Electroless Ni-P and Ni-P-Al2O3 Nanocomposite Coatings and Their Corrosion and Wear Resistance

[1]  Ashutosh Kumar Singh,et al.  Corrosion and wear resistance study of Ni-P and Ni-P-PTFE nanocomposite coatings , 2011 .

[2]  D. Sun,et al.  Effect of Nano-Al2O3 Particles on the NiP/nano-Al2O3 Coatings’ Properties , 2011 .

[3]  Weigang Huang,et al.  Preparation and characterization of Ni-P-nanoTiN electroless composite coatings , 2011 .

[4]  D. Vojtěch,et al.  Influence of heat treatment on tribological properties of electroless Ni–P and Ni–P–Al2O3 coatings on Al–Si casting alloy , 2010 .

[5]  B. Ramamoorthy,et al.  Novel approaches on the study of wear performance of electroless Ni–P/diamond composite deposites , 2009 .

[6]  Di Wu,et al.  Modeling of Strain-Induced Precipitation Kinetics and Evolution of Austenite Grains in Nb Microalloyed Steels , 2008 .

[7]  Lin Cheng,et al.  The effect of SiC particles added in electroless Ni–P plating solution on the properties of composite coatings , 2008 .

[8]  A. Hamdy,et al.  Corrosion behavior of electroless Ni–P alloy coatings containing tungsten or nano-scattered alumina composite in 3.5% NaCl solution , 2007 .

[9]  J. Balaraju,et al.  Electroless Deposition and Characterization of High Phosphorus Ni-P-Si3N4 Composite Coatings , 2007, International Journal of Electrochemical Science.

[10]  A. K. Suri,et al.  Preparation and characterization of silicon nitride codeposited electroless nickel composite coatings , 2007 .

[11]  Xinglong Dong,et al.  Synthesis and tribological behavior of electroless Ni-P-WC nanocomposite coatings , 2007 .

[12]  S. Alirezaei,et al.  Wear behavior of Ni–P and Ni–P–Al2O3 electroless coatings , 2007 .

[13]  Charles S. Barrett,et al.  The Structure of Metals , 1904, Nature.

[14]  Z. Hamid,et al.  Novel composite coatings containing (TiC–Al2O3) powder , 2007 .

[15]  J. Balaraju,et al.  Influence of particle size on the microstructure, hardness and corrosion resistance of electroless Ni–P–Al2O3 composite coatings , 2006 .

[16]  M. Staia,et al.  Wear mechanism of Ni–P–BN(h) composite autocatalytic coatings , 2005 .

[17]  J. Balaraju,et al.  Electroless deposition of Ni–Cu–P, Ni–W–P and Ni–W–Cu–P alloys , 2005 .

[18]  T. narayanan,et al.  Electroless Ni–P/Ni–B duplex coatings: preparation and evaluation of microhardness, wear and corrosion resistance , 2003 .

[19]  Stefano Rossi,et al.  Corrosion protection properties of electroless Nickel/PTFE, Phosphate/MoS2 and Bronze/PTFE coatings applied to improve the wear resistance of carbon steel , 2003 .

[20]  Joseph R. Davis Surface Engineering for Corrosion and Wear Resistance , 2001 .

[21]  A. Molinari,et al.  Surface durability of electroless Ni–P composite deposits , 1999 .

[22]  A. Saatchi,et al.  Deposition and properties of electroless nickel-phosphorus-molybdenum disulfide composites , 1997 .

[23]  M. Staia,et al.  Wear performance and mechanism of electroless NiP coating , 1996 .

[24]  R. Daniels,et al.  Structural changes induced by heating in electroless nickel-phosphorus alloys , 1988 .

[25]  A. Müller The Structure of Metals , 1881, The American journal of dental science.

[26]  Guang-hong Zhou,et al.  Structure and Mechanical Properties of Ni-P-Nano Al2 O3 Composite Coatings Synthesized by Electroless Plating , 2008 .

[27]  M. Yao,et al.  Characterization of electroless Ni--P--PTFE composite deposits , 1998 .

[28]  Pradyot Patnaik,et al.  Handbook of Inorganic Chemicals , 1997 .