Layered Machinable and Electrically Conductive Ti2AlC and Ti3AlC2 Ceramics: a Review

[1]  Ulf Jansson,et al.  The Mn+1AXn phases: Materials science and thin-film processing , 2010 .

[2]  I. Low,et al.  Oxidation characteristics of Ti3AlC2 over the temperature range 500–900 °C , 2009 .

[3]  Yanchun Zhou,et al.  In-situ synthesis of Ti3AlC2/TiC-Al2O3 composite from TiO2-Al-C system , 2009 .

[4]  Yanchun Zhou,et al.  Current Status in Layered Ternary Carbide Ti 3 SiC 2 , a Review , 2009 .

[5]  J. Heinrich,et al.  Reduction of the porcelain firing temperature by preparation of the raw materials , 2009 .

[6]  Yanchun Zhou,et al.  Surface Chemistry, Dispersion Behavior, and Slip Casting of Ti3AlC2 Suspensions , 2009 .

[7]  Xiaodong He,et al.  Rapid synthesis of bulk Ti_2AlC by self-propagating high temperature combustion synthesis with a pseudo-hot isostatic pressing process , 2009 .

[8]  K. Nickel,et al.  High-pressure powder x-ray diffraction experiments and ab initio calculation of Ti3AlC2 , 2009 .

[9]  Bingchu Mei,et al.  Effect of tin on the reaction synthesis of ternary carbide Ti3AlC2 , 2009 .

[10]  Yanchun Zhou,et al.  Recent Progress in Theoretical Prediction, Preparation, and Characterization of Layered Ternary Transition-Metal Carbides , 2009 .

[11]  Yanchun Zhou,et al.  Direct diffusion bonding of Ti3SiC2 and Ti3AlC2 , 2009 .

[12]  R. Ritchie,et al.  On the Fracture Toughness of Advanced Materials , 2009 .

[13]  S. Zwaag,et al.  Toughening of a ZrC Particle‐Reinforced Ti3AIC2 Composite , 2009 .

[14]  C. Yeh,et al.  Effects of using Al4C3 as a reactant on formation of Ti3AlC2 by combustion synthesis in SHS mode , 2009 .

[15]  C. L. Yeh,et al.  Effects of TiC and Al4C3 addition on combustion synthesis of Ti2AlC , 2009 .

[16]  Lin Cheng,et al.  Synthesis reactions for Ti3AlC2 through pulse discharge sintering TiH2/Al/C powder mixture , 2009 .

[17]  Yanchun Zhou,et al.  Reciprocating friction and wear behavior of Ti3AlC2 and Ti3AlC2/Al2O3 composites against AISI52100 bearing steel , 2009 .

[18]  J. Knott 25 years of Materials Science and Technology , 2009 .

[19]  Yanchun Zhou,et al.  First-principles investigation of intrinsic defects and (N, O) impurity atom stimulated Al vacancy in Ti2AlC , 2008 .

[20]  S. Zwaag,et al.  Early stages of oxidation of Ti3AlC2 ceramics , 2008 .

[21]  C. Yeh,et al.  Combustion synthesis of Ti3AlC2 from Ti/Al/C/TiC powder compacts , 2008 .

[22]  Michel W. Barsoum,et al.  Electronic and thermal properties of Ti3Al(C0.5,N0.5)2, Ti2Al(C0.5,N0.5) and Ti2AlN , 2008 .

[23]  D. Mckenzie,et al.  Elastic properties of Tin+1AlCn and Tin+1AlNn MAX phases , 2008 .

[24]  Yanchun Zhou,et al.  Ab initio modeling of the formation and migration of monovacancies in Ti2AlC , 2008 .

[25]  K. Stiller,et al.  Ti2AlC coatings deposited by High Velocity Oxy-Fuel spraying , 2008 .

[26]  Z. Zhang,et al.  Formation of a single-phase Ti3AlC2 from a mixture of Ti, Al and TiC powders with Sn as an additive , 2008 .

[27]  Y. Gogotsi,et al.  Micro and mesoporosity of carbon derived from ternary and binary metal carbides , 2008 .

