Initial bond formation in thermosonic gold ball bonding on aluminium metallization pads

The morphological features of lift-off footprints on the aluminium metallization pads were investigated to gain an understanding of the effects of bonding parameters on formation of initial bonds during thermosonic gold ball bonding. The obtained results showed that metallurgical bonding initiated at the peripheral areas of the contact area situated along the direction of ultrasonic vibration. Those areas extended inwards with an increase in ultrasonic power. Both the external bonded area and central non-bonded area increased with increasing bonding force. Based on the evolution of footprints, the bonding models were proposed, and the effects of the bonding parameters on the formation of initial bonds were discussed.

[1]  Michael Mayer,et al.  Footprint study of ultrasonic wedge-bonding with aluminum wire on copper substrate , 2006 .

[2]  G. Harman Wire Bonding in Microelectronics: Materials, Processes, Reliability, and Yield , 1997 .

[3]  Zhaowei Zhong,et al.  Wire-bonding process development for low-k materials , 2005 .

[4]  M. Heinstein,et al.  New Approximations for Elastic Spheres Under an Oscillating Torsional Couple , 2005 .

[5]  B. Langenecker Effects of Ultrasound on Deformation Characteristics of Metals , 1966, IEEE Transactions on Sonics and Ultrasonics.

[6]  A.D. Wilson,et al.  Holographic Interferometry Applied to Motion Studies of Ultrasonic Bonders , 1972, IEEE Transactions on Sonics and Ultrasonics.

[7]  S. Khoury,et al.  A comparison of copper and gold wire bonding on integrated circuit devices , 1990 .

[8]  G. Harman,et al.  The Ultrasonic Welding Mechanism as Applied to Aluminum-and Gold-Wire Bonding in Microelectronics , 1977 .

[9]  V. Winchell,et al.  Enhancing Ultrasonic Bond Development , 1978 .

[10]  Michael Mayer,et al.  In situ ultrasonic force signals during low-temperature thermosonic copper wire bonding , 2008 .

[11]  Jeng-Rong Ho,et al.  Thin film thermal sensor for real time measurement of contact temperature during ultrasonic wire bonding process , 2004 .

[12]  Deming Liu,et al.  Effects of process parameters on bondability in ultrasonic ball bonding , 2006 .

[13]  Weihua Li,et al.  A microslip model of the bonding process in ultrasonic wire bonders Part I: Transient response , 2006 .

[14]  S. Timoshenko,et al.  Theory of elasticity , 1975 .

[15]  Chunqing Wang,et al.  Investigation of ultrasonic copper wire wedge bonding on Au/Ni plated Cu substrates at ambient temperature , 2008 .

[16]  Mingyu Li,et al.  Evolution of the bond interface during ultrasonic Al–Si wire wedge bonding process , 2007 .

[17]  Jae Pil Jung,et al.  Bonding mechanism in ultrasonic gold ball bonds on copper substrate , 2005 .

[18]  Raymond D. Mindlin,et al.  Compliance of elastic bodies in contact , 1949 .

[19]  Vadim V. Silberschmidt,et al.  A re-examination of the mechanism of thermosonic copper ball bonding on aluminium metallization pads , 2009 .