An Experimental Study on the Thermal Stability of Mg2Si/Ni Interface under Thermal Cycling

Mg2Si is a promising eco-friendly thermoelectric material, and Ni is suited for electrical contact on it. In this study, Bi-doped Mg2Si ingots with Ni contacts were fabricated by co-sintering, and thermal stability was investigated by long-time (500 h, 500 cycles) temperature cycling from 25 °C to a peak temperature (Th = 400 and 450 °C) in N2. The as-sintered Ni/Mg2Si interfacial region is a multilayer consisting of Mg3Bi2, a series of MgxSiyNiz ternary compounds (ω, ν, ζ, and η-phases), and MgNi2. In the complex microstructure, the MgNi2 / η-phase interface was vulnerable to stress-induced voiding at Th = 450 °C, which arises from the mismatch of the thermal expansion coefficients. Interfacial voiding was avoided by adding 10 mol% Ag in Ni, which is probably due to the suppression of vacancy migration by the Ag-containing 2nd phase formation at the MgNi2/η-phase interface.

[1]  A. Abbasi,et al.  A new intermetallic phase formation in Mg Si Ni magnesium-based in-situ formed alloys , 2019, Vacuum.

[2]  Z. A. Munir,et al.  Interfacial properties of Cu/Ni/Mg2Si joints prepared in one step by the spark plasma sintering method , 2017 .

[3]  J. Janek,et al.  Thermal Stability of Magnesium Silicide/Nickel Contacts , 2016, Journal of Electronic Materials.

[4]  M. Imai,et al.  Thermal expansion of semiconducting silicides β-FeSi2 and Mg2Si , 2015 .

[5]  P. Ziółkowski,et al.  Fabrication and characterization of nickel contacts for magnesium silicide based thermoelectric generators , 2015 .

[6]  G. J. Snyder,et al.  Low Electron Scattering Potentials in High Performance Mg2Si0.45Sn0.55 Based Thermoelectric Solid Solutions with Band Convergence , 2013 .

[7]  Wei Liu,et al.  Convergence of conduction bands as a means of enhancing thermoelectric performance of n-type Mg2Si(1-x)Sn(x) solid solutions. , 2012, Physical review letters.

[8]  D. Castro,et al.  Void growth modeling upon electromigration stressing in narrow copper lines , 2007 .

[9]  E. A. Gurieva,et al.  Highly effective Mg 2 Si 1 − x Sn x thermoelectrics , 2006 .

[10]  P. Ziółkowski,et al.  Potential-Seebeck-microprobe (PSM): measuring the spatial resolution of the Seebeck coefficient and the electric potential , 2005, ICT 2005. 24th International Conference on Thermoelectrics, 2005..

[11]  J. Bisschop,et al.  Fast thermal cycling-enhanced electromigration in power metallization , 2004, IEEE Transactions on Device and Materials Reliability.

[12]  Kirsten Weide-Zaage,et al.  Simulation of time depending void formation in copper, aluminum and tungsten plugged via structures , 2003, Microelectron. Reliab..

[13]  Y. Kato,et al.  Stress-induced voiding in stacked tungsten via structure , 1999, 1998 IEEE International Reliability Physics Symposium Proceedings. 36th Annual (Cat. No.98CH36173).

[14]  O. Chang-Seok,et al.  Assessment of the mg-bi system , 1992 .

[15]  K. Nishio,et al.  Silicide modules practical issues in developing Mg2Si with good stability for generating power from waste heat sources , 2017 .

[16]  E. A. Gurieva,et al.  Highly effective Mg2Si1- xSnx thermoelectrics , 2006 .

[17]  R. Varin,et al.  Phase equilibria and intermetallic phases in the Ni-Si-Mg ternary system , 2001 .

[18]  R. Varin,et al.  New intermetallic phases in the NiSiMg ternary system , 1998 .