Microstructural Characterization of Solid State Reaction Phase Formed During Sintering of Hexagonal Boron Nitride with Iron

Abstract In the development of dry self-lubricating composites, not only solid lubricant particle size and distribution are important, but also the correct selection of the solid lubricant characteristics, which should be stable, i.e. not reactive, during the whole processing. In this work, Fe+9 vol% h-BN composites were produced by uniaxial cold compaction and sintering, for which a reaction between h-BN and iron was detected after sintering at 1,150°C. The reaction phase was characterized by optical and scanning electron microscopy and identified by X-ray diffraction and energy-dispersive X-ray spectroscopy. The newly formed phase had high hardness when compared with the iron matrix. The resulting composites presented a high friction coefficient and high wear.

[1]  K. Miyoshi Solid Lubrication Fundamentals and Applications , 2019 .

[2]  K. Furlan,et al.  Influence of alloying elements on the sintering thermodynamics, microstructure and properties of Fe–MoS2 composites , 2015 .

[3]  K. Furlan,et al.  Sintering Studies and Microstructural Evolution of Fe-MoS2 Mixtures , 2014 .

[4]  S. Raadnui,et al.  Dry sliding wear behavior of SS316L composites containing h-BN and MoS2 solid lubricants , 2014 .

[5]  N. Sombatsompop,et al.  Effects of hexagonal boron nitride and sintering temperature on mechanical and tribological properties of SS316L/h-BN composites , 2013 .

[6]  K. Furlan,et al.  Thermal Stability of the MoS2 Phase in Injection Moulded 17-4 PH Stainless Steel , 2012 .

[7]  H. Danninger,et al.  Sintering of Fe–C–BN steel compacts in different atmospheres studied by dilatometry and DTA/TG , 2012 .

[8]  R. Gnanamoorthy,et al.  Microstructure, strength and tribological behavior of Fe–C–Cu–Ni sintered steels prepared with MoS2 addition , 2007 .

[9]  Ali Erdemir,et al.  Review of engineered tribological interfaces for improved boundary lubrication , 2005 .

[10]  B. Yao,et al.  Mechanism of formation of Fe–N alloy in the solid-state reaction process between iron and boron nitride , 2004 .

[11]  Ali Erdemir,et al.  Historical developments and new trends in tribological and solid lubricant coatings. , 2004 .

[12]  S. Dolinsek,et al.  The characteristics of vacuum sintered M3/2 type HSSs with MoS2 addition , 2003 .

[13]  P. Kotula,et al.  Automated Analysis of SEM X-Ray Spectral Images: A Powerful New Microanalysis Tool , 2003, Microscopy and Microanalysis.

[14]  S. Lim,et al.  Friction and wear characteristics of Al–Cu/C composites synthesized using partial liquid phase casting process , 1997 .

[15]  N. Chen,et al.  A study of the optimization mechanism of solid lubricant concentration in self-lubricating composite , 1997 .

[16]  G. Rowe Some observations on the frictional behaviour of boron nitride and of graphite , 1960 .

[17]  R. Gnanamoorthy,et al.  Dry sliding friction and wear characteristics of Fe–C–Cu alloy containing molybdenum di sulphide , 2007 .

[18]  Bonfiglioli Riduttori S.p.A. Lubricants and Lubrication , 1995 .

[19]  M. Gardos,et al.  Friction of hexagonal boron nitride in various environments , 1992 .

[20]  William D. Callister,et al.  Materials Science and Engineering: An Introduction , 1985 .