Long-term ceramic matrix composite for aeroengine

[1]  Zhihua Yang,et al.  A comparative study on high temperature oxidation behavior of SiC, SiC-BN and SiBCN monoliths , 2021, Corrosion Science.

[2]  Aijun Li,et al.  Oxidation behavior of 3D SiCf/SiBCN composites at 800–1200 °C , 2021 .

[3]  Qin Shan,et al.  More effective crack self‐healing capability of SiC f /SiC‐B 4 C with Al 2 O 3 modified under wet environment , 2020 .

[4]  Lai-fei Cheng,et al.  Wet oxidation behavior of C/SiC–SiHf(B)CN composites at high temperature , 2020, Advanced Composites and Hybrid Materials.

[5]  Lai-fei Cheng,et al.  Self-healing enhancing tensile creep of 2D-satin weave SiC/(SiC-SiBCN)x composites in wet oxygen environment , 2020 .

[6]  Zhihua Yang,et al.  Incorporation of BN-coated carbon fibers into ZrB2/SiBCN ceramic composites and their ablation behavior , 2020 .

[7]  Lai-fei Cheng,et al.  Wet oxidation behavior of SiC/(SiC‐ SiBCN)x composites prepared by CVI combined with PIOP process , 2019, Journal of the American Ceramic Society.

[8]  Qin Shan,et al.  The Surface Cracking Resistance of Al2O3‐Modified SiCf/SiC‐B4C Composites after Cyclic Oxidation in Wet Environment , 2019, Advanced Engineering Materials.

[9]  Lai-fei Cheng,et al.  Oxidation behavior of C/SiC-SiBCN composites at high temperature , 2019, Journal of the European Ceramic Society.

[10]  Lai-fei Cheng,et al.  Improved tensile strength and toughness of dense C/SiC-SiBC with tailored PyC interphase , 2019, Journal of the European Ceramic Society.

[11]  Hejun Li,et al.  Gradient HfB2-SiC multilayer oxidation resistant coating for C/C composites , 2018, Ceramics International.

[12]  Qin Shan,et al.  Influence of boron nitride nanotubes on the damage evolution of SiCf/SiC composites , 2018, Journal of the European Ceramic Society.

[13]  Hong Wang,et al.  Mechanical properties and microstructure evolution of 3D Cf/SiBCN composites at elevated temperatures , 2018 .

[14]  Lai-fei Cheng,et al.  Degradation mechanisms of a self-healing SiC(f)/BN(i)/[SiC-B4C](m) composite at high temperature under different oxidizing atmospheres , 2018, Journal of the European Ceramic Society.

[15]  Wei Liu,et al.  Oxidation behavior of a 2D‐SiCf/BN/SiBCN composite at 1350–1650 °C in air , 2018 .

[16]  Xiaowei Yin,et al.  Oxidation Behavior of Tyranno ZMI-SiC Fiber/SiC-SiBC Matrix Composite from 800 to 1200 °C , 2018, Materials.

[17]  Longbiao Li Modeling matrix multicracking development of fiber-reinforced ceramic-matrix composites considering fiber debonding , 2018, International Journal of Applied Ceramic Technology.

[18]  Han Zhang,et al.  High temperature self-healing SiBCN ceramics derived from hyperbranched polyborosilazanes , 2018, Advanced Composites and Hybrid Materials.

[19]  Zhihua Yang,et al.  Microstructure and thermal shock behavior of sol–gel introduced ZrB2 reinforced SiBCN matrix , 2018, Journal of Sol-Gel Science and Technology.

[20]  Yiguang Wang,et al.  Formation and growth of silica layer beneath environmental barrier coatings under water-vapor environment , 2018 .

[21]  Haibin Zhang,et al.  KD-S SiCf/SiC composites with BN interface fabricated by polymer infiltration and pyrolysis process , 2018, Journal of Advanced Ceramics.

[22]  Zhihua Yang,et al.  Oxidation behavior of SiBCN-Zr composites at 1500 °C prepared by reactive spark plasma sintering , 2018 .

