Suspension thermal spraying of hydroxyapatite: microstructure and in vitro behaviour.
暂无分享,去创建一个
Rainer Gadow | Devis Bellucci | Valeria Cannillo | Luca Lusvarghi | Andreas Killinger | Antonella Sola | Luigi De Nardo | L. Altomare | A. Sola | R. Gadow | A. Killinger | D. Bellucci | V. Cannillo | G. Bolelli | L. De Nardo | Philipp Müller | Giovanni Bolelli | Nico Stiegler | Lina Altomare | L. Lusvarghi | N. Stiegler | Philipp Müller | P. Müller
[1] M. Krane,et al. Column Formation in Suspension Plasma-Sprayed Coatings and Resultant Thermal Properties , 2011 .
[2] B. Bonferroni,et al. Microstructure and in vitro behaviour of 45S5 bioglass coatings deposited by high velocity suspension flame spraying (HVSFS) , 2011, Journal of materials science. Materials in medicine.
[3] R. Mcpherson. A model for the thermal conductivity of plasma-sprayed ceramic coatings , 1984 .
[4] K. Khor,et al. Significance of melt-fraction in HVOF sprayed hydroxyapatite particles, splats and coatings. , 2004, Biomaterials.
[5] R. Gadow,et al. Properties of High Velocity Suspension Flame Sprayed (HVSFS) TiO2 coatings , 2009 .
[6] Khiam Aik Khor,et al. PHASE TRANSFORMATIONS IN PLASMA SPRAYED HYDROXYAPATITE COATINGS , 1999 .
[7] C. James,et al. Long-term follow-up of a hydroxyapatite ceramic-coated threaded cup: an analysis of survival and fixation at up to 15 years. , 2007, The Journal of arthroplasty.
[8] R. Gadow,et al. High-Velocity Suspension Flame Sprayed (HVSFS) Hydroxyapatite Coatings for Biomedical Applications , 2012, Journal of Thermal Spray Technology.
[9] K. Rungcharassaeng,et al. Peri-implant tissue response of immediately loaded, threaded, HA-coated implants: 1-year results. , 2002, The Journal of prosthetic dentistry.
[10] G. Georgiou,et al. Hydroxyapatite, fluor-hydroxyapatite and fluorapatite produced via the sol-gel method: bonding to titanium and scanning electron microscopy. , 2013, Dental materials : official publication of the Academy of Dental Materials.
[11] J. Nohava,et al. Interesting aspects of indentation and scratch methods for characterization of thermally-sprayed coatings , 2010 .
[12] H. Farnoush,et al. Sol–gel derived nanohydroxyapatite film on friction stir processed Ti–6Al–4V substrate , 2013 .
[13] M. Fitzpatrick,et al. Neutron diffraction residual strain measurements in nanostructured hydroxyapatite coatings for orthopaedic implants. , 2011, Journal of the mechanical behavior of biomedical materials.
[14] P. Chandran,et al. Periprosthetic Bone Remodeling after 12 Years Differs in Cemented and Uncemented Hip Arthroplasties , 2012, Clinical orthopaedics and related research.
[15] Michael C. Mosier,et al. Hydroxyapatite (HA) coating appears to be of benefit for implant durability of tibial components in primary total knee arthroplasty , 2011, Acta orthopaedica.
[16] B. Marple,et al. High weibull modulus HVOF titania coatings , 2003 .
[17] E. Dongmo,et al. Numerical approach and optimization of the combustion and gas dynamics in High Velocity Suspension Flame Spraying (HVSFS) , 2009 .
[18] J. Jansen,et al. Calcium phosphate coatings for medical implants , 1998, Proceedings of the Institution of Mechanical Engineers. Part H, Journal of engineering in medicine.
[19] L. Visai,et al. Titanium Oxide Antibacterial Surfaces in Biomedical Devices , 2011, The International journal of artificial organs.
[20] H. N. Cheang,et al. Surface characteristics and dissolution behavior of plasma-sprayed hydroxyapatite coating. , 2002, Journal of biomedical materials research.
[21] T. Lui,et al. Effect of crystallization on the bonding strength and failures of plasma-sprayed hydroxyapatite , 2007 .
[22] C. C. Berndt,et al. The variability in strength of thermally sprayed coatings , 1988 .
[23] C. Berndt,et al. Biomedical Application of Apatites , 2002 .
[24] C. Berndt,et al. Thermal Analysis of Amorphous Phases in Hydroxyapatite Coatings , 2005 .
[25] A. Sola,et al. Deposition mechanisms in high velocity suspension spraying: Case study for two bioactive materials , 2012 .
[26] T. Lui,et al. Microstructural self-healing effect of hydrothermal crystallization on bonding strength and failure mechanism of hydroxyapatite coatings , 2008 .
