Electro-impulse de-icing - A status report

The advantages and disadvantages of the Electro-Impulse De-Icing (EIDI) system are examined. The design and operation of the EIDI are described. The effect of repeated impulsive loads on the structure and skin of the aircraft surface is investigated. It is observed that the wing skin directly over the coil receives the greatest stresses. Data from the testing of metal leading edges reveal that after 11,500 impulses cracks appear in the sheet brackets attaching the ribs to the coil beams. The composite leading edge was evaluated for fatigue, and after 20,000 impulses no cracks were detected. The advantages of the band-aid coil mount are discussed.