corrosion-wear behaviour of a Ti-6Al-4V alloy. , 2004, Biomaterials.

[11]  A. Rahmel,et al.  Mechanism of isothermal oxidation of the intel-metallic TiAl and of TiAl alloys , 1992 .

[12]  P. Dearnley,et al.  Corrosion response of surface engineered titanium alloys damaged by prior abrasion , 2001 .

[13]  Fu-hui Wang,et al.  Oxidation and H2O/NaCl-induced corrosion behavior of sputtered Ni–Si coatings on Ti6Al4V at 600–650 °C , 2007 .

[14]  C. Coddet,et al.  Influence of alloying elements on the dissolution of oxygen in the metallic phase during the oxidation of titanium alloys , 1987 .

[15]  C. Leyens,et al.  Titanium and titanium alloys : fundamentals and applications , 2005 .

[16]  C. Coddet,et al.  Measurements of the adhesion of thermal oxide films: application to the oxidation of titanium , 1987 .

[17]  P. K. Datta,et al.  Air oxidation behaviour of Ti6Al4V alloy between 650 and 850 , 1994 .

[18]  Xiaoying Li,et al.  Characterisation of the palladium-modified thermal oxidation-treated titanium , 2002 .

[19]  Per Kofstad,et al.  High Temperature Corrosion , 1988 .

[20]  Hongbiao Dong,et al.  Enhanced wear resistance of titanium surfaces by a new thermal oxidation treatment , 2000 .

[21]  R. N. Shenoy,et al.  Oxidation of commercial purity titanium , 1986 .

[22]  Xiaoying Li,et al.  Oxygen boost diffusion for the deep-case hardening of titanium alloys , 2000 .

[23]  M. F. Stroosnijder,et al.  On the Determination of Diffusion Coefficients of Oxygen in One-Phase Ti (α-Ti) and Two-Phase Ti–4Nb (α- and β-Ti) by Micro-Hardness Measurements , 2001 .

[24]  Yun-De Lu,et al.  Effect of Nb on the high temperature oxidation of Ti (0-50 at.%)Al , 2002 .

[25]  S. Frangini,et al.  Various aspects of the air oxidation behaviour of a Ti6Al4V alloy at temperatures in the range 600–700 °C , 1994, Journal of Materials Science.

[26]  H. Cimenoglu,et al.  Surface modification of a Ti–6Al–4V alloy by thermal oxidation , 2005 .