[27] E. Skwarek,et al. The study of the properties of the hydroxyapatite/electrolyte interface , 2009 .
[28] R. Gadow,et al. Microstructural and in vitro characterisation of high-velocity suspension flame sprayed (HVSFS) bioactive glass coatings , 2009 .
[29] C. Y. Ho,et al. Thermophysical properties of matter - the TPRC data series. Volume 14. Master index - to materials and properties. (Reannouncement). Data book , 1979 .
[30] W. Capello,et al. Hydroxyapatite coated femoral components , 2015 .
[31] Rainer Gadow,et al. High velocity suspension flame sprayed (HVSFS) potassium-based bioactive glass coatings with and without TiO2 bond coat , 2012 .
[32] R. Cuscó,et al. Differentiation between hydroxyapatite and β-tricalcium phosphate by means of μ-Raman spectroscopy , 1998 .
[33] D. D’Lima,et al. Hydroxyapatite-Coated Femoral Stem Survivorship at 10 Years , 2005 .
[34] K. A. Khora,et al. Significance of melt-fraction in HVOF sprayed hydroxyapatite particles, splats and coatings , 2003 .
[35] 尹志坚,et al. Evaluating microhardness of plasma sprayed Al2O3 coatings using Vickers indentation techniques , 2007 .
[36] R. Gadow,et al. Microstructural and Tribological Investigation of High-Velocity Suspension Flame Sprayed (HVSFS) Al2O3 Coatings , 2009 .
[37] T. Albrektsson,et al. Osteoinduction, osteoconduction and osseointegration , 2001, European Spine Journal.
[38] Xuanyong Liu,et al. Effect of hydroxyapatite coating crystallinity on dissolution and osseointegration in vivo. , 2005, Journal of biomedical materials research. Part A.
[39] R. Heimann. Characterization of as‐plasma‐sprayed and incubated hydroxyapatite coatings with high resolution techniques , 2009 .
[40] O. Reikerås,et al. Long-term results of HA coated threaded versus HA coated hemispheric press fit cups: 287 hips followed for 11 to 16 years , 2006, Archives of Orthopaedic and Trauma Surgery.
[41] T. Lei,et al. Osteoblastic cell response on biphasic fluorhydroxyapatite/strontium-substituted hydroxyapatite coatings. , 2014, Journal of biomedical materials research. Part A.
[42] Young-yool Chung,et al. Measurement of extent of bone ongrowth and hydroxyapatite absorption in retrieved acetabular cups , 2008, Journal of orthopaedic science : official journal of the Japanese Orthopaedic Association.
[43] M. Ameil,et al. Survival analysis at 10 years of a cohort of 297 atlas total hip prostheses , 2007, European Journal of Orthopaedic Surgery & Traumatology.
[44] L. Palm,et al. Hydroxyapatite coating improves 8- to 10-year performance of the link RS cementless femoral stem. , 2002, The Journal of arthroplasty.
[45] M. Manley,et al. Fixation Choices for Primary Hip and Knee Applications , 2006 .
[46] W. Capello,et al. Hydroxyapatite-coated Femoral Components: 15-Year Minimum Followup , 2006, Clinical orthopaedics and related research.
[47] Sen Yang,et al. Adhesion strength of plasma-sprayed hydroxyapatite coatings on laser gas-nitrided pure titanium , 2009 .
[48] E. Liarokapis,et al. Micro-Raman and FTIR studies of synthetic and natural apatites. , 2007, Biomaterials.
[49] Hua Li,et al. HVOF spraying of nanostructured hydroxyapatite for biomedical applications , 2005 .
[50] R. Gadow,et al. Effect of the suspension composition on the microstructural properties of high velocity suspension flame sprayed (HVSFS) Al2O3 coatings , 2010 .
[51] A. Sosna,et al. Hydroxyapatite porous coating and the osteointegration of the total hip replacement , 2007, Archives of Orthopaedic and Trauma Surgery.
[52] K. Khor,et al. An in vitro investigation of plasma sprayed hydroxyapatite (HA) coatings produced with flame-spheroidized feedstock. , 2002, Biomaterials.
[53] R. Petit. The use of hydroxyapatite in orthopaedic surgery: A ten-year review , 1999, European Journal of Orthopaedic Surgery & Traumatology.
[54] C. Qiu,et al. Manufacturing Process of Nanostructured Alumina Coatings by Suspension Plasma Spraying , 2009 .
[55] P. K. Panigrahi,et al. Room temperature synthesis of highly hemocompatible hydroxyapatite, study of their physical properties and spectroscopic correlation of particle size. , 2010, Nanoscale.
[56] P. Fauchais,et al. Phenomena Involved in Suspension Plasma Spraying Part 2: Zirconia Particle Treatment and Coating Formation , 2006 .
[57] Gwo‐Jaw Wang,et al. Eight-year results of hydroxyapatite-coated hip arthroplasty. , 2006, The Journal of arthroplasty.