[23]  Qin Shan,et al.  Oxidation behavior in wet oxygen environment of Al2O3 added reaction-sintered Si-B-C ceramics , 2018 .

[24]  Lai-fei Cheng,et al.  Oxidation resistance of SiC/SiC composites containing SiBC matrix fabricated by liquid silicon infiltration , 2018 .

[25]  Y. Liu,et al.  A novel high yield polyborosilazane precursor for SiBNC ceramic fibers , 2017 .

[26]  Zhihua Yang,et al.  Effects of boron addition on the high temperature oxidation resistance of dense sSiBCN monoliths at 1500 °C , 2017 .

[27]  Zhihua Yang,et al.  High-temperature oxidation behavior of dense SiBCN monoliths: Carbon-content dependent oxidation structure, kinetics and mechanisms , 2017 .

[28]  Liping Wang,et al.  Mechanical Property, Oxidation and Ablation Resistance of C/C-ZrB2-ZrC-SiC Composite Fabricated by Polymer Infiltration and Pyrolysis with Preform of Cf/ZrB2 , 2017 .

[29]  Lai-fei Cheng,et al.  Fibre-reinforced multifunctional SiC matrix composite materials , 2017 .

[30]  Hejun Li,et al.  A ZrC-SiC/ZrC-LaB6/ZrC multilayer ablation resistance coating for SiC-coated carbon/carbon composites , 2017 .

[31]  Li Longbiao Synergistic Effects of Temperature and Oxidation on Matrix Cracking in Fiber-Reinforced Ceramic-Matrix Composites , 2017, Applied Composite Materials.

[32]  Yongqiang Sun,et al.  Synthesis and characteristic of SiBCN/HfN ceramics with high temperature oxidation resistance , 2016 .

[33]  Lai-fei Cheng,et al.  Fatigue behavior of 2D C/SiC composites modified with Si-B-C ceramic in static air , 2016 .

[34]  Lai-fei Cheng,et al.  Oxidation behaviors and mechanisms of CVD Si-B-C ceramic in wet oxygen from 700 °C to 1400 °C , 2016 .

[35]  H. Jianfeng,et al.  Self-healing ZrB2–SiO2 oxidation resistance coating for SiC coated carbon/carbon composites , 2016 .

[36]  Zhihua Yang,et al.  A novel in situ synthesis of SiBCN-Zr composites prepared by a sol-gel process and spark plasma sintering. , 2016, Dalton transactions.

[37]  Zhihua Yang,et al.  Amorphous silicoboron carbonitride monoliths resistant to flowing air up to 1800 °C , 2016 .

[38]  Lai-fei Cheng,et al.  Effect of heat treatment on the mechanical properties of SiCf/BN/SiC fabricated by CVI , 2016 .

[39]  Zhihua Yang,et al.  Preparation, microstructures, mechanical properties and oxidation resistance of SiBCN/ZrB2–ZrN ceramics by reactive hot pressing , 2015 .

[40]  Lai-fei Cheng,et al.  Oxidation behavior of 2D C/SiC composites coated with multi-layer SiC/Si–B–C/SiC coatings under wet oxygen atmosphere , 2015 .

[41]  M. Grujicic,et al.  Computational investigation of foreign object damage sustained by environmental barrier coatings (EBCs) and SiC/SiC ceramic-matrix composites (CMCs) , 2015 .

[42]  Lai-fei Cheng,et al.  The improvement in the mechanical and thermal properties of SiC/SiC composites by introducing CNTs into the PyC interface , 2015 .

[43]  Hejun Li,et al.  Ablation behavior and mechanism of C/C-HfC-SiC composites , 2015 .

[44]  Zhu Kong-jun,et al.  Microstructure and oxidation protection of borosilicate glass coating prepared by pulse arc discharge deposition for C/C composites , 2015 .

[45]  Ze Feng,et al.  Preparation and anti-oxidation characteristics of ZrSiO4–SiBCN(O) amorphous coating , 2015 .

