Infiltration behavior of Cu and Ti fillers into Ti2AlC/Ti3AlC2 composites during tungsten inert gas (TIG)brazing
暂无分享,去创建一个
T. Sahraoui | N. Chiker | M. Hadji | M. Barsoum | M. Azzaz | Y. Hadji | A. Haddad | M. Yahi | M. Benammar
[1] T. Sahraoui,et al. Microstructure and microindentation of Ti3SiC2 – Titanium filler brazed joints by tungsten inert gas (TIG) process , 2017 .
[2] O. Dezellus,et al. Experimental evidence of copper insertion in a crystallographic structure of Ti3SiC2 MAX phase , 2015 .
[3] G. Fan,et al. Microstructure evolution and brazing mechanism of Ti2AlC–Ti2AlC joint by using pure-silver filler metal , 2015 .
[4] B. Hallstedt,et al. Thermodynamic description of the Al–C–Ti system , 2015 .
[5] Yanming He,et al. Effect of joining temperature and holding time on microstructure and shear strength of Ti2AlC/Cu joints brazed using Ag-Cu filler alloy , 2013 .
[6] K. Suganuma. Joining Ceramics and Metals , 2013 .
[7] M. Barsoum,et al. Structure of a new bulk Ti5Al2C3 MAX phase produced by the topotactic transformation of Ti2AlC , 2012 .
[8] Isabelle Choquet,et al. Review of Arc Efficiency Values for Gas Tungsten Arc Welding , 2012 .
[9] R. Drew,et al. Joining of engineering ceramics , 2009 .
[10] T. Cabioc’h,et al. Reaction synthesis of layered ternary Ti2AlC ceramic , 2009 .
[11] M. Barsoum,et al. Tribological behavior of select MAX phases against Al2O3 at elevated temperatures , 2008 .
[12] Yanchun Zhou,et al. A first-principles investigation of the phase stability of Ti(2)AlC with Al vacancies , 2008 .
[13] Y. Zhou,et al. Structure stability of Ti3AlC2 in Cu and microstructure evolution of Cu-Ti3AlC2 composites , 2007 .
[14] A. K. Ray,et al. Characterization of interface of Al2O3–304 stainless steel braze joint , 2007 .
[15] Yanchun Zhou,et al. Microstructure and mechanical strength of transient liquid phase bonded Ti3SiC2 joints using Al interlayer , 2007 .
[16] R. Ahuja,et al. Electronic structure and chemical bonding in Ti2AlC investigated by soft x-ray emission spectroscopy , 2006, 1111.2910.
[17] K. Frisk. A revised thermodynamic description of the Ti–C system , 2003 .
[18] Yong Huang,et al. A possible mechanism on synthesis of Ti3AlC2 , 2003 .
[19] Yanfei Zhou,et al. High-Temperature Oxidation Behavior of Ti2AlC in Air , 2003 .
[20] Michel W. Barsoum,et al. The MN+1AXN phases: A new class of solids , 2000 .
[21] H. Wenk,et al. MAUD: a friendly Java program for material analysis using diffraction , 1999 .
[22] M. Barsoum,et al. Layered machinable ceramics for high temperature applications , 1997 .
[23] Pierre Villars,et al. Handbook of Ternary Alloy Phase Diagrams , 1995 .
[24] M. De,et al. An X‐ray determination of the thermal expansion of α‐phase Cu–Si alloys at high temperature , 1986 .
[25] C. J. Engberg,et al. THERMAL EXPANSION OF AlO, BeO, MgO, BC, SiC, AND TiC ABOVE 1000 C , 1959 .