Absence of defect state creation in nanocrystalline silicon thin film transistors deduced from constant current stress measurements

The authors discuss time and temperature dependences of the shift in threshold voltage (Delta V-T) of nanocrystalline silicon (nc-Si) thin film transistors (TFTs) stressed at constant drain currents. In contrast to the behavior of the hydrogenated amorphous silicon (a-Si:H) counterpart, a weak temperature dependence of Delta V-T was observed. The results follow the charge trapping model and the predicted stretched-exponential time dependence that saturates at prolonged stress times. In addition, Delta V-T does not fit into the thermalization energy concept that was developed based on the defect state creation model for a-Si:H TFTs. The results indicate absence of defect state creation in nc-Si TFTs.

[1]  I. D. French,et al.  Bias dependence of instability mechanisms in amorphous silicon thin‐film transistors , 1987 .

[2]  J. R. Hughes,et al.  Time and temperature dependence of instability mechanisms in amorphous silicon thin-film transistors , 1989 .

[3]  Jerzy Kanicki,et al.  Bias‐stress‐induced stretched‐exponential time dependence of charge injection and trapping in amorphous thin‐film transistors , 1993 .

[4]  Ralf B. Wehrspohn,et al.  Unification of the time and temperature dependence of dangling-bond-defect creation and removal in amorphous-silicon thin-film transistors , 1998 .

[5]  Regis Vanderhaghen,et al.  Stable microcrystalline silicon thin-film transistors produced by the layer-by-layer technique , 1999 .

[6]  Augusto Nascetti,et al.  Metastability of hot-wire amorphous-silicon thin-film transistors , 2000 .

[7]  M. J. Powell,et al.  Relative importance of the Si–Si bond and Si–H bond for the stability of amorphous silicon thin film transistors , 2000 .

[8]  M. J. Powell,et al.  Stability of plasma deposited thin film transistors comparison of amorphous and microcrystalline silicon , 2001 .

[9]  W. Anderson,et al.  Thin-film transistors on plastic and glass substrates using silicon deposited by microwave plasma ECR-CVD , 2003, IEEE Electron Device Letters.

[10]  S. Wagner,et al.  Nanocrystalline silicon thin film transistors , 2003 .

[11]  Takatoshi Tsujimura,et al.  Amorphous/Microcrystalline Silicon Thin Film Transistor Characteristics for Large Size Oled Television Driving , 2004 .

[12]  A. Nathan,et al.  Drain-bias dependence of threshold voltage stability of amorphous silicon TFTs , 2004, IEEE Electron Device Letters.

[13]  Kapil Sakariya,et al.  Threshold voltage instability of amorphous silicon thin-film transistors under constant current stress , 2005 .

[14]  Arokia Nathan,et al.  High-mobility nanocrystalline silicon thin-film transistors fabricated by plasma-enhanced chemical vapor deposition , 2005 .

[15]  John Robertson,et al.  Instability measurements in amorphous hydrogenated silicon using capacitance-voltage techniques , 2005 .

[16]  A. Nathan,et al.  Stability of nc-Si:H TFTs With Silicon Nitride Gate Dielectric , 2007, IEEE Transactions on Electron Devices.