Fracture behavior and mechanism of 2D C/SiC–BCx composite at room temperature

[1]  Q. Zeng,et al.  Preparation and oxidation resistance of 2D C/SiC composites modified by partial boron carbide self-sealing matrix , 2008 .

[2]  F. Rebillat,et al.  Self-healing mechanisms of a SiC fiber reinforced multi-layered ceramic matrix composite in high pressure steam environments , 2007 .

[3]  F. Christin A Global Approach to Fiber nD Architectures and Self-Sealing Matrices: From Research to Production , 2005 .

[4]  Jan Schulte-Fischedick,et al.  Oxidation behaviour of C/C–SiC coated with SiC–B4C–SiC–cordierite oxidation protection system , 2004 .

[5]  R. Naslain Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview , 2004 .

[6]  Xavier Bourrat,et al.  Boron-bearing species in ceramic matrix composites for long-term aerospace applications , 2004 .

[7]  Barry Marsden,et al.  A numerical study on the application of the Weibull theory to brittle materials , 2001 .

[8]  Xavier Bourrat,et al.  Synthesis of highly tailored ceramic matrix composites by pressure-pulsed CVI , 2001 .

[9]  J. Viricelle,et al.  Oxidation behaviour of a multi-layered ceramic-matrix composite (SiC)f/C/(SiBC)m , 2001 .

[10]  R. Pailler,et al.  Oxidation-resistant carbon-fiber-reinforced ceramic-matrix composites , 1999 .

[11]  R. Pailler,et al.  A Multilayer Ceramic Matrix for Oxidation Resistant Carbon Fibers-Reinforced CMCs , 1998 .

[12]  S. Phoenix,et al.  The single-filament-composite test: a new statistical theory for estimating the interfacial shear strength and Weibull parameters for fiber strength , 1998 .

[13]  L. Vandenbulcke,et al.  The oxidation behaviour of two- and three-dimensional C/SiC thermostructural materials protected by chemical-vapour-deposition polylayers coatings , 1994, Journal of Materials Science.

[14]  Jacques Lamon,et al.  Statistical Approaches to Failure for Ceramic Reliability Assessment , 1988 .