Measuring critical stress for shear failure of interfacial regions in coating/interlayer/substrate systems through a micro-pillar testing protocol

Mechanical integrity of the interfacial region between ceramic coatings and substrates is critical to high performance coated mechanical components and manufacturing tools. Mechanical failure of the coating/substrate interfacial region often leads to catastrophic failure of the coated system as a whole. Despite extensive research over the past two decades, quantitative assessment of the mechanical response of coating/substrate interfacial regions remains a challenge. The lack of reliable protocols for measuring the mechanical response of coating/substrate interfacial regions quantitatively hampers the understanding of key factors controlling the mechanical integrity of coating/substrate interfaces. In this paper, we describe a new micro-pillar testing protocol for quantitative measurement of critical stresses for inducing shear failure of interfacial regions in ceramic-coating/metal-adhesion-layer/substrate systems. We observe significant differences in the critical stress for shear failure of interfacial regions in CrN/Cu/Si, CrN/Cr/Si, and CrN/Ti/Si systems. The present testing protocol has general applicability to a wide range of coating/interlayer/substrate systems.

[1]  T. Cselle,et al.  Today's applications and future developments of coatings for drills and rotating cutting tools , 1995 .

[2]  A. G. Evans,et al.  Structure and mechanics of W-DLC coated spur gears , 2003 .

[3]  C. V. Cooper,et al.  Material removal on lubricated steel gears with W-DLC-coated surfaces , 2003 .

[4]  H. Ichimura,et al.  Mechanical properties of arc-evaporated CrN coatings: Part I — nanoindentation hardness and elastic modulus , 2001 .

[5]  S. K. Choudhury,et al.  Machining of hardened steel—Experimental investigations, performance modeling and cooling techniques: A review , 2015 .

[6]  W. Meng,et al.  Thickness dependence of flow stress of Cu thin films in confined shear plastic flow , 2014 .

[7]  J. Vlassak,et al.  A simple technique for measuring the adhesion of brittle films to ductile substrates with application to diamond-coated titanium , 1997 .

[8]  R. Smoluchowski,et al.  Elements of X‐Ray Diffraction , 1957 .

[9]  S. Brown,et al.  Adherence* failure and measurement: some troubling questions , 1994 .

[10]  J. Hutchinson,et al.  Measurement of the adhesion of a brittle film on a ductile substrate by indentation , 1996, Proceedings of the Royal Society of London. Series A: Mathematical, Physical and Engineering Sciences.

[11]  K. Holmberg Coatings Tribology: Properties, Techniques and Applications in Surface Engineering , 1994 .

[12]  W. Meng,et al.  Manufacturing of metal-based microparts: Fabrication strategies and surface engineering applications , 2013 .

[13]  R. D. Evans,et al.  Deposition, characterization, and performance of tribological coatings on spherical rolling elements , 2015 .

[14]  Kilian Wasmer,et al.  Strength and fracture of Si micropillars: A new scanning electron microscopy-based micro-compression test , 2007 .

[15]  M. Jackson,et al.  A review of machining theory and tool wear with a view to developing micro and nano machining processes , 2007 .

[16]  Theo Z. Kattamis,et al.  On the evaluation of adhesion of coatings by automatic scratch testing , 1993 .

[17]  W. Meng,et al.  Temperature dependence of inductively coupled plasma assisted growth of TiN thin films , 1999 .

[18]  K. Mittal,et al.  Adhesion measurement of films and coatings , 2014 .

[19]  John W. Hutchinson,et al.  Micro-pillar measurements of plasticity in confined Cu thin films , 2014 .

[20]  D. C. Agrawal,et al.  Measurement of the ultimate shear strength of a metal-ceramic interface , 1989 .

[21]  John W. Hutchinson,et al.  Analysis of a wedge impression test for measuring the interface toughness between films/coatings and ductile substrates , 2000 .

[22]  Michael N Kotzalas,et al.  Tribological advancements for reliable wind turbine performance , 2010, Philosophical Transactions of the Royal Society A: Mathematical, Physical and Engineering Sciences.

[23]  W. Brantley Calculated elastic constants for stress problems associated with semiconductor devices , 1973 .

[24]  Ke Chen,et al.  A new experimental approach for evaluating the mechanical integrity of interfaces between hard coatings and substrates , 2014 .

[25]  Jia-Hong Huang,et al.  In situ observation of the cracking behavior of TiN coating on 304 stainless steel subjected to tensile strain , 1999 .

[26]  Xiaoman Zhang,et al.  Dependence of confined plastic flow of polycrystalline Cu thin films on microstructure , 2016 .

[27]  Marco Sebastiani,et al.  Depth-resolved residual stress analysis of thin coatings by a new FIB–DIC method , 2011 .