[1]  Gang Liu,et al.  Mechanism of saturated flow stress during hot tensile deformation of a TA15 Ti alloy , 2015 .

[2]  M. Fu,et al.  Work-hardening effect and strain-rate sensitivity behavior during hot deformation of Ti–5Al–5Mo–5V–1Cr–1Fe alloy , 2015 .

[3]  Shi-ao Pu,et al.  Evaluation of the hot workability corresponding to complex deformation mechanism evolution for Ti–10V–2Fe–3Al alloy in a wide condition range , 2015 .

[4]  Y. Ning,et al.  Dynamic softening behavior of TC18 titanium alloy during hot deformation , 2015 .

[5]  W. Huang,et al.  Strain rate sensitivity and evolution of dislocations and twins in a twinning-induced plasticity steel , 2015 .

[6]  Y. H. Zhou,et al.  Research on hot deformation behavior of Ti–5Al–5Mo–5V–1Cr–1Fe alloy , 2015 .

[7]  T. Langdon,et al.  Enhancement of strain-rate sensitivity and shear yield strength of a magnesium alloy processed by high-pressure torsion , 2015 .

[8]  Mara Cristina Lopes de Oliveira,et al.  Materials selection for hot stamped automotive body parts: An application of the Ashby approach based on the strain hardening exponent and stacking fault energy of materials , 2014 .

[9]  Bingfeng Wang,et al.  High temperature deformation and creep behavior of Ti–5Al–5Mo–5V–1Fe–1Cr alloy , 2014 .

[10]  E. Pereloma,et al.  The effect of ageing on microstructure and mechanical properties of powder Ti–5Al–5Mo–5V–1Cr–1Fe alloy , 2014 .

[11]  J. Ndjaka,et al.  Mechanical tensile properties by spherical macroindentation using an indentation strain-hardening exponent , 2013 .

[12]  Changmeng Liu,et al.  Microstructural characterization of laser melting deposited Ti–5Al-5Mo–5V–1Cr–1Fe near β titanium alloy , 2013 .

[13]  K. Zhou,et al.  Hot Deformation of Ti-5Al-5Mo-5 V-1Cr-1Fe Near β Titanium Alloys Containing Thin and Thick Lamellar α Phase , 2013 .

[14]  S. Semiatin,et al.  Microstructure evolution during warm working of Ti–5Al–5Mo–5V–1Cr–1Fe at 600 and 800 °C , 2013 .

[15]  K. Zhou,et al.  Relationship between lamellar α evolution and flow behavior during isothermal deformation of Ti–5Al–5Mo–5V–1Cr–1Fe near β titanium alloy , 2012 .

[16]  D. Wang,et al.  Determination of the maximum strain–hardening exponent , 2012 .

[17]  N. Pardis,et al.  Determination of strain-hardening exponent using double compression test , 2009 .

[18]  Miaoquan Li,et al.  High temperature deformation behavior of near alpha Ti-5.6Al-4.8Sn-2.0Zr alloy , 2007 .

[19]  Thomas R. Bieler,et al.  The effect of alpha platelet thickness on plastic flow during hot working of TI–6Al–4V with a transformed microstructure , 2001 .