Electrochemical properties of lithium sulfur cells using PEO polymer electrolytes prepared under three different mixing conditions

Abstract Lithium sulfur cells were prepared by composing with sulfur cathode (PEO) 6 LiBF 4 polymer electrolyte and lithium anode. (PEO) 6 LiBF 4 polymer electrolyte was prepared under three different mixing conditions: stirred polymer electrolyte (SPE), ball-milled polymer electrolyte (BPE) and ball-milled polymer electrolyte with 10 wt%Al 2 O 3 (BCPE). The effects of ball milling and additive were investigated by discharge test according to depth of discharge. The initial discharge capacity of lithium sulfur cell using BCPE was 1670 mAh g −1 -sulfur, which was better than those of SPE and BPE, and approximately equal to the theoretical capacity. The cycle performance of Li/(PEO) 6 LiBF 4 /S cell was remarkably improved by the addition of Al 2 O 3.