[58] R. Heimann,et al. Laser‐Raman and Nuclear Magnetic Resonance (NMR) studies on plasma‐sprayed hydroxylapatite coatings: Influence of bioinert bond coats on phase composition and resorption kinetics in simulated body fluid , 2003 .
[59] R. Gadow,et al. Advances in High Velocity Suspension Flame Spraying (HVSFS) , 2009 .
[60] Jingchuan Zhu,et al. Optimal design and fabrication of hydroxyapatite-Ti asymmetrical functionally graded biomaterial , 2003 .
[61] Rainer Gadow,et al. Modeling of Combustion as well as Heat, Mass, and Momentum Transfer During Thermal Spraying by HVOF and HVSFS , 2009 .
[62] D. Tarnow,et al. Five-year prospective clinical evaluation of highly crystalline HA MP-1-coated dental implants. , 2008, The Journal of oral implantology.
[63] H. Rezaie,et al. In vitro antibacterial evaluation of sol-gel-derived Zn-, Ag-, and (Zn + Ag)-doped hydroxyapatite coatings against methicillin-resistant Staphylococcus aureus. , 2013, Journal of biomedical materials research. Part A.
[64] B. Cetegen,et al. Modeling of liquid ceramic precursor droplets in a high velocity oxy-fuel flame jet , 2008 .
[65] O. Reikerås,et al. Excellent results with femoral revision surgery using an extensively hydroxyapatite-coated stem: 59 patients followed for 10–16 years , 2006, Acta orthopaedica.
[66] M. Chu,et al. Pressureless sintering of nanocrystalline hydroxyapatite at different temperatures , 2010 .
[67] 若月達也. Hydroxyapatite , 2023, Reactions Weekly.
[68] E. Wintermantel,et al. Chemical and morphological changes of vacuum-plasma-sprayed hydroxyapatite coatings during immersion in simulated physiological solutions , 2005 .
[69] M. Froimson,et al. Hydroxyapatite-Coated, Tapered Titanium Hip Arthroplasty , 2009 .
[70] J. Breme,et al. Development of a titanium alloy suitable for an optimized coating with hydroxyapatite. , 1995, Biomaterials.
[71] Y. Ha,et al. Cementless bipolar hemiarthroplasty using a hydroxyapatite-coated long stem for osteoporotic unstable intertrochanteric fractures. , 2011, The Journal of arthroplasty.
[72] G. G. Stokes. "J." , 1890, The New Yale Book of Quotations.
[73] S. Best,et al. Structural analysis of Si-substituted hydroxyapatite: zeta potential and X-ray photoelectron spectroscopy , 2002, Journal of materials science. Materials in medicine.
[74] J. Jansen,et al. Synthesis and application of nanostructured calcium phosphate ceramics for bone regeneration. , 2012, Journal of biomedical materials research. Part B, Applied biomaterials.
[75] G. Albertini,et al. Plasma sprayed hydroxyapatite coatings from nanostructured granules , 2008 .
[76] K A Gross,et al. Material fundamentals and clinical performance of plasma-sprayed hydroxyapatite coatings: a review. , 2001, Journal of biomedical materials research.
[77] C. Rey,et al. Hydroxyapatite coating on titanium by a low energy plasma spraying mini-gun , 2012 .
[78] Miloš B. Volf,et al. Mathematical approach to glass , 1988 .
[79] F. Ren,et al. Part II: fracture strength and elastic modulus as a function of porosity for hydroxyapatite and other brittle materials. , 2012, Journal of the mechanical behavior of biomedical materials.
[80] L. Rimondini,et al. Osteointegration of titanium and hydroxyapatite rough surfaces in healthy and compromised cortical and trabecular bone: in vivo comparative study on young, aged, and estrogen‐deficient sheep , 2007, Journal of orthopaedic research : official publication of the Orthopaedic Research Society.
[81] C. Ranawat,et al. The Hydroxyapatite-Tapered Stem: Any Added Value? , 2011 .
[82] H. Owada,et al. High-temperature stability of hydroxyl ions in yttrium-substituted oxyhydroxyapatites , 1991 .
[83] K. Søballe,et al. Inferior Survival of Hydroxyapatite versus Titanium-coated Cups at 15 Years , 2009, Clinical orthopaedics and related research.
[84] Jianguo Li,et al. Thermal expansion of hot isostatically pressed hydroxyapatite , 1994 .
[85] Shin-Yoon Kim,et al. Early Failure of Hemispheric Hydroxyapatite-coated Acetabular Cups , 2006, Clinical orthopaedics and related research.
[86] Tadashi Kokubo,et al. How useful is SBF in predicting in vivo bone bioactivity? , 2006, Biomaterials.
