Ablation depth control with 40 nm resolution on ITO thin films using a square, flat top beam shaped femtosecond NIR laser

Abstract We reported on the ablation depth control with a resolution of 40 nm on indium tin oxide (ITO) thin film using a square beam shaped femtosecond (190 fs) laser (λp=1030 nm). A slit is used to make the square, flat top beam shaped from the Gaussian spatial profile of the femtosecond laser. An ablation depth of 40 nm was obtained using the single pulse irradiation at a peak intensity of 2.8 TW/cm2. The morphologies of the ablated area were characterized using an optical microscope, atomic force microscope (AFM), and energy dispersive X-ray spectroscopy (EDS). Ablations with square and rectangular types with various sizes were demonstrated on ITO thin film using slits with varying x–y axes. The stereo structure of the ablation with the depth resolution of approximately 40 nm was also fabricated successfully using the irradiation of single pulses with different shaped sizes of femtosecond laser.

[1]  Suwas Nikumb,et al.  Femtosecond laser patterning of Ta0.1W0.9Ox/ITO thin film stack , 2007 .

[2]  G. Perrone,et al.  Indium tin oxide overlayered waveguides for sensor applications. , 1997, Applied optics.

[3]  C. Barbero,et al.  Simple fabrication of active electrodes using direct laser transference , 2014 .

[4]  M. Gedvilas,et al.  Patterning of ITO Layer on Glass with High Repetition Rate Picosecond Lasers , 2007 .

[5]  Mikio Takai,et al.  EFFECT OF SUBSTRATE ABSORPTION ON THE EFFICIENCY OF LASER PATTERNING OF INDIUM TIN OXIDE THIN FILMS , 1999 .

[6]  S. Kwon,et al.  A new laser direct etching method of indium tin oxide electrode for application to alternative current plasma display panel , 2009 .

[7]  Jianzhao Li,et al.  F2-laser patterning of indium tin oxide (ITO) thin film on glass substrate , 2006 .

[8]  Wen-Wei Shen,et al.  Fabrication of micro/nano crystalline ITO structures by femtosecond laser pulses , 2010 .

[9]  A. Mitwalsky,et al.  Microstructure and etching properties of sputtered indium—tin oxide (ITO) , 1991 .

[10]  S. Tseng,et al.  Laser patterning with beam shaping on indium tin oxide thin films of glass/plastic substrate , 2009 .

[11]  Mindaugas Gedvilas,et al.  Patterning of indium–tin oxide on glass with picosecond lasers , 2007 .

[12]  D F Farson,et al.  Direct-write patterning of indium-tin-oxide film by high pulse repetition frequency femtosecond laser ablation. , 2007, Applied optics.

[13]  S. Lei,et al.  Femtosecond laser ablation of indium tin-oxide narrow grooves for thin film solar cells , 2013 .

[14]  Hye Yong Chu,et al.  Ultrafast laser ablation of indium tin oxide thin films for organic light-emitting diode application , 2006 .

[15]  R. Hellmann,et al.  Influence of film thickness on laser ablation threshold of transparent conducting oxide thin-films , 2014 .

[16]  Han Kim,et al.  Direct laser patterning of transparent ITO–Ag–ITO multilayer anodes for organic solar cells , 2015 .

[17]  Parallel patterning of indium tin oxide with ultra short pulses , 2013 .

[18]  Dara Feili,et al.  Sub-100 nm structuring of indium-tin-oxide thin films by sub-15 femtosecond pulsed near-infrared laser light. , 2012, Optics letters.

[19]  Chung-Wei Cheng,et al.  High precision patterning of ITO using femtosecond laser annealing process , 2014 .

[20]  Razvan Stoian,et al.  Fundamentals and advantages of ultrafast micro-structuring of transparent materials , 2003 .