[46]  Yongcheng Liu,et al.  Microstructural evolution and self‐healing mechanism of a 2D C/SiC‐BCx composite under constant load in static wet oxygen and dynamic combustion atmosphere , 2015 .

[47]  Lai-fei Cheng,et al.  Oxidation behavior of SiBC matrix modified C/SiC composites with different PyC interphase thicknesses , 2015 .

[48]  Yue Zhang,et al.  Oxidation behavior of SiC–SiBCN ceramics , 2015 .

[49]  Xiaohong Shi,et al.  Ablation resistance of SiC–ZrC coating prepared by a simple two-step method on carbon fiber reinforced composites , 2014 .

[50]  J. DiCarlo Advances in SiC/SiC Composites for Aero‐Propulsion , 2014 .

[51]  Lai-fei Cheng,et al.  Effect of PyC interphase thickness on mechanical behaviors of SiBC matrix modified C/SiC composites fabricated by reactive melt infiltration , 2014 .

[52]  Song Wang,et al.  Preparation of 3D Cf/ZrC–SiC composites by joint processes of PIP and RMI , 2014 .

[53]  Ankur H. Parikh,et al.  Ceramic Matrix Composites for High Pressure Turbine Vanes , 2014 .

[54]  Lai-fei Cheng,et al.  High-temperature flexural properties of SiBC modified C/SiC composites , 2014 .

[55]  Hejun Li,et al.  Effect of SiC/ZrC ratio on the mechanical and ablation properties of C/C–SiC–ZrC composites , 2014 .

[56]  P. David,et al.  High temperature oxidation of two- and three-dimensional hafnium carbide and silicon carbide coatings , 2014 .

[57]  I. Low Advances in ceramic matrix composites , 2014 .

[58]  M. Pope,et al.  Creep Behavior in Interlaminar Shear of a SiC/SiC Ceramic Composite with a Self-healing Matrix , 2014, Applied Composite Materials.

[59]  C. Heveran,et al.  Simulation of stresses in TBC–EBC coating systems for ceramic components in gas turbines , 2013 .

[60]  G. Morscher,et al.  Matrix Cracking in 3D Orthogonal Melt-Infiltrated Sic/Sic Composites with Various Z-Fiber Types , 2013 .

[61]  Yue Zhang,et al.  Structure and oxidation behavior of high temperature ZrB2–SiBCN ceramics with polyborosilazane as a sintering additive , 2013 .

[62]  Hejun Li,et al.  Ablation behavior and mechanism of C/C–ZrC–SiC composites under an oxyacetylene torch at 3000 °C , 2013 .

[63]  J. DiCarlo Advances in SiC/SiC Composites for , 2013 .

[64]  Zhihua Yang,et al.  Progress of a novel non-oxide Si-B-C-N ceramic and its matrix composites , 2012, Journal of Advanced Ceramics.

[65]  Lai-fei Cheng,et al.  Oxidation behaviour of two-dimensional C/SiC modified with self-healing Si–B–C coating in static air , 2012 .

[66]  Lai-fei Cheng,et al.  Fabrication of Si3N4–SiBC composite ceramic and its excellent electromagnetic properties , 2012 .

[67]  E. Burresi,et al.  Optimization of a Pyrolysis Procedure for Obtaining SiC-SiCf CMC by PIP for Thermostructural Applications , 2012 .

[68]  V. Lavrenko,et al.  High-temperature oxidation of ZrB2–SiC and ZrB2–SiC–ZrSi2 ceramics up to 1700°C in air , 2012, Powder Metallurgy and Metal Ceramics.

[69]  Hejun Li,et al.  SiC/HfC/SiC ablation resistant coating for carbon/carbon composites , 2012 .

[70]  J. Lamon,et al.  Fatigue Behavior at High Temperatures in Air of a 2D SiC/Si‐B‐C Composite with a Self‐Healing Multilayered Matrix , 2012 .

[71]  Hejun Li,et al.  A SiC–Si–ZrB2 multiphase oxidation protective ceramic coating for SiC-coated carbon/carbon composites , 2012 .