[87] S. Saber-Samandari,et al. Amorphous calcium phosphate offers improved crack resistance: a design feature from nature? , 2011, Acta biomaterialia.
[88] T. Lee,et al. Effect of post vacuum heating on the microstructural feature and bonding strength of plasma-sprayed hydroxyapatite coatings , 2006 .
[89] J. Vidalain. Twenty-year results of the cementless Corail stem , 2011, International Orthopaedics.
[90] H. F. Morris,et al. Hydroxyapatite-coated implants: a case for their use. , 1998, Journal of oral and maxillofacial surgery : official journal of the American Association of Oral and Maxillofacial Surgeons.
[91] C. Doyle,et al. Plasma sprayed hydroxyapatite coatings on titanium substrates. Part 2: optimisation of coating properties. , 1998, Biomaterials.
[92] J. Jansen,et al. Thin Calcium Phosphate Coatings for Medical Implants , 2009 .
[93] A. Wennerberg,et al. Different patterns of bone fixation with hydroxyapatite and resorbable CaP coatings in the rabbit tibia at 6, 12, and 52 weeks. , 2011, Journal of biomedical materials research. Part B, Applied biomaterials.
[94] P. Fauchais,et al. Phenomena Involved in Suspension Plasma Spraying Part 1: Suspension Injection and Behavior , 2006 .
[95] Robert B. Heimann,et al. Thermal spraying of biomaterials , 2006 .
[96] J. Goosen,et al. Excellent results from proximally HA-coated femoral stems with a minimum of 6 years follow-up , 2005, Acta orthopaedica.
[97] Saeed Saber-Samandari,et al. Evaluation of commercial implants with nanoindentation defines future development needs for hydroxyapatite coatings. , 2010, Journal of biomedical materials research. Part B, Applied biomaterials.
[98] L. Pawłowski,et al. Numerical simulation of hydroxyapatite powder behaviour in plasma jet , 2004 .
[99] K. Wong,et al. Early failure of smooth hydroxyapatite-coated press-fit acetabular cup--7 years of follow-up. , 2005, The Journal of arthroplasty.
[100] D. C. Agrawal,et al. Sol–gel derived hydroxyapatite coatings on titanium substrates , 2011 .
[101] F. Najafi,et al. Preparation and characterization of multi-walled carbon nanotube/hydroxyapatite nanocomposite film dip coated on Ti-6Al-4V by sol-gel method for biomedical applications: an in vitro study. , 2013, Materials science & engineering. C, Materials for biological applications.
[102] Takashi Nakamura,et al. Process and kinetics of bonelike apatite formation on sintered hydroxyapatite in a simulated body fluid. , 2005, Biomaterials.
[103] Rainer Gadow,et al. High-Velocity Suspension Flame Spraying (HVSFS), a new approach for spraying nanoparticles with hypersonic speed , 2006 .
[104] Toshio Uehara,et al. Histological evidence of osseointegration in human retrieved fractured hydroxyapatite-coated screw-type implants: a case report. , 2004, Clinical oral implants research.
[105] A. Riis,et al. Effect of hydroxyapatite coating on risk of revision after primary total hip arthroplasty in younger patients: Findings from the Danish Hip Arthroplasty Registry , 2007, Acta orthopaedica.
[106] Sam Zhang,et al. ADHESION STRENGTH OF SOL-GEL DERIVED FLUORIDATED HYDROXYAPATITE COATINGS , 2006 .
[107] M. Hamdia,et al. Sintering properties of hydroxyapatite powders prepared using different methods , 2012 .
[108] L. Nordsletten,et al. A prospective randomized study comparing electrochemically deposited hydroxyapatite and plasma-sprayed hydroxyapatite on titanium stems , 2011, Acta orthopaedica.
[109] K. Khor,et al. Plasma-sprayed hydroxyapatite (HA) coatings with flame-spheroidized feedstock: microstructure and mechanical properties. , 2000, Biomaterials.
[110] J. Laureyns,et al. Advanced Microstructural Study of Suspension Plasma Sprayed Hydroxyapatite Coatings , 2010 .
[111] Rainer Gadow,et al. Hydroxyapatite coatings for biomedical applications deposited by different thermal spray techniques , 2010 .
[112] C. Doyle,et al. Plasma sprayed hydroxyapatite coatings on titanium substrates. Part 1: Mechanical properties and residual stress levels. , 1998, Biomaterials.
[113] F. Carinci,et al. Five-year outcome of 111 immediate nonfunctional single restorations. , 2006, Journal of Oral Implantology.
[114] F. S. Baker,et al. Temperature-programmed dehydration of hydroxyapatite , 1979 .
[115] B. Del Curto,et al. Electrochemical surface modifications of titanium and titanium alloys for biomedical applications , 2012 .
[116] A. L. Patterson. The Scherrer Formula for X-Ray Particle Size Determination , 1939 .