[28]  Jow-Lay Huang,et al.  Investigation of ballistic impact properties and fracture mechanisms of Ti3SiC2 ternary ceramics , 2008 .

[29]  S. Hashimoto,et al.  Pressureless sintering and mechanical properties of titanium aluminum carbide , 2008 .

[30]  Yanchun Zhou,et al.  Microstructure, mechanical, and electrical properties of Cu–Ti_3AlC_2 and in situ Cu–TiC_x composites , 2008 .

[31]  D. Mckenzie,et al.  A solid phase reaction between TiCx thin films and Al2O3 substrates , 2008 .

[32]  N. D. Rago,et al.  Corrosion of ternary carbides by molten lead , 2008 .

[33]  Yanchun Zhou,et al.  A first-principles investigation of the phase stability of Ti(2)AlC with Al vacancies , 2008 .

[34]  Zhengming Sun,et al.  Low temperature synthesis of single-phase Ti3AlC2 through reactive sintering Ti/Al/C powders , 2008 .

[35]  J. Rau,et al.  Pulsed laser deposited hard TiC, ZrC, HfC and TaC films on titanium: Hardness and an energy-dispersive X-ray diffraction study , 2008 .

[36]  C. Li,et al.  In Situ Synthesis and Properties of Ti3AlC2/TiB2 Composites , 2007 .

[37]  Zhengming Sun,et al.  Mechanical behavior of Ti3AlC2 prepared by pulse discharge sintering method , 2007 .

[38]  Y. Zhou,et al.  Structure stability of Ti3AlC2 in Cu and microstructure evolution of Cu-Ti3AlC2 composites , 2007 .

[39]  Yanchun Zhou,et al.  Thermal stability of Ti3AlC2/Al2O3 composites in high vacuum , 2007 .

[40]  Peter Greil,et al.  Three-Dimensional Printing of Nanolaminated Ti3AlC2 Toughened TiAl3–Al2O3 Composites , 2007 .

[41]  M. Radovic,et al.  Microstructure and Residual Stress of Alumina Scale Formed on Ti2AlC at High Temperature in Air , 2007 .

[42]  Xiong Yin,et al.  Diffusion bonding of Ti3AlC2 ceramic via a Si interlayer , 2007 .

[43]  Zhengming Sun,et al.  Rapid synthesis of single-phase Ti3AlC2 through pulse discharge sintering a TiH2/Al/TiC powder mixture , 2007 .

[44]  D. Lee,et al.  High Temperature Corrosion of Ti3AlC2 in Ar-1%SO2 Atmosphere , 2007 .

[45]  L. Peng Preparation and Properties of Ternary Ti3AlC2 and its Composites from Ti–Al–C Powder Mixtures With Ceramic Particulates , 2007 .

[46]  W. Zhou,et al.  Tribological behaviors and mechanisms of Ti3AlC2 , 2007 .

[47]  M. Bilek,et al.  Deposition of epitaxial Ti2AlC thin films by pulsed cathodic arc , 2007 .

[48]  M. Aenlle,et al.  Fatigue behaviour of hot rolled reinforcing bars of austenitic and duplex stainless steels , 2007 .

[49]  J. Ferreira,et al.  Layered growth of Ti2AlC and Ti3AlC2 in combustion synthesis , 2007 .

[50]  M. Barsoum,et al.  Corrosion behavior of select MAX phases in NaOH, HCl and H2SO4 , 2006 .

[51]  Yanchun Zhou,et al.  Microstructures and Theoretical Bulk Modulus of Layered Ternary Tantalum Aluminum Carbides , 2006 .

[52]  Zhengming Sun,et al.  Synthesis reactions for Ti3AlC2 through pulse discharge sintering Ti/Al4C3/TiC powder mixture , 2006 .

[53]  D. Lee,et al.  High-temperature oxidation of Ti 3AlC 2 between 1173 and 1473 K in air , 2006 .

[54]  Yanchun Zhou,et al.  Improving the Na2SO4-induced corrosion resistance of Ti3AlC2 by pre-oxidation in air , 2006 .

[55]  Y. Zhou,et al.  Abnormal thermal shock behavior of Ti_3SiC_2 and Ti_3AlC_2 , 2006 .