[72]  A. Kohyama,et al.  Fabrication of Environmentally Resistant NITE-SiC/SiC Composites , 2011, MSE 2011.

[73]  Yang Jinlin,et al.  Study of thermal stability of fumed silica based thermal insulating composites at high temperatures , 2011 .

[74]  T. Parthasarathy,et al.  Oxidation Resistance of Hafnium Diboride Ceramics with Additions of Silicon Carbide and Tungsten Boride or Tungsten Carbide , 2011 .

[75]  W. Curtin,et al.  Prediction of first matrix cracking in micro/nanohybrid brittle matrix composites , 2010 .

[76]  Lai-fei Cheng,et al.  Preparation and properties of 2D C/ZrB2-SiC ultra high temperature ceramic composites , 2009 .

[77]  J. Lamon,et al.  Single‐ and Multilayered Interphases in SiC/SiC Composites Exposed to Severe Environmental Conditions: An Overview , 2009 .

[78]  Gregory N. Morscher,et al.  Effects of Fiber Architecture on Matrix Cracking for Melt‐Infiltrated SiC/SiC Composites , 2009 .

[79]  A. Kohyama,et al.  Development of the tailored SiC/SiC composites by the combined fabrication process of ICVI and NITE methods , 2009 .

[80]  Laifei Cheng,et al.  Mechanical Self-adaptability of a SiC/PyC/SiC Composite During Oxidation in Air , 2009 .

[81]  Lai-fei Cheng,et al.  Mechanical Self-adaptability of a SiC/PyC/SiC Composite During Oxidation in Air , 2009 .

[82]  Q. Zeng,et al.  Preparation and oxidation resistance of 2D C/SiC composites modified by partial boron carbide self-sealing matrix , 2008 .

[83]  Ji Yeon Park,et al.  Microstructure and Properties of SiC Nanowire-Reinforced SiCf/SiC Composites , 2008 .

[84]  Jiecai Han,et al.  High-Temperature Oxidation at 1900°C of ZrB2-xSiC Ultrahigh-Temperature Ceramic Composites , 2008 .

[85]  J. DiCarlo,et al.  Processing and Structural Advantages of the Sylramic‐iBN SiC Fiber for SiC/SiC Components , 2008 .

[86]  T. Mccue,et al.  Thermal Stability of Melt Infiltrated SiC/SiC Composites , 2008 .

[87]  T. Mccue,et al.  Modeling the Thermostructural Stability of Melt-infiltrated Sic/sic Composites , 2008 .

[88]  Sung R. Choi,et al.  Impact resistance of uncoated SiC/SiC composites , 2008 .

[89]  Lai-fei Cheng,et al.  Preparation and Properties of Self‐Healing Coating for C/SiC Brake Materials , 2008 .

[90]  Jiecai Han,et al.  Oxidation-resistant ZrB2-SiC composites at 2200 °C , 2008 .

[91]  J. DiCarlo,et al.  Further Developments in Modeling Creep Effects Within Structural SiC/SiC Components , 2008 .

[92]  R. Telle,et al.  Thermal stability of zircon (ZrSiO4) , 2008 .

[93]  G. Morscher,et al.  In‐Plane Cracking Behavior and Ultimate Strength for 2D Woven and Braided Melt‐Infiltrated SiC/SiC Composites Tensile Loaded in Off‐Axis Fiber Directions , 2007 .

[94]  J. Lamon,et al.  Analysis of crack deviation in ceramic matrix composites and multilayers based on the Cook and Gordon mechanism , 2007 .

[95]  G. Morscher,et al.  Modeling stress-dependent matrix cracking and stress-strain behavior in 2D woven SiC fiber reinforced CVI SiC composites , 2007 .

[96]  F. Rebillat,et al.  Self-healing mechanisms of a SiC fiber reinforced multi-layered ceramic matrix composite in high pressure steam environments , 2007 .

[97]  G. Hilmas,et al.  Evolution of structure during the oxidation of zirconium diboride–silicon carbide in air up to 1500 °C , 2007 .

