The effect of pre-deformation on environmental embrittlement of Ni3(Si,Ti) alloys
暂无分享,去创建一个
[1] T. Radhakrishnan,et al. A Reexamination of the Trapping of Hydrogen in Iron and Steel , 1993 .
[2] T. Takasugi,et al. Strength anomaly and dislocation structure at 4.2 k in ni3(si, ti) single crystals , 1992 .
[3] T. Takasugi,et al. Effects of Boron and Carbon Additions on Environmental Embrittlement of a Ni3(Si, Ti) Alloy at Ambient Temperature , 1995 .
[4] T. Misawa,et al. Critical pressures of water vapor and hydrogen gas causing intergranular brittle fracture of Co3Ti at room temperature , 1994 .
[5] T. Takasugi,et al. The effect of temperature on dislocation structures in l12-type ni3(si, ti) single crystals , 1992 .
[6] R. Cahn,et al. Ordered intermetallics--physical metallurgy and mechanical behaviour , 1992 .
[7] T. Takasugi,et al. Grain boundary structure and controlling embrittlement in ordered alloys , 1988 .
[8] H. Hagi,et al. Effect of dislocation trapping on hydrogen and deuterium diffusion in iron , 1987 .
[9] H. Hagi,et al. Effects of Interstitial Impurities on Dislocation Trapping of Hydrogen in Iron , 1987 .
[10] C. T. Liu,et al. High-temperature ordered intermetallic alloys , 1985 .
[11] R. A. Oriani,et al. The diffusion and trapping of hydrogen in steel , 1970 .