[56]  Yanchun Zhou,et al.  Microstructures and adhesion of the oxide scale formed on titanium aluminum carbide substrates , 2006 .

[57]  Q. Shen,et al.  Preparation of zirconium pyrophosphate bonded silicon nitride porous ceramics , 2006 .

[58]  Yong Huang,et al.  A novel simple method to stably synthesize Ti3AlC2 powder with high purity , 2006 .

[59]  Ze Zhang,et al.  Formation of Ti3AlC2 by mechanically induced self-propagating reaction in Ti–Al–C system at room temperature , 2006 .

[60]  Yanchun Zhou,et al.  Deformation modes and ideal strengths of ternary layered Ti2AlC and Ti2AlN from first-principles calculations , 2006 .

[61]  Surya R. Kalidindi,et al.  On the elastic properties and mechanical damping of Ti3SiC2, Ti3GeC2, Ti3Si0.5Al0.5C2 and Ti2AlC in the 300–1573 K temperature range , 2006 .

[62]  Jiaoqun Zhu,et al.  High-temperature oxidation behavior of Ti3AlC2 in air , 2006 .

[63]  R. Ahuja,et al.  Deposition and characterization of ternary thin films within the Ti–Al–C system by DC magnetron sputtering , 2006 .

[64]  Y. Zhou,et al.  Interfacial microstructure of Ti3AlC2 and Al2O3 oxide scale , 2006 .

[65]  Zhang Zhili,et al.  Synthesis of Ti3AlC2 Powders Using Sn as an Additive , 2006 .

[66]  Yanchun Zhou,et al.  Strengthening of Ti3AlC2 by incorporation of Si to form Ti3Al1 − xSixC2 solid solutions , 2006 .

[67]  Y. Zhou,et al.  Damage tolerance of nanolayer grained ceramics and quantitative estimation , 2006 .

[68]  Jinbang Wang,et al.  Microstructural characterization of layered ternary Ti2AlC , 2006 .

[69]  Y. Zhou,et al.  Strengthening of Ti2AlC by substituting Ti with V , 2005 .

[70]  Zhang Zhili,et al.  Tribophysical Properties of Polycrystalline Bulk Ti3AlC2 , 2005 .

[71]  Karren L. More,et al.  Coating and near‐surface modification design strategies for protective and functional surfaces , 2005 .

[72]  Hui Zhang,et al.  Thermal shock behavior of Ti3AlC2 from between 200 °C and 1300 °C , 2005 .

[73]  Jiaoqun Zhu,et al.  Synthesis of high-purity Ti3SiC2 and Ti3AlC2 by spark plasma sintering (SPS) technique , 2005 .

[74]  Y. Gogotsi,et al.  Synthesis of Carbide-Derived Carbon by Chlorination of Ti2AlC , 2005 .

[75]  Yanchun Zhou,et al.  Raman active phonon modes and heat capacities of Ti2AlC and Cr2AlC ceramics: first-principles and experimental investigations , 2005 .

[76]  J. Schneider,et al.  Towards Large Area MAX Phase Coatings on Steel , 2005 .

[77]  Z. Zhang,et al.  Ti3AlC2 — A Soft Ceramic Exhibiting Low Friction Coefficient , 2005 .

[78]  M. Barsoum,et al.  Synthesis and Characterization of Ti3AlC2 , 2004 .

[79]  J. Lewis Colloidal Processing of Ceramics , 2004 .

[80]  A. Nagy,et al.  Investigation of indentation-caused cracking in surface-modified silica glasses , 2004 .

[81]  E. Gutmanas,et al.  Pressure‐Assisted Combustion Synthesis of Dense Layered Ti3AlC2 and its Mechanical Properties , 2004 .

[82]  Y. Zhou,et al.  Bending Creep and Stress Relaxation of Ti3AlC2 at High Temperature , 2004 .

[83]  Y. Zhou,et al.  Investigation of the relationship between elastic modulus and hardness based on depth-sensing indentation measurements , 2004 .

[84]  Y. L. Zhu,et al.  Microstructural characterization of bulk Ti3AlC2 ceramics , 2004 .