[98]  Zi-kui Liu,et al.  Thermodynamic modeling of the Hf–Si–O system , 2006, 0708.4239.

[99]  E. Bouillon,et al.  Composites in Aerospace Industry , 2006 .

[100]  A. Bunsell,et al.  A review of the development of three generations of small diameter silicon carbide fibres , 2006 .

[101]  Weon-Ju Kim,et al.  Effect of a SiC whisker formation on the densification of tyranno SA/SiC composites fabricated by the CVI process , 2006 .

[102]  G. Morscher,et al.  Progress in SiC/SiC Composites for Engine Applications , 2006 .

[103]  Mark van Roode,et al.  Ceramic Composite Development for Gas Turbine Engine Hot Section Components , 2006 .

[104]  M. Schütze,et al.  Oxidation behaviour of particle reinforced MoSi2 composites at temperatures up to 1700°C. , 2005 .

[105]  R. Naslain SiC‐Matrix Composites: Nonbrittle Ceramics for Thermo‐Structural Application , 2005 .

[106]  G. Fantozzi,et al.  Outstanding Ceramic Matrix Composites for High Temperature Applications , 2005 .

[107]  F. Christin A Global Approach to Fiber nD Architectures and Self-Sealing Matrices: From Research to Production , 2005 .

[108]  W. Ryu,et al.  Characterization of the SiCf/SiC Composite Fabricated by the Whisker Growing Assisted CVI Process , 2005 .

[109]  Ramakrishna T. Bhatt,et al.  SiC/SiC Composites for 1200°C and Above , 2005 .

[110]  L. Zawada,et al.  Performance of Four Ceramic‐Matrix Composite Divergent Flap Inserts Following Ground Testing on an F110 Turbofan Engine , 2004 .

[111]  F. Aldinger,et al.  Novel Silicon‐Boron‐Carbon‐Nitrogen Materials Thermally Stable up to 2200°C , 2004 .

[112]  T. Parthasarathy,et al.  Characterization of Oxidized Polymer‐Derived SiBCN Fibers , 2004 .

[113]  K. Nickel,et al.  Precursor derived Si-B-C-N Ceramics: oxidation kinetics , 2004 .

[114]  J. A. DiCarlo,et al.  Fracture mechanisms for SiC fibers and SiC/SiC composites under stress-rupture conditions at high temperatures , 2004, Appl. Math. Comput..

[115]  C. P. Logan,et al.  Engine Test and Post Engine Test Characterization of Self-Sealing Ceramic Matrix Composites for Nozzle Applications in Gas Turbine Engines , 2004 .

[116]  K. Nickel,et al.  Si/B/C/N/Al precursor-derived ceramics: Synthesis, high temperature behaviour and oxidation resistance , 2004 .

[117]  A. Kohyama,et al.  Processing optimization and mechanical evaluation of hot pressed 2D Tyranno-SA/SiC composites , 2003 .

[118]  R. Srinivasan,et al.  Tensile properties of nicalon fiber-reinforced carbon following aerospace turbine engine testing , 2003 .

[119]  A. Shida,et al.  High temperature crack sealant based on SiO2-B2O3 for SiC coating on carbon–carbon composites , 2003 .

[120]  G. Morscher Matrix Cracking in Four Different 2D SiC/SiC Composite Systems , 2003 .

[121]  F. Christin Design, Fabrication, and Application of Thermostructural Composites (TSC) like C/C, C/SiC, and SiC/SiC Composites , 2002 .

[122]  Akira Kohyama,et al.  Thermo-mechanical properties and microstructure of silicon carbide composites fabricated by nano-infiltrated transient eutectoid process , 2002 .

[123]  E. Bouillon,et al.  An Improved Long Life Duration CMC for Jet Aircraft Engine Applications , 2002 .

[124]  Ramakrishna T. Bhatt,et al.  Progress in SiC/SiC Ceramic Composite Development for Gas Turbine Hot-Section Components Under NASA EPM and UEET Programs , 2002 .

