Grain-refinement mechanisms in titanium alloys

Despite the importance of the prior-beta grain structure in determining the properties of titanium-based alloys, there are few published studies on methods of controlling the size of these grains in commercial alloys. The existing research raises questions about the relative importance of solute elements in grain-refining mechanisms, particularly the common alloying elements of aluminum and vanadium. The effect of these elements was investigated by producing a series of castings in a nonconsumable arc-melting furnace, and the results were interpreted with the aid of available phase-diagram information and solute-based models of grain refinement. A small reduction in grain size was obtained with increasing solute additions; however, this was not expected from the theoretical analysis. Possible reasons for this discrepancy are discussed.

[1]  G. V. Samsonov,et al.  Effect of transition metals on the grain size of titanium , 1970 .

[2]  S. Burns,et al.  Improved toughness from prior beta grains in Ti6A14V , 1977 .

[3]  D. G. McCartney Grain refining of aluminium and its alloys using inoculants , 1989 .

[4]  H. Baker,et al.  Alloy phase diagrams , 1992 .

[5]  J. Yu,et al.  Corrosion fatigue resistances of surgical implant stainless steels and titanium alloy , 1993 .

[6]  A. K. Dahle,et al.  On the assumption of an additive effect of solute elements in dendrite growth , 1997 .

[7]  A. K. Dahle,et al.  The effect of grain refinement and silicon content on grain formation in hypoeutectic Al–Si alloys , 1999 .

[8]  D. StJohn,et al.  Partitioning of titanium during solidification of aluminium alloys , 2000 .

[9]  W. G. Frazier,et al.  Effect of prior β-grain size on the hot deformation behavior of Ti-6Al-4V: Coarse vs coarser , 2000 .

[10]  D. StJohn,et al.  A model of grain refinement incorporating alloy constitution and potency of heterogeneous nucleant particles , 2001 .

[11]  A. Kamiya,et al.  Influence of boron addition on microstructure and mechanical properties of dental cast titanium alloys , 2003 .

[12]  T. Bieler,et al.  An automated method to determine the orientation of the high-temperature beta phase from measured EBSD data for the low-temperature alpha-phase in Ti–6Al–4V , 2003 .

[13]  Peter Schumacher,et al.  Grain Refinement of Aluminium Alloys by Inoculation , 2003 .

[14]  M. Ramulu,et al.  Influence of grain size and microstructure on oxidation rates in titanium alloy Ti-6Al-4V under superplastic forming conditions , 2004 .

[15]  V. Stolyarov,et al.  Corrosion resistance of ultra fine-grained Ti , 2004 .

[16]  P. Comley Manufacturing advantages of superplastically formed fine-grain Ti-6Al-4V alloy , 2004 .

[17]  D. StJohn,et al.  Grain refinement of magnesium alloys , 2005 .

[18]  D. Miracle,et al.  Grain refinement of cast titanium alloys via trace boron addition , 2005 .

[19]  D. StJohn,et al.  An analysis of the relationship between grain size, solute content, and the potency and number density of nucleant particles , 2005 .

[20]  D. Miracle,et al.  Processing, microstructure, and properties of β titanium alloys modified with boron , 2005 .