[85]  R. Ahuja,et al.  Mn+1AXn phases in the Ti-Si-C system studied by thin-film synthesis and ab initio calculations , 2004 .

[86]  Xuan Wang,et al.  Hot Corrosion of Na2 SO 4-Coated Ti3AlC2 in Air at 700-1000°C , 2004 .

[87]  M. Brady,et al.  Alloy Design of Intermetallics for Protective Scale Formation and for Use as Precursors for Complex Ceramic Phase Surfaces , 2004 .

[88]  Yanchun Zhou,et al.  Dependence of elastic stiffness on electronic band structure of nanolaminate M2AlC (M=Ti,V,Nb, and Cr) ceramics , 2004 .

[89]  Yanchun Zhou,et al.  Shear strength and shear failure of layered machinable Ti3AlC2 ceramics , 2004 .

[90]  Y. Zhou,et al.  Ab initio elastic stiffness of nano-laminate (MxM '(2-x))AlC (M and M ' = Ti, V and Cr) solid solution , 2004 .

[91]  R. Ahuja,et al.  Calculated elastic properties of M2AlC M = Ti, V, Cr, Nb and Ta , 2004 .

[92]  Y. Zhou,et al.  Strengthening of Ti3AlC2 by incorporation of Al2O3 , 2004 .

[93]  S. Lofland,et al.  Elastic and electronic properties of select M2AX phases , 2004 .

[94]  Y. Zhou,et al.  Oxidation behavior of TiC-containing Ti3AlC2 based material at 500–900 °C in air , 2003 .

[95]  Y. Zhou,et al.  Stability and selective oxidation of aluminum in nano-laminate Ti3AlC2 upon heating in argon , 2003 .

[96]  Jiaoqun Zhu,et al.  Synthesis of high-purity Ti3SiC2 and Ti3AlC2 by hot-pressing (HP) , 2003 .

[97]  R. Ahuja,et al.  Structure and bulk modulus of M2AlC (M=Ti, V, and Cr) , 2003 .

[98]  Yong Huang,et al.  A possible mechanism on synthesis of Ti3AlC2 , 2003 .

[99]  Y. Zhou,et al.  Improvement of intermediate-temperature oxidation resistance of Ti3AlC2 by pre-oxidation at high temperatures , 2003 .

[100]  S. Lofland,et al.  Low-temperature transport properties of nanolaminatesTi3AlC2andTi4AlN3 , 2003 .

[101]  Yanchun Zhou,et al.  Oxidation behavior of Ti3AlC2 at 1000–1400 °C in air , 2003 .

[102]  Yanfei Zhou,et al.  High-Temperature Oxidation Behavior of Ti2AlC in Air , 2003 .

[103]  J. Ferreira,et al.  Combustion synthesis of ternary carbide Ti3AlC2 in Ti–Al–C system , 2003 .

[104]  Y. Zhou,et al.  Intermediate-temperature oxidation behavior of Ti_2AlC in air , 2002 .

[105]  H. Seifert,et al.  Thermal and electrical properties of Nb2AlC, (Ti, Nb)2AlC and Ti2AlC , 2002 .

[106]  Y. Zhou,et al.  Oxidation behavior of Ti3AlC2 powders in flowing air , 2002 .

[107]  Y. Miyamoto,et al.  Investigation of TiAl/Ti2AlC composites prepared by spark plasma sintering , 2002 .

[108]  Yanchun Zhou,et al.  Solid–liquid reaction synthesis of layered machinable Ti3AlC2 ceramic , 2002 .

[109]  G. Hug,et al.  Full-potential electronic structure of Ti 2 AlC and Ti 2 AlN , 2002 .

[110]  R. Rapp,et al.  Hot corrosion of materials: a fluxing mechanism? , 2002 .

[111]  M. Li,et al.  High temperature oxidation behavior of Ti3SiC2-based material in air , 2001 .

[112]  Jan A. Puszynski,et al.  Synthesis of Ternary Titanium Aluminum Carbides Using Self-Propagating High-Temperature Synthesis Technique , 2001 .

[113]  Chang-an Wang,et al.  Preparation of Ti3AlC2 and Ti2AlC by self-propagating high-temperature synthesis , 2001 .

[114]  Y. Zhou,et al.  Deformation of polycrystalline Ti2AlC under compression , 2001 .

[115]  W. J. Zhang,et al.  Physical properties of TiAl-base alloys , 2001 .

[116]  M. Barsoum,et al.  Oxidation of Ti n + 1AlX n ( n = 1 ­ 3 and X = C , N): II. Experimental Results , 2001 .

[117]  C. Wen,et al.  Fabrication of TiAl by blended elemental powder semisolid forming , 2001 .

[118]  C. J. Lee,et al.  Effect of β-Si3N4 starting powder size on elongated grain growth in β-Si3N4 ceramics , 2000 .

[119]  Yanchun Zhou,et al.  LETTER TO THE EDITOR: Electronic structure and bonding properties in layered ternary carbide Ti3SiC2 , 2000 .

[120]  M. W. Barsoum,et al.  Processing and characterization of Ti2AlC, Ti2AlN, and Ti2AlC0.5N0.5 , 2000 .

[121]  Yanchun Zhou,et al.  Electronic structure and bonding properties of layered machinable Ti 2 AlC and Ti 2 AlN ceramics , 2000 .

[122]  P. Finkel,et al.  Low temperature dependencies of the elastic properties of Ti4AlN3, Ti3Al1.1C1.8, and Ti3SiC2 , 2000 .

[123]  H. Grabke Oxidation of NiAl and FeAl , 1999 .

[124]  J. C. Ho,et al.  Low temperature heat capacities of Ti3Al1.1C1.8, Ti4AlN3, and Ti3SiC2 , 1999 .

[125]  Yanchun Zhou,et al.  Ab initio calculation of titanium silicon carbide , 1999 .

[126]  T. Darling,et al.  Elastic constants and thermal expansion of single crystal γ-TiAl from 300 to 750 K , 1997 .

[127]  A. Boccaccini Machinability and brittleness of glass-ceramics , 1997 .

[128]  M. Barsoum,et al.  Layered machinable ceramics for high temperature applications , 1997 .

[129]  M. Barsoum,et al.  Synthesis and Characterization of a Remarkable Ceramic: Ti3SiC2 , 1996 .

[130]  J. L. Henshall,et al.  Indentation hardness and fracture toughness in single crystal TiC0.96 , 1996 .

[131]  P. Ettmayer,et al.  Solid state properties of group IVb carbonitrides , 1995 .

[132]  P. Ettmayer,et al.  Lattice parameters and thermal expansion of Ti(CxN1−x), Zr(CxN1−x), Hf(CxN1−x) and TiN1−x from 298 to 1473 K as investigated by high-temperature X-ray diffraction , 1994 .

[133]  J. Schuster,et al.  Summary of constitutional data on the Aluminum-Carbon-Titanium system , 1994 .

[134]  F. Langlais,et al.  Solid-state synthesis and characterization of the ternary phase Ti3SiC2 , 1994, Journal of Materials Science.

[135]  C. Chiu Influence of surface oxidation on thermal shock resistance and flexural strength of SiC/Al2O3 composites , 1994 .

[136]  R. Rapp,et al.  Electrochemical impedance of a platinum electrode in fused Na[sub 2]SO[sub 4] melts in SO[sub 2]-O[sub 2] environments , 1993 .

[137]  S. Shimada,et al.  Oxidation of TiC at low temperatures , 1992 .

[138]  H. Tsuda,et al.  Fabrication of Ti2AlC/TiAl Composites Using Cobustion Reaction Process. , 1991 .

[139]  A. Rahmel,et al.  Thermodynamic aspects of TiAl and TiSi2 oxidation: The Al-Ti-O and Si-Ti-O Phase diagrams , 1991 .

[140]  F. Lange,et al.  Powder Processing Science and Technology for Increased Reliability , 1989 .

[141]  T. Grobstein,et al.  The oxidation of high-temperature intermetallics , 1989 .

[142]  G. Rybicki,et al.  Effect of theθ-α-Al2O3 transformation on the oxidation behavior ofβ-NiAl + Zr , 1989 .

[143]  T. Hirai,et al.  Chemically vapor deposited Ti3SiC2 , 1987 .

[144]  K. Luthra Kinetics of the Low Temperature Hot Corrosion of Co‐Cr‐Al Alloys , 1985 .

[145]  R. Rapp,et al.  Electrochemical Reactions in a Pure Na2 SO 4 Melt , 1983 .

[146]  D. A. Shores,et al.  Transport of Oxidant in Molten Na2 SO 4 in O 2 ‐ SO 2 ‐ SO 3 Environments , 1981 .

[147]  D. A. Shores,et al.  Mechanism of Na2 SO 4 Induced Corrosion at 600°–900°C , 1980 .

[148]  V. I. Ivchenko,et al.  Some physical properties of ternary compounds in the system Ti-Al-C , 1976 .

[149]  J. Nickl,et al.  Gasphasenabscheidung im system TiSiC , 1972 .

[150]  N. S. Bornstein,et al.  The role of sodium in the accelerated oxidation phenomenon termed sulfidation , 1971 .

[151]  D. Hasselman Strength Behavior of Polycrystalline Alumina Subjected to Thermal Shock , 1970 .

[152]  J. Goebel,et al.  Na2SO4-induced accelerated oxidation (hot corrosion) of nickel , 1970 .

[153]  O. Anderson,et al.  A simplified method for calculating the debye temperature from elastic constants , 1963 .

[154]  H. Nowotny,et al.  Kohlenstoffhaltige ternäre Verbindungen (H-Phase) , 1963 .

[155]  L. Hultman,et al.  Sputter deposition from a Ti2AlC target: Process characterization and conditions for growth of Ti2AlC , 2010 .

[156]  C. Yang,et al.  Low-temperature synthesis of high-purity Ti3AlC2 by MA-SPS technique , 2009 .

[157]  J. Lis,et al.  Ceramic nanolaminates—Processing and application , 2008 .

[158]  Dongyun Lee,et al.  Synthesis and mechanical properties of Ti3AlC2 by hot pressing TiCx/Al powder mixture , 2008 .

[159]  Yanchun Zhou,et al.  Effect of grain size, notch width, and testing temperature on the fracture toughness of Ti3Si(Al)C2 and Ti3AlC2 using the chevron-notched beam (CNB) method , 2008 .

[160]  J.Th.M. De Hosson,et al.  Oxidation-induced crack healing in Ti3AlC2 ceramics , 2008 .

[161]  Y. Zhou,et al.  Influence of water vapor on the oxidation behavior of Ti3AlC2 and Ti2AlC , 2008 .

[162]  K. Hirao,et al.  Effects of processing method and additive composition on microstructure and thermal conductivity of Si3N4 ceramics , 2006 .

[163]  Yanchun Zhou,et al.  Hot corrosion and protection of Ti2AlC against Na2SO4 salt in air , 2006 .

[164]  Jiaoqun Zhu,et al.  Rapid synthesis of Ti 2AlC by spark plasma sintering technique , 2005 .

[165]  Jae,et al.  Fabrication and Mechanical Properties of Sm2O3 Doped CeO2 Reinforced Ti3AlC2 Nano Composite , 2004 .

[166]  M. Sundberg,et al.  Alumina forming high temperature silicides and carbides , 2004 .

[167]  Yanchun Zhou,et al.  Solid–liquid reaction synthesis and simultaneous densification of polycrystalline Ti2AlC , 2002 .

[168]  Y. Zhou,et al.  Electronic and structural properties of the layered ternary carbide Ti3AlC2 , 2001 .

[169]  Michel W. Barsoum,et al.  The MN+1AXN phases: A new class of solids , 2000 .

[170]  A. Boccaccini,et al.  Glass matrix composites from coal flyash and waste glass , 1997 .

[171]  A. Tomsia,et al.  Joining of ceramics , 1988 .

[172]  Von Hans Nowotny Strukturchemie einiger Verbindungen der Übergangsmetalle mit den elementen C, Si, Ge, Sn , 1971 .

[173]  W. Kingery,et al.  Factors Affecting Thermal Stress Resistance of Ceramic Materials , 1955 .