[125]  Lai-fei Cheng,et al.  Effect of glass sealing on the oxidation behavior of three dimensional C/SiC composites in air , 2001 .

[126]  J. Viricelle,et al.  Oxidation behaviour of a multi-layered ceramic-matrix composite (SiC)f/C/(SiBC)m , 2001 .

[127]  Yongdong Xu,et al.  Effect of carbon interlayer on oxidation behavior of C/SiC composites with a coating from room temperature to 1500°C , 2001 .

[128]  Kang N. Lee Current status of environmental barrier coatings for Si-Based ceramics , 2000 .

[129]  Lai-fei Cheng,et al.  Oxidation behavior and mechanical properties of C/SiC composites with Si-MoSi2 oxidation protection coating , 1999 .

[130]  David Brewer,et al.  HSR/EPM combustor materials development program , 1999 .

[131]  Q. Guo,et al.  Relationship between oxidation resistance and structure of B4C–SiC/C composites with self-healing properties , 1999 .

[132]  J. Lamon,et al.  Fatigue Behavior at High Temperature in Air of a 2D Woven SiC/SiBC with a Self Healing Matrix , 1998 .

[133]  R. Pailler,et al.  A Multilayer Ceramic Matrix for Oxidation Resistant Carbon Fibers-Reinforced CMCs , 1998 .

[134]  N. Bansal,et al.  Hi-Nicalon fiber-reinforced celsian matrix composites: Influence of interface modification , 1998 .

[135]  R. Naslain,et al.  The design of the fibre-matrix interfacial zone in ceramic matrix composites , 1998 .

[136]  M. Ferraris,et al.  Protective glass coating for carbon-carbon composites , 1998 .

[137]  P. Sherwood,et al.  Surface studies of potentially oxidation protective Si-B-N-C films for carbon fibers , 1997 .

[138]  F. Aldinger,et al.  A Silicoboron Carbonitride Ceramic Stable to 2000 °C. , 1996 .

[139]  M. Jansen,et al.  Properties of Amorphous SIBNC-Ceramic Fibres , 1996 .

[140]  F. Aldinger,et al.  A silicoboron carbonitride ceramic stable to 2,000°C , 1996, Nature.

[141]  R. Naslain Challenging ceramic matrix composites for applications in severe environments , 1995 .

[142]  L. Vandenbulcke,et al.  The oxidation behaviour of two- and three-dimensional C/SiC thermostructural materials protected by chemical-vapour-deposition polylayers coatings , 1994, Journal of Materials Science.

[143]  L. Vandenbulcke,et al.  Oxidation behavior of 2D and 3D carbon/carbon thermostructural materials protected by CVD polylayer coatings , 1994 .

[144]  Lionel Vandenbulcke,et al.  Oxidation tests of carbonaceous composite materials protected by SiBC CVD coatings , 1994 .

[145]  M. Jansen,et al.  New Materials in the System Si-(N,C)-B and Their Characterization , 1993 .

[146]  T. I. Barry,et al.  The calculation of phase equilibria of oxide core-concrete systems , 1993 .

[147]  N. Jacobson,et al.  Reactions of Silicon Carbide and Silicon(IV) Oxide at Elevated Temperatures , 1992 .

[148]  A. Evans,et al.  Effects of residual stress and frictional sliding on cracking and pull-out in brittle matrix composites , 1989 .

[149]  F. Langlais,et al.  THE CVI-PROCESSING OF CERAMIC MATRIX COMPOSITES , 1989 .

[150]  K. More,et al.  The effect of fiber coatings on interfacial shear strength and the mechanical behavior of ceramic composites , 1989 .

[151]  W. Hillig Strength and Toughness of Ceramic Matrix Composites , 1987 .

[152]  V. G. Borisov,et al.  Reaction thermodynamics in the SiO2-SiC system , 1968 .

[153]  J. E. Gordon,et al.  A mechanism for the control of crack propagation in all-brittle systems , 1964, Proceedings of the Royal Society of London. Series A. Mathematical and Physical Sciences.