Development of coatings based on Fe-Cr-Ni-Al for resisting fretting wear in the temperature range 20–700 °C
暂无分享,去创建一个
[1] R. B. Waterhouse,et al. A new high-temperature fretting wear test rig , 1981 .
[2] B. L. Daniell,et al. The influence of microstructure on the adhesive wear resistance of a CoCrMo alloy , 1980 .
[3] P. L. Hurricks. The fretting wear of mild steel from 200° to 500°C , 1974 .
[4] R. Bill. Fretting of Secondary-Seal-Ring Candidate Materials in Air at Temperatures to 816 